This baseline changes based on binding method, fold direction, and paper caliper:

  • Saddle-stitched booklets (12–40 pages): Supply all interior and cover pages as single trimmed pages in reading order; the press imposes signatures and compensates for creep.
  • Perfect-bound (28+ pages) and sewn-bound (80–100+ pages) rulebooks: Supply interiors as single trimmed pages, and supply the cover as a single continuous flat (Back + Spine + Front) sized to the confirmed spine width.
  • Folded leaflets (4, 6, or 8 panels): Supply as two-sided flat spreads with fold marks outside the trim box; narrow inward-folding panels on roll or gate folds, while keeping accordion (Z-fold) panels equal width.
  • Scorepads: Supply as single-page layouts with extended top-edge clearance for the adhesive binding strip and backing board.

For broader prepress setup, separation rules, and file-handoff requirements, see the file layout and prepress overview.


Specifications and Paper Standards

Binding Methods and Page Counts

Bound signatures must be laid out in multiples of 4 pages (one folded sheet yields 4 pages). If a rulebook's content lands on an odd count, add blank or note pages at the end to reach the next multiple of 4.

Format Page / Panel Structure Recommended Range Layout Delivery
Saddle Stitch Multiples of 4 pages 12–40 pages Single trimmed pages (1 to N)
Perfect Binding Multiples of 4 pages 28+ pages Single trimmed interior pages + 1 wrap cover flat
Sewn Binding Multiples of 4 pages 80–100+ pages Single trimmed interior pages + 1 wrap cover flat
Folded Leaflets 4, 6, or 8 panels 2-sided flat sheet Front flat + Back flat with non-printing fold marks
Scorepads Single-sided or 2-sided sheets Variable pad count Single trimmed page with top glue-edge safety

Paper Stock and Basis Weight Equivalents

Paper weight is specified in grams per square meter (gsm). When converting to US pound (lb) ratings, distinguish US Text LB from US Cover LB by their basis sheet sizes:

  • Interior stock: 80–120 gsm (approximately 54–81 lb US Text, measured on a 25 × 38 in / 635 × 965 mm basis sheet). Typical caliper is 0.08–0.13 mm (0.003–0.005 in) per sheet.
  • Cover stock: 200–300 gsm (approximately 74–111 lb US Cover, measured on a 20 × 26 in / 508 × 660 mm basis sheet).

Prepress, Bleed, and Color Limits

  • File format: Native AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
  • Resolution: ≥300 DPI at 100% final trim size for all raster imagery.
  • Bleed: 3 mm (0.118 in) on all outer trim edges. Do not place bleed into the binding edge of a single-page interior file unless the imposition workflow specifies a gutter trim.
  • Safety margin: ≥3 mm (0.118 in) inside all trim edges and fold lines for text, page numbers, and critical icons.
  • Black and ink density: Use 100% K only for body copy and fine rules. Use rich black (C40–60 M30–40 Y30–40 K100) only for large solid fills. Keep Total Area Coverage (TAC) at ≤280%–300%.
  • Cover lamination: Use anti-scuff matte lamination on dark cover artwork to prevent marking during folding, trimming, and handling.

Page Geometry and Plain-Text Formulas

1. Spine-Width Geometry (Perfect and Sewn Binding)

Build the wrap cover flat as one continuous artboard containing the Back Cover, Spine, and Front Cover from left to right, plus 3 mm (0.118 in) bleed on all four outer edges.

Total Cover Flat Width = Back Trim Width + Spine Width + Front Trim Width + (2 × 3 mm Bleed)
Total Cover Flat Height = Trim Height + (2 × 3 mm Bleed)

Estimate spine width from the interior sheet count and paper caliper before requesting the final press confirmation:

Estimated Spine Width = (Interior Page Count / 2) × Caliper per Sheet (0.08–0.13 mm)
  • Hinge and glue allowance: Keep spine text at least 1.5–2 mm (0.059–0.079 in) narrower than the total spine width so type does not wrap onto the front or back score lines.
  • Gutter clearance (perfect binding): Side-glued spines pull the inner edge of each page into the bind. Keep text and essential diagram labels at least 6–8 mm (0.236–0.315 in) away from the binding edge, and avoid spanning critical tables or small text across the center gutter.

2. Saddle-Stitch Creep

As nested sheets fold inside one another, the innermost pages protrude farther toward the outer face edge than the outer cover sheet. When the booklet is face-trimmed flush, inner pages lose slightly more outer margin. Keep page numbers and borders inside the ≥3 mm (0.118 in) outer safety zone, with extra margin on 32–40 page booklets on heavier 120 gsm stock.

