Conditions that change this choice:
- Flat lid and base panels vs. side walls: Keep raised UV primarily on the flat top face and large flat side panels. Narrow side walls on shallow lids leave little room once fold clearance and safety margins are subtracted.
- Greyboard caliper: Thicker greyboard increases the wrap bend radius at each 90-degree corner, requiring wider flat-sheet clearance from the fold line so post-wrap registration stays on the flat face.
- Dark artwork and surface finish: Pair dark printed wraps with anti-scuff matte lamination before applying raised UV so the wrap resists abrasion during machine wrapping and preserves tactile contrast.
Specifications
| Parameter | Requirement | Notes |
|---|---|---|
| File formats | AI, PDF, or PSD; PDF/X-1a or PDF/X-4 | Outlined or embedded fonts; ≥300 DPI raster resolution |
| Color and separations | CMYK + separate spot layer | 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% |
| Flat-sheet bleed | 3 mm (0.118 in) per side | Applied outside the outer cut line of the wrap sheet |
| Flat-face safety margin | ≥3 mm (0.118 in) inside fold lines | Keep all raised UV mask elements inside this flat-face boundary |
| Greyboard caliper | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Determines fold radius and flat-sheet-to-post-wrap clearance |
| Turn-in wrap margin | 15–20 mm (0.591–0.787 in) | Zero raised UV allowed on turn-in flaps or corner miters |
| Base lamination | Anti-scuff matte | Recommended for dark artwork under raised UV |
Prepress Setup Steps
- Map flat-sheet geometry to post-wrap faces: On the wrap dieline, identify the flat top/bottom faces, the four side walls, the 90-degree fold zones, the corner notches/miters, and the 15–20 mm (0.591–0.787 in) turn-in margins.
- Calculate post-wrap fold clearance: Account for the greyboard thickness—1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in)—around every 90-degree fold. Because the wrap bends over the board edge, keep the raised UV mask inside the ≥3 mm (0.118 in) safety zone on each flat face rather than running it up to the nominal score line.
- Isolate the raised UV mask on a dedicated spot layer: Place all raised UV artwork on a separate spot channel named clearly for finishing, set to overprint the underlying CMYK/lamination. Strip all mask vectors from 90-degree edges, corner wraps, and the 15–20 mm (0.591–0.787 in) turn-in flaps.
- Prepare the underlying CMYK wrap artwork: Verify that dark backgrounds use rich black (C40–60 M30–40 Y30–40 K100) within a TAC limit of ≤280%–300%, fine text is 100% K, and anti-scuff matte lamination is specified where dark ink covers wrap faces.
- Export and preflight: Output as PDF/X-1a or PDF/X-4 (or packaged AI/PSD) with 3 mm (0.118 in) bleed, ≥300 DPI effective resolution, and outlined or embedded fonts.
Sign-Off Criteria
- Spot separation check: Output separation preview shows the raised UV mask as an independent spot channel, not merged into CMYK.
- Clearance verification: No raised UV geometry touches a 90-degree fold zone, corner miter, or the 15–20 mm (0.591–0.787 in) turn-in margin; all mask objects sit at least 3 mm (0.118 in) inside flat-face fold boundaries.
- Board-caliper alignment: Wrap dieline and mask clearance match the specified 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) greyboard thickness.
- Print-readiness: Bleed is 3 mm (0.118 in) per side, TAC is ≤280%–300%, raster images are ≥300 DPI, and all fonts are outlined or embedded.
Failure Modes
- Resin cracking along box edges: Raised UV extends into a 90-degree fold zone over 1.5–3 mm (0.059–0.118 in) greyboard. High-build cured resin is rigid and fractures or crazes when the wrap is folded around the board edge.
- Turn-in lifting and adhesive failure: Raised UV overlaps the 15–20 mm (0.591–0.787 in) turn-in margin or corner overlap, creating uneven thickness that prevents wrap glue from bonding cleanly to the inner greyboard.
- Post-wrap registration drift onto side walls: Flat-sheet placement ignores greyboard caliper shift, causing a mask intended for the lid face to wrap partially onto the side wall or corner miter.
- Wrap scuffing and low contrast: Dark wrap artwork without anti-scuff matte lamination or with TAC above 300% scuffs during wrapping, reducing visual contrast against the raised UV gloss.
Parent guide Raised and 3D Spot UV Mask Setup