This rule governs how cold foil masks are positioned across bound booklet covers produced with Card Deck Press specialist offset and tabletop manufacturing partners. The exact mask clearance and bleed allowance depend on three job conditions: the binding method (folded saddle-stitch vs. flat-spine perfect or sewn binding), the cover stock weight (200–300 gsm), and whether an outer protective film (such as anti-scuff matte lamination) seals the trimmed edges.

Cover Spread & Separation Specifications

Parameter Production Specification
File format & standard AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4; fonts outlined or embedded; ≥300 DPI
Color & foil separation CMYK process plates plus 1 dedicated 100% solid spot layer for the cold foil mask
Black & ink limits Fine text at 100% K; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300%
Trim bleed 3 mm (0.118 in) per outer trimmed edge (foil allowed in bleed only when laminated)
Safety & score clearance ≥3 mm (0.118 in) from outer trim edges, center folds, and spine-hinge scores
Binding & signatures Signatures in multiples of 4: saddle stitch (12–40 pages), perfect binding (28+ pages), sewn binding (80–100+ pages recommended)
Paper stock Interior: 80–120 gsm (~0.08–0.13 mm / 0.003–0.005 in per sheet; US Text LB measured on a 25 × 38 in basis sheet). Cover: 200–300 gsm (US Cover LB measured on a 20 × 26 in basis sheet)
Surface protection Outer protective lamination (anti-scuff matte suits dark artwork); adds 0.03–0.05 mm (0.0012–0.0020 in) for double-sided film equivalents

Prepress Layout & Mask Steps

  1. Build the outer cover spread to the exact signature bulk. Calculate the cover spread width from the front cover, back cover, and spine width derived from your final multiple-of-4 page count and interior stock caliper (0.08–0.13 mm / 0.003–0.005 in per sheet), plus 3 mm (0.118 in) bleed on all four outer edges. Restrict the cold foil mask to the outer cover spread; do not extend foil onto inside cover spreads unless separately specified and laminated.
  2. Isolate the foil mask from folds and spine-hinge scores.
    • Saddle-stitched booklets (12–40 pages): Keep all cold foil elements at least 3 mm (0.118 in) clear on both sides of the center fold score.
    • Perfect-bound (28+ pages) and sewn-bound (80–100+ pages) booklets: Keep the cold foil mask completely out of the two side-hinge score channels flanking the spine. If metallic titling is placed on a flat spine, center it within the flat spine width with ≥3 mm (0.118 in) clearance from each hinge score.
  3. Match edge bleed to the protective finish. Extend the cold foil mask into the 3 mm (0.118 in) outer trim bleed only when the cover receives protective lamination (such as anti-scuff matte) to lock down the cut edge. On unlaminated covers, pull the cold foil mask back to the ≥3 mm (0.118 in) safety margin inside the trim line.
  4. Configure overprint CMYK tinting over the foil plate. Place the cold foil mask on its own named spot separation at 100% solid fill. Set any CMYK color fills intended to tint the foil to overprint on top of the foil layer so they do not knock out the metallic base. Keep total area coverage (TAC) ≤280%–300%, use 100% K for fine text, and avoid placing heavy rich black (C40–60 M30–40 Y30–40 K100) directly over foil where a clean 100% K knockout or lighter overprint tint is required.
  5. Export and verify separations. Export the cover spread as PDF/X-1a or PDF/X-4 with fonts outlined or embedded and raster assets at ≥300 DPI. Inspect the separation preview before submission to confirm the cold foil mask appears as a single spot plate and that overprinting CMYK tints do not knock out the foil beneath them.

Sign-Off Criteria Before Plate Output

  • Spot plate isolation: Separation preview shows one dedicated spot channel for the cold foil mask, distinct from CMYK.
  • Score and hinge clearance: Foil geometry clears every saddle-stitch fold or perfect/sewn spine-hinge score by ≥3 mm (0.118 in).
  • Bleed-to-lamination pairing: Any foil extending into the 3 mm (0.118 in) trim bleed is paired with outer protective lamination; unlaminated covers hold foil inside the ≥3 mm (0.118 in) safety margin.
  • Ink density & text legibility: Combined CMYK overprint tints stay ≤280%–300% TAC, and fine body text prints as 100% K without metallic glare underneath.
  • Spread-to-bulk alignment: Cover spine width matches the locked signature count (multiples of 4) and interior sheet caliper.

Concrete Failure Modes

  • Spine-score cracking and flaking: Extending cold foil across a saddle-stitch fold or perfect/sewn hinge score fractures the metallic layer and adhesive when scored and opened, exposing raw paper fibers along the crease.
  • Guillotine edge lifting: Bleeding cold foil into the 3 mm (0.118 in) trim without protective lamination allows the trimmer blade to shear and peel the foil edge during finishing and handling.
  • Muddy or mottled overprint tints: Exceeding 280%–300% TAC or printing rich black (C40–60 M30–40 Y30–40 K100) over non-absorbent foil dulls metallic reflectance and causes ink set-off.
  • Accidental foil knockouts: Leaving overprint disabled on CMYK tint layers above the foil mask knocks out the spot foil plate underneath, replacing metallic color shifts with flat process ink.
  • Spine drift into hinge channels: Using an estimated spine width rather than the final multiple-of-4 page count and 0.08–0.13 mm (0.003–0.005 in) sheet caliper shifts spine foil into the hinge scores, causing premature cracking.