3. Leaflet Panel-Width Compensation

When a panel folds inside two outer panels (such as a 6-panel letter/roll fold or 8-panel roll/gate fold), the inner panel must be narrower than the outer panels so the paper thickness does not buckle at the crease.

  • 6-panel letter (roll) fold:
    Front Panel = W
    Back Panel = W
    Inward-Folding Panel = W - (1 to 2 mm / 0.04 to 0.08 in)
    
  • 8-panel roll fold:
    Outer Panels = W
    First Inward Panel = W - (1 to 2 mm / 0.04 to 0.08 in)
    Second Inward Panel = W - (2 to 4 mm / 0.08 to 0.16 in)
    
  • 4-panel half fold and 6/8-panel accordion (Z-fold): All panels fold outward in alternating directions and can share equal width W.
  • Fold-line safety: Keep text ≥3 mm (0.118 in) clear of every crease line. Do not place thin, high-contrast borders directly on a fold score.

4. Scorepads and Boxed Fit Clearances

  • Scorepads: Lay out pads as single trimmed pages with 3 mm (0.118 in) bleed on the three cut edges. Leave 8–12 mm (0.315–0.472 in) of clear header space at the glued top edge so padding adhesive and tear-off perforations do not intersect scoring tables.
  • Boxed components: When sizing rulebooks or folded leaflets to sit inside a rigid box, account for 1.5–2.5 mm (0.059–0.098 in) clearance across width and height, and 1.5–3 mm (0.059–0.118 in) clearance for stack height.

Production Steps and Sign-Off Criteria

Job-Specific Production Steps

  1. Lock page count and binding: Confirm whether the booklet fits saddle stitch (12–40 pages), perfect binding (28+ pages), or sewn binding (80–100+ pages) and pad to a multiple of 4 pages.
  2. Confirm caliper and spine width: Match interior paper (80–120 gsm) and cover stock (200–300 gsm) to calculate the exact spine width before finalizing the cover flat.
  3. Set up interior artboards: Create single-page artboards at exact trim size with 3 mm (0.118 in) outer bleed and ≥3 mm (0.118 in) safety margins.
  4. Set up cover or leaflet flats: Build wrap covers around the confirmed spine width, or build leaflet flats with 1–2 mm (0.04–0.08 in) panel narrowing on inward-folding flaps. Place fold and spine indicators outside the trim box as non-printing slug marks.
  5. Check ink and black separations: Convert body text to 100% K, cap TAC at ≤280%–300%, and separate any spot varnish or foil masks onto dedicated layers.
  6. Export and verify: Export as PDF/X-1a or PDF/X-4 with embedded or outlined fonts and inspect page boxes (TrimBox and BleedBox) in Acrobat or your layout tool.

Prepress Sign-Off Criteria

  • Total interior PDF page count is an exact multiple of 4 and matches the binding method's range.
  • Interior PDF is supplied as single pages in sequential reading order (1 to N), not reader or printer spreads.
  • Wrap cover flat matches Back + Spine + Front + Bleed to the tenth of a millimeter, with spine text centered inside the score lines.
  • Inward-folding leaflet panels are narrowed by 1–2 mm (0.04–0.08 in) and back-side panel order is mirrored correctly relative to the front flat.
  • All raster images are ≥300 DPI, fine text is 100% K, and TAC does not exceed 300%.

Concrete Failure Modes

  • Supplying imposed reader spreads: Exporting pages 2–3, 4–5 as paired spreads breaks press imposition for saddle-stitched and perfect-bound jobs, forcing manual page splitting and risking misaligned inner bleeds.
  • Equal-width inward leaflet panels: Making all panels identical width on a 6- or 8-panel roll fold causes the inner flap to hit the outer crease, bowing the leaflet and preventing it from lying flat in a game box.
  • Unconfirmed spine width on wrap covers: Guessing spine width instead of using the confirmed paper caliper shifts spine titles onto the front or back cover hinge, causing off-center spines and cracked ink along the score.
  • Insufficient saddle-stitch outer safety: Placing page numbers or borders closer than 3 mm (0.118 in) to the outer trim on 32–40 page booklets leads to clipped numbers on inner signatures after face-trimming.
  • Rich-black body text and high TAC: Setting small rulebook text in four-color rich black causes registration haloes on uncoated 80–120 gsm stock, while TAC >300% causes ink set-off, slow drying, and cracking along cover and leaflet folds.