This rule tightens under two conditions:
- Shuffling vs. collector decks: Keep card backs smooth and limit face coverage to small, centered accents on play decks; reserve heavier or broader raised UV zones for display, collector, or non-shuffled reference cards.
- Laminated vs. bare stock: Pair raised UV with a matte or anti-scuff matte film base so the gloss resin contrasts cleanly and anchors without cracking under flex.
For general spot-mask setup across packaging and printed components, see the raised UV masks overview. For physical finish behavior—including how resin height drives stack lean, shuffle drag, and edge chipping—see the card raised UV finish guide.
Raised UV Mask Specifications
| Parameter | Card Mask Specification | Notes |
|---|---|---|
| Mask edge & corner setback | 2–3 mm (0.079–0.118 in) inside trim | Follow the R3–R3.5 mm (R0.118–R0.138 in) corner curve; never enter bleed. |
| CMYK bleed & safety | 3 mm (0.118 in) bleed per side; >=3 mm (0.118 in) safety | Bordered card backs require >=4–5 mm (0.157–0.197 in) safety. |
| File & PDF standard | AI, PDF, or PSD; PDF/X-1a or PDF/X-4 | Fonts outlined or embedded; >=300 DPI for any raster elements. |
| Layer & plate separation | Separate top spot-color layer set to overprint | 100% solid spot swatch (never merged into CMYK channels). |
| Underlying ink & lamination | TAC <=280%–300%; rich black C40–60 M30–40 Y30–40 K100 | Anti-scuff matte lamination suits dark artwork beneath gloss UV. |
| Fine text handling | 100% K on CMYK plate only | Exclude fine body text and tight hairlines from the raised UV mask. |
Card Mask Preparation Steps
- Create a dedicated spot-color layer: Place all raised UV shapes on an isolated top layer (for example,
Raised_UV) colored with a single 100% spot swatch. Set every object on this layer to overprint so the underlying CMYK artwork prints continuously beneath the resin without white knockouts. - Enforce the 2–3 mm (0.079–0.118 in) perimeter setback: Offset the live mask boundary at least 2–3 mm (0.079–0.118 in) inward from the card trim box and match the R3–R3.5 mm (R0.118–R0.138 in) corner radius. Strip any mask fills or strokes that extend into the 3 mm (0.118 in) bleed area.
- Filter fine detail and balance deck coverage: Remove small type, thin rules, and tight halftones from the UV layer, keeping crisp text in 100% K on the CMYK plate. On decks that will be shuffled or stacked tall inside a box—where standard stack-height clearance is 1.5–3 mm (0.059–0.118 in)—keep raised UV areas compact and centered rather than concentrated in one corner.
- Verify base ink limits and export: Confirm total area coverage (TAC) under the mask stays at or below 280%–300% (using C40–60 M30–40 Y30–40 K100 for rich black backgrounds) and note matte or anti-scuff matte lamination on the job specification. Export as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
Prepress Sign-Off Criteria
- Separation integrity: Opening the PDF in output preview shows the raised UV mask on its own spot plate with overprint active and zero unintended CMYK knockouts.
- Perimeter clearance: Every raised UV path sits at least 2–3 mm (0.079–0.118 in) inside the trim line and clears all R3–R3.5 mm (R0.118–R0.138 in) corner arcs.
- Base file compliance: CMYK layers include 3 mm (0.118 in) bleed per side, >=3 mm (0.118 in) safety (>=4–5 mm / 0.157–0.197 in for bordered backs), >=300 DPI resolution, and TAC <=280%–300%.
- Deck suitability: Coverage density aligns with how the cards are handled—minimal, centered accents for shuffling decks, and balanced placement so stacked cards do not rock or exceed box height tolerances.
Failure Modes
- Resin bleeding to the trim or corner radius: When a raised UV mask enters the 2–3 mm (0.079–0.118 in) perimeter zone, die-cutting blades shear directly through cured resin, causing edge flaking and corner chipping (detailed in card raised UV finish behavior).
- Asymmetric heavy coverage: Placing thick raised UV blocks along one edge or corner compounds across 50+ cards, making the deck lean, rock on a table, and bind against the 1.5–3 mm (0.059–0.118 in) box stack-height clearance.
- High-coverage masks on card backs: Broad raised UV patterns on the back face create uneven drag between cards during riffle and mash shuffles.
- Mask set to knockout instead of overprint: Any slight press registration shift between the CMYK pass and the UV pass exposes an unprinted white paper halo beside the raised graphic.
- Fine text or hairlines in the UV layer: High-build resin bridges across tight letter counters and small serifs, blurring legibility instead of sharpening it.
Parent guide Raised and 3D Spot UV Mask Setup