Hinge Mechanics and Specifications
A folding board or screen does not bend the rigid core itself; instead, separate greyboard panels sit side by side with a controlled gap bridged by the outer paper wrap and inner liner.
| Component / Parameter | Specification / Range | Practical Implication for Hinges |
|---|---|---|
| Greyboard core caliper | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), 3 mm (0.118 in) | Thicker boards require a wider hinge gap so adjacent panel edges clear each other during a 180-degree fold. |
| Wrap margin (turn-in) | 15–20 mm (0.591–0.787 in) | Edges of the outer printed sheet wrap around the perimeter of the outer panels to anchor the assembly against peeling. |
| Bleed and safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety | Artwork extends across the wrap edges, while critical text and borders stay clear of the outer trim and hinge crease zone. |
| Artwork and prepress | CMYK with separate spot layers, ≥300 DPI, AI/PDF/PSD, PDF/X-1a or PDF/X-4, outlined or embedded fonts | High-resolution continuous art aligns across panels; fine text uses 100% K and rich black uses C40–60 M30–40 Y30–40 K100 with TAC ≤280%–300%. |
| Surface finish | Anti-scuff matte lamination | Protects dark artwork from rubbing and burnishing along high-contact fold lines when boards are stacked or packed. |
Fold Direction and Multi-Panel Clearance
- Single-fold (bi-fold) joints: Two panels fold face-to-face or back-to-back along one central hinge. The gap only needs to accommodate the thickness of the two panels meeting at 180 degrees plus the wrap and liner layers.
- Accordion, tri-fold, and quad-fold joints: When a board or GM screen folds over itself multiple times, an outer hinge must wrap around the combined thickness of the inner folded panels. Deeper-stacking hinges require proportionally wider panel spacing than flat inner hinges so the stack closes squarely without bowing.
- Inward vs. outward wrap tension: The sheet on the outside of a fold stretches around the outer radius of the greyboard, while the sheet on the inside compresses into the channel.
Production Steps
- Prepress and layout setup: Export the board face and backing liner as continuous spreads in PDF/X-1a or PDF/X-4 (from AI, PDF, or PSD) with 3 mm (0.118 in) perimeter bleed and ≥3 mm (0.118 in) safety clearance from outer edges and fold axes.
- Core cutting: Cut the 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) greyboard into individual rigid panel blanks with square, burr-free edges.
- Lamination and printing: Print the wrap and liner sheets in CMYK (with separate spot layers if specified) and apply surface film, such as anti-scuff matte for dark designs, before mounting.
- Panel positioning and mounting: Glue the printed face wrap and position the individual greyboard panels onto it with the required hinge gap between adjacent edges, keeping the 15–20 mm (0.591–0.787 in) wrap margin even around the perimeter.
- Turn-in and lining: Fold the wrap margins over the outer panel edges, then apply the backing liner across the inside faces and hinge channels so both sides of the gap are bridged.
- Channel pressing and folding: Press the liner and wrap firmly into the gap between panels to form a defined hinge trough, then fold the board along its intended sequence while the adhesive sets.
Sign-Off Criteria
- Flat open lay: When opened on a table, all panels rest level without springing upward at the hinge line.
- Square closure: When folded closed, panel edges align flush without forcing, bowing, or springing open.
- Unbroken surface film: Repeated opening and closing produces no white stress marks, cracking, or film lifting along the hinge trough.
- Graphic continuity: Lines, grids, and illustrations crossing the hinge align accurately between adjacent panels, with no critical text or icons distorted inside the crease.
Concrete Failure Modes
- Gap too narrow for greyboard thickness: Adjacent panel edges collide before reaching a 180-degree fold, crushing the board edges, straining the outer wrap, or tearing the paper along the spine.
- Insufficient multi-fold allowance: In four-panel or six-panel boards and GM screens, using the same narrow gap for every joint prevents the outer hinge from wrapping around the inner folded stack, causing the closed board to wedge open.
- Gap too wide: Excess unsupported wrap between panels creates a loose, sagging channel that shifts laterally during play and wears prematurely at the panel corners.
- Lamination cracking or delamination: Brittle or poorly bonded film splits along the sharp bend of the hinge trough, especially where heavy ink coverage (TAC >300%) reduces paper flexibility.
- Scuffing on dark fold lines: Dark solid areas along the outer spine rub against box interiors or adjacent panels and show glossy burnish marks when anti-scuff matte lamination is omitted.
- Text or borders in the flex zone: Placing fine rules or labels inside the hinge channel causes characters to distort into the recessed trough or wear off from repeated flexing.