Two physical conditions govern how strictly you apply that inset:

  • Board thickness and beveling: Thicker greyboard—2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) versus 1.5 mm (0.059 in)—compresses more under the steel-rule blade during die-cutting. Keeping foil at least 3 mm (0.118 in) inside every cut line keeps the stamped metallic layer on the flat face of the token rather than on the compressed bevel.
  • Die gaps, nicks, and surface finish: Adjacent tokens separated by a 3–4 mm (0.118–0.157 in) die gap, or held in the sheet by small die nicks, leave no stable flat surface across the waste bridge. For dark printed wraps around foil accents, anti-scuff matte lamination protects the surrounding ink during punching and handling.

For general foil-mask layer setup outside die-cut boards, see the Hot Foil Masks guide.

Specifications and File Layout

Parameter Requirement Notes
File format AI, PDF, or PSD (PDF/X-1a or PDF/X-4) Outline or embed all fonts
Color separations CMYK + separate spot layer for foil Keep die lines on a non-printing reference layer
Resolution ≥300 DPI Vector paths preferred for foil masks and die lines
Ink limits 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100 Total area coverage (TAC) ≤280%–300%
Greyboard caliper 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) Sheet wrap margin 15–20 mm (0.591–0.787 in)
Bleed 3 mm (0.118 in) per side Extends CMYK wrap artwork past outer trim and cut edges
Token safety inset ≥3 mm (≥0.118 in) inside cut line Applies to every token, tile, and standee perimeter
Punchboard die gap 3–4 mm (0.118–0.157 in) between tokens No foil mask elements inside waste bridges

Job-Specific Prepress Steps

  1. Lock the die-line and nick-map reference layer. Place the steel-rule die lines—token perimeters, standee slots, and marked nick positions—on a dedicated, non-printing vector layer above the artwork.
  2. Confine the hot foil spot layer per token. Build the foil mask as a 100% solid spot-color layer or channel. Keep every foil shape inside each token, tile, or standee's ≥3 mm (≥0.118 in) safety zone so no foil crosses a 3–4 mm (0.118–0.157 in) die gap or enters a standee slot.
  3. Clear die nicks and tight intersections. Check the nick positions where tokens remain attached to the waste skeleton before punching. Keep foil clear of nick bridges and follow rounded token corners rather than extending into sharp die intersections.
  4. Verify underlying CMYK and TAC. Keep the wrap artwork continuous beneath the foil mask (or knocked out only where the job specification requires) while keeping rich black at C40–60 M30–40 Y30–40 K100 and TAC ≤280%–300%.
  5. Export and inspect separations. Export as PDF/X-1a or PDF/X-4 with fonts outlined or embedded and raster assets at ≥300 DPI. Confirm in separation preview that the foil spot plate toggles independently from CMYK and the non-printing die layer.

Sign-Off Criteria Before Printing

  • Isolated spot plate: The hot foil mask sits on a single, clearly named spot separation with no foil artwork flattened into CMYK.
  • Full perimeter clearance: Every foil element on every token, tile, and standee clears the cut line by ≥3 mm (≥0.118 in) and stays completely outside 3–4 mm (0.118–0.157 in) die gaps and die nicks.
  • Print bleed and wrap: CMYK artwork includes 3 mm (0.118 in) bleed per side and accounts for the 15–20 mm (0.591–0.787 in) greyboard wrap margin on the sheet edge.
  • Print-ready PDF compliance: File is PDF/X-1a or PDF/X-4, ≥300 DPI, with outlined or embedded fonts, 100% K fine text, and TAC ≤280%–300%.

Concrete Failure Modes

  • Foil crossing cut lines or die gaps: When foil extends into the 3–4 mm (0.118–0.157 in) die gap or sits closer than 3 mm (0.118 in) to the blade path, steel-rule punching crushes the metallic layer and flakes the foil edge.
  • Foil overlapping die nicks: Punching out a token whose foil reaches a nick bridge pulls and tears the foil across the breakaway tab, leaving ragged metallic burrs on the token edge.
  • Foil merged into CMYK: Flattening the foil mask into process ink prevents generation of a separate stamping plate and causes the foil graphic to print as flat ink, requiring file rejection before press.
  • Insufficient bleed or TAC overload: Omitting the 3 mm (0.118 in) bleed exposes unprinted paper along token edges under normal die-to-print shift, while exceeding TAC 280%–300% under foil areas causes ink set-off and poor foil adhesion on the wrap sheet.