The compensation amount depends on the fold geometry and paper bulk:
- Z-fold (accordion) 4-, 6-, and 8-panel leaflets: Each fold alternates direction, so no panel nests inside another. Keep all panels equal in width.
- Roll-fold (barrel) 6- and 8-panel leaflets: Each successive inward-turning panel wraps tighter inside the outer cover. Step down each nested panel by 1–2 mm (0.04–0.08 in) relative to the outer panels.
- Gate-fold 4-panel (single gate) and 6-panel (double/closed gate) leaflets: Two side flaps fold inward toward a center spine or center panel. Reduce each inward-folding flap by 1–2 mm (0.04–0.08 in) so the meeting edges clear the outer folds without colliding.
- Stock weight and caliper: Standard leaflet stocks of 80–120 gsm (approximately 0.08–0.13 mm / 0.0031–0.0051 in per sheet) typically require 1 mm (0.04 in) per nested turn, while heavier 200–300 gsm cover stocks (distinguished in US specs by Cover LB on a 20 × 26 in / 508 × 660 mm basis sheet versus US Text LB on a 25 × 38 in / 635 × 965 mm basis sheet) or multi-turn 8-panel roll folds require 1.5–2 mm (0.06–0.08 in) per step. For physical bulk allowances, closure tolerances, and fold-skew limits, see fold compensation and skew tolerance and roll- and gate-fold leaflets.
Panel Width Formulas and Specifications
Calculate the flat-sheet trim width by summing the individual compensated panel widths rather than dividing a fixed sheet evenly. Use W for the outer/primary panel width and S for the step-down allowance (1–2 mm / 0.04–0.08 in).
Plain-Text Panel Width Formulas
- 4-panel Z-fold (accordion):
Flat Width = 4 * W(all 4 panels equal)
- 4-panel Gate-fold (two flaps meeting at center):
Center Panel = W(or2 * Wif folded over a full-width back, with two flaps ofW - S)- For a standard 4-panel closed gate:
Outer Back = W,Two Side Flaps = (W / 2) - Seach,Flat Width = W + 2 * ((W / 2) - S)
- 6-panel Z-fold (accordion):
Flat Width = 6 * W(all 3 panels per side equal)
- 6-panel Roll-fold (3 panels per side, 1 inward-tucked panel):
Front Cover = W,Back Cover = W,Inward Roll Panel = W - SFlat Width = W + W + (W - S)
- 6-panel Double Gate-fold (center fold with two inward flaps):
Two Center Panels = Weach,Two Outer Flaps = W - SeachFlat Width = 2 * W + 2 * (W - S)(when structured as 4 panels) or for 3-panel-wide gate:Center = W,Two Flaps = W - Seach (Flat Width = W + 2 * (W - S))
- 8-panel Z-fold (accordion):
Flat Width = 8 * W(all 4 panels per side equal)
- 8-panel Roll-fold (4 panels per side, 2 nested inward panels):
Front Cover = W,Back Cover = W,First Inward Panel = W - S,Innermost Panel = W - (2 * S)Flat Width = W + W + (W - S) + (W - 2 * S)
Layout and Prepress Specifications
| Fold Structure | Panel Count (2-Sided) | Step-Down (S) per Nested Turn |
Bleed Margin | Fold-Crease Safety Margin |
|---|---|---|---|---|
| Z-Fold (Accordion) | 4, 6, or 8 panels | 0 mm (0 in) — equal panels | 3 mm (0.118 in) per side | >= 3 mm (0.118 in) each side of crease |
| Roll-Fold (Barrel) | 6 or 8 panels | 1–2 mm (0.04–0.08 in) per nested panel | 3 mm (0.118 in) per side | >= 3 mm (0.118 in) each side of crease |
| Gate-Fold (Single / Double) | 4 or 6 panels | 1–2 mm (0.04–0.08 in) per inward flap | 3 mm (0.118 in) per side | >= 3 mm (0.118 in) each side of crease |
- Artwork & Export Formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 at >= 300 DPI.
- Color & Ink Limits: CMYK with separate spot layers if required; total area coverage (TAC) <= 280%–300%. Use 100% K for fine body text and rich black (
C40–60 M30–40 Y30–40 K100) only for large solid fills. - Fonts: Outlined or fully embedded in the exported PDF.
Job-Specific Prepress Steps
- Lock the finished folded size first: Define
W(the finished closed width) and the finished height, then apply the fold formula above to determine each panel's exact width and the total flat-sheet trim width. - Build non-printing fold and crease guides: Set up an artboard or page matching the exact flat-sheet trim size. Place fold marks in the slug/bleed area outside the trim box—never inside the live artwork—at the cumulative panel boundaries (for example, at
W - S, then+ W, then+ Won a 6-panel roll fold). - Establish front-to-back registration: Flip the panel order horizontally on the reverse side so the
W - Sinward panel on the front aligns back-to-back with the sameW - Spanel on the back. - Apply 3 mm (0.118 in) outer bleed and fold-crease safety: Extend background colors and artwork 3 mm (0.118 in) past all four flat-sheet trim edges. Keep all text, rules, and icons at least 3 mm (0.118 in) clear of outer trim edges and at least 3 mm (0.118 in) clear on both sides of every fold crease (creating a 6 mm / 0.236 in total text-free zone straddling each fold).
- Configure multilingual black-plate swaps: Keep all CMY artwork, bleeds, panel widths, and outer fold marks identical across language versions. Isolate language-specific copy on a dedicated 100% K layer positioned strictly within the panel safety margins so black-plate swaps do not cross fold lines.
- Export and verify separations: Export a 2-page PDF/X-1a or PDF/X-4 (Front and Back) with trim and bleed boxes intact, and confirm in separation preview that fine text knocks out cleanly on the K plate only.
Pre-Print Sign-Off Criteria
Before releasing the leaflet file to imposition and plating, verify all of the following conditions:
- Panel sum matches trim box: The sum of all compensated panel widths equals the exact PDF TrimBox width to 0.1 mm (0.004 in).
- Front/back panel alignment: Narrowed (
W - SorW - 2S) panels mirror accurately between Page 1 (Front) and Page 2 (Back). - Crease clearance: No body text, table borders, or critical graphic elements sit within 3 mm (0.118 in) of any fold line.
- Marks outside live area: Fold/score marks appear only in the bleed/slug area outside the TrimBox, not on the printed sheet.
- Color and font compliance: All images are >= 300 DPI, TAC is <= 280%–300%, fine text is 100% K, and all fonts are embedded or outlined.
Failure Modes
- Equal panel widths on a roll-fold or gate-fold leaflet: Nested panels collide with the inner spine of the fold, causing the outer cover to bow open, buckle along the crease, or telescope at the fore-edge.
- Unmirrored back-side panel widths: If the
W - Spanel is placed on the left edge of the front page and also on the left edge of the back page without horizontal mirroring, back-side borders and backgrounds shift 1–2 mm (0.04–0.08 in) across the fold crease. - Text or borders inside the 3 mm (0.118 in) crease safety zone: Mechanical fold-skew and paper cracking along the score line clip characters or split thin rules unevenly across adjacent panels.
- Over-inked creases (TAC > 300%) or rich-black body text: Heavy ink coverage along a fold line cracks during folding on coated stocks, and 4-color text shows misregistration halos near the crease.
- Printing fold marks inside the TrimBox: Solid or dashed fold lines placed on the live artboard print directly on the finished leaflet edges.