That rule holds whenever inline cold foil is applied to a folding carton before die-cutting and gluing. Two physical conditions govern how strictly you must relieve the mask:
- Glue-seam contact: Carton adhesives bond to paperboard fibers, not metallic foil transfer layers. Any foil inside a side-seam glue tab or glued bottom flap blocks fiber-to-fiber adhesion.
- Board caliper and fold angle: Heavier folding-carton stocks—such as 350 gsm art stock at 0.34–0.38 mm (0.013–0.015 in) or 400 gsm stock at 0.40–0.44 mm (0.016–0.017 in), measured on a US Cover LB basis sheet (20 x 26 in) rather than US Text LB (25 x 38 in)—generate high outer-fiber tension along 90-degree panel scores and 180-degree tuck-flap folds. Continuous solid foil spanning those creases fractures and flakes when folded.
For general spot-channel setup, knockout/overprint behavior, and metallic ink interactions, follow the Cold Foil Masks parent specification.
Tuck-Box Cold Foil Specifications
| Parameter | Requirement | Notes |
|---|---|---|
| File formats & PDF standard | AI, PDF, or PSD; PDF/X-1a or PDF/X-4 | Outlined or embedded fonts; CMYK plus separate spot layers |
| Raster resolution | ≥300 DPI | Applies to placed artwork and rasterized mask edges |
| Bleed & safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety | Keep critical foil details and fine text ≥3 mm (0.118 in) inside cuts and away from scores |
| Glue-tab exclusion | 0% cold foil on glue tabs and glue-seam folds | Keep foil inside the adjacent panel safety zone |
| Crease-line relief | No heavy solid foil across sharp scores | Break solids at creases or use fine elements/screens where artwork crosses a panel edge |
| Text & ink limits | 100% K for fine text; TAC ≤280%–300% | Rich black C40–60 M30–40 Y30–40 K100; avoid high-TAC overprints on folds |
| Protective finish | Anti-scuff matte for dark artwork | Protects overprinted foil panels during folding-gluing and handling |
Note on tuck-box sizing: Tuck-box trim dimensions derive from the specific deck's card dimensions plus box clearance of 1.5–2.5 mm (0.059–0.098 in) across width/height and 1.5–3 mm (0.059–0.118 in) for stack height; apply the foil mask directly to the locked job dieline rather than a generic template.
Job-Specific Prepress Steps
- Lock the dieline layers: Place the structural tuck-box dieline on a dedicated, non-printing overprint layer with distinct spot colors for cut lines, crease/score lines, and glue-tab zones.
- Strip foil from all glue tabs: Clear the cold foil spot channel completely from the side-seam glue flap and any glued bottom flaps. Pull the foil mask back at least 3 mm (0.118 in) from the glue-tab fold line into the visible panel so glue-wheel tolerances and sheet-to-sheet register shifts never push foil into the seam.
- Relieve sharp carton creases: Inspect every 90-degree spine/side score and 180-degree tuck-flap score. Remove solid cold foil floods from the crease path; if metallic artwork must visually cross from one face to an adjacent panel, break the mask into discrete design elements, fine rules, or open screen patterns rather than a continuous solid band.
- Set CMYK overprints and ink limits: Keep total area coverage (TAC) at ≤280%–300% across overprinted foil areas, use 100% K for fine text instead of multi-plate rich black, and extend edge-bleeding background CMYK and foil 3 mm (0.118 in) beyond outer cut lines (excluding glue tabs).
- Export separations: Output as PDF/X-1a or PDF/X-4 with the cold foil mask on its own named spot separation and all fonts outlined or embedded.
Pre-Press Sign-Off Criteria
- Separation check: Output preview shows 0% cold foil on all glue tabs and no foil encroaching within 3 mm (0.118 in) of the glue-seam fold.
- Crease check: No heavy solid foil floods or high-TAC rich black builds bridge sharp 90-degree or 180-degree carton scores.
- Geometry & bleed check: Bleed extends 3 mm (0.118 in) past cut edges, critical elements sit ≥3 mm (0.118 in) inside cuts/creases, and the dieline layer is set to non-printing overprint.
- Asset check: All raster images are ≥300 DPI and all fonts are outlined or embedded in a PDF/X-1a or PDF/X-4 file.
Concrete Failure Modes
- Side-seam delamination: Cold foil extending onto the glue tab blocks carton adhesive from wetting the paperboard fibers, causing tucked boxes to pop open at the seam during packing or transit.
- Fold cracking and foil flaking: Continuous solid foil (especially under dense CMYK overprint on 350–400 gsm / 0.34–0.44 mm / 0.013–0.017 in stock) splits along sharp scores, leaving jagged white board cracks and loose foil flakes along spines and tuck flaps.
- Misregistered metallic lips at panel edges: Solid foil placed flush against a crease line without a 3 mm (0.118 in) safety buffer shifts onto the fold radius during die-cutting, creating an unintended metallic stripe on the neighboring panel.
- Panel scuffing in folding-gluing: Dark CMYK-overprinted foil panels run without an anti-scuff matte finish show rub marks from folder-gluer belts and carton-to-carton friction.
Parent guide Cold Foil Transfer Mask Setup