Conditions that change mask placement:

  • Box construction: Two-piece lid-and-base boxes, drawer boxes, and rigid sleeves have crisp 90-degree exterior corners where wrap paper stretches tightly over the board edge. Magnetic book-style boxes add V-grooved spine hinges and a front flap crease that flex repeatedly after assembly; keep foil masks off both the 90-degree corners and the hinge channels.
  • Greyboard caliper: Thicker board—2.5 mm (0.098 in) or 3.0 mm (0.118 in) versus 1.5 mm (0.059 in) or 2.0 mm (0.079 in)—increases the turn-over radius and wrap tension along every edge, requiring strict clearance from the corner crease lines.
  • Surface finish: Anti-scuff matte film suits dark artwork and provides a smooth, uniform carrier for hot foil release; uncoated or heavily textured wraps require clean vector edges without fine hairlines that can break up over paper grain.

Rigid Wrap & Foil Mask Specifications

Parameter Specification Notes
Greyboard thickness 1.5 / 2.0 / 2.5 / 3.0 mm (0.059 / 0.079 / 0.098 / 0.118 in) Dictates board edge step-down and wrap tension
Turn-in wrap margin 15–20 mm (0.591–0.787 in) Folded inside the board; keep 100% free of foil
Panel safety clearance >= 3 mm (0.118 in) inside flat panel crease lines Protects foil from 90-degree corner stretching
Wrap sheet bleed 3 mm (0.118 in) per side Applies to background CMYK artwork outside the turn-in
File formats AI, PDF, PSD (PDF/X-1a or PDF/X-4) Fonts outlined or embedded
Foil mask color setup 100% single spot swatch on a separate spot layer Named clearly (e.g., FOIL_GOLD) and set to overprint
Artwork resolution Vector preferred for foil; >= 300 DPI for raster base Prevents stair-stepping on stamped edges
Base ink limits TAC <= 280%–300%; rich black C40–60 M30–40 Y30–40 K100 Use 100% K for fine printed text

Plain-text wrap layout relationship: Flat Wrap Span = Sum of Outer Panel Faces + Board Thickness Allowances + (2 x 15–20 mm Wrap Margin) Max Foil Width or Height per Panel = Flat Panel Face - (2 x >= 3 mm Safety Clearance)

Building the Hot Foil Mask

  1. Lock artwork to the structural dieline: Place the thin paper wrap dieline on a non-printing reference layer. Identify flat lid, base, and side wall faces separately from 90-degree corner folds, magnetic spine V-grooves, and the 15–20 mm (0.591–0.787 in) turn-in flaps.
  2. Isolate foil elements on a dedicated spot layer: Move all foil graphics and typography onto a separate top layer above the CMYK artwork. Assign a single 100% spot color swatch to every foil shape so prepress separates it cleanly as its own stamping die plate.
  3. Restrict masks to flat panels: Keep every foil vector at least 3 mm (0.118 in) inside the crease lines of each flat lid or wall face. On drawer sleeves and two-piece lids, verify that side-wall foil sits centered on the flat wall panel without touching the top or bottom corner bends.
  4. Set overprint and ink density underneath: Set the spot foil objects to overprint so the underlying CMYK background prints continuously without white registration gaps around the stamped edges. Keep underlying dark backgrounds within rich black C40–60 M30–40 Y30–40 K100 and total area coverage (TAC) at or below 280%–300% so heavy ink does not interfere with foil adhesion.
  5. Prepare and export print-ready files: Outline or embed all fonts, flatten or verify transparency under PDF/X-1a or PDF/X-4, and keep CMYK base layers at >= 300 DPI.

Sign-Off Criteria Before Printing

  • Separation preview check: Turning off the spot foil layer leaves an intact CMYK background with no unintended white knockouts; turning on only the spot foil layer shows 100% solid spot fills with zero CMYK process builds.
  • Corner and turn-in clearance: No foil path crosses a dieline crease, 90-degree board edge, magnetic hinge groove, or the 15–20 mm (0.591–0.787 in) turn-in margin.
  • Typography and line integrity: Fine printed text on the wrap uses 100% K, and all foil vector paths are closed, merged (no overlapping duplicate strokes), and free of stray anchor points.
  • Bleed and box fit context: Background wrap artwork extends 3 mm (0.118 in) past the outer trim, while final assembled rigid boxes maintain 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack height clearance for internal contents.

Failure Modes

  • Foil cracking and splitting at corners: Placing a foil border or flood across a 90-degree greyboard fold causes the metallic layer to fracture when the thin paper wrap stretches tightly over 1.5–3.0 mm (0.059–0.118 in) board edges.
  • Flaking and glue failure in turn-in margins: Foil extending into the 15–20 mm (0.591–0.787 in) wrap margin interferes with wrap adhesive bonding to the inner greyboard and peels during corner tucking.
  • White halos around stamped graphics: Leaving foil set to knockout instead of overprint punches holes in the CMYK background; minor die-to-print registration shift during wrapping exposes unprinted paper edges.
  • Soft or bridged fine detail: Building the foil mask from rasterized CMYK pixels instead of clean vector paths—or placing foil over excessive ink buildup above 300% TAC—produces ragged edges and incomplete foil release.