Packed Weight, Volume, and Freight Mode Formulas

Use outer-carton length (L), width (W), and height (H) alongside units per carton to compute packed weight and shipment volume before booking a carrier.

Plain-Text Calculation Formulas

Packed Carton Gross Weight = (Units per Carton * Unit Weight) + Inner Packaging + Outer Carton Tare

Total Shipment Weight = Carton Gross Weight * Total Cartons

Carton Volume (CBM) = (L_mm * W_mm * H_mm) / 1,000,000,000
Total Ocean Volume (CBM) = Carton Volume (CBM) * Total Cartons

Air Dimensional Weight (kg) = (L_cm * W_cm * H_cm) / Metric Divisor
Air Dimensional Weight (lb) = (L_in * W_in * H_in) / Imperial Divisor

Air Chargeable Weight = max(Actual Gross Weight, Air Dimensional Weight)
-> Flag whichever value is larger as the billing weight.

Freight Mode and Divisor Variants

Freight Mode Volume / Divisor Basis Metric Formula Imperial Formula Billing Rule
Express Air Courier 5,000 cm³/kg · 139 in³/lb (L_cm * W_cm * H_cm) / 5,000 (L_in * W_in * H_in) / 139 Compare actual vs. dim weight; larger value governs
Standard Air Freight (IATA) 6,000 cm³/kg · 166 in³/lb (L_cm * W_cm * H_cm) / 6,000 (L_in * W_in * H_in) / 166 Compare actual vs. dim weight; larger value governs
Ocean Freight (LCL / FCL) Cubic Meters (CBM) (L_mm * W_mm * H_mm) / 1,000,000,000 Report separately in CBM Report total CBM and gross kg/lb separately for booking

Master Carton Variants and Governing Weight

Keep individual master cartons at or below 15–20 kg (33.07–44.09 lb) for safe manual handling and under 22.7 kg (50.04 lb) to avoid heavy-parcel handling surcharges at destination hubs.

Carton Variant Outer Dimensions (mm) Outer Dimensions (in) Units / Carton Example Gross Weight Volume (CBM) Air Dim Weight (5,000 / 139) Air Dim Weight (6,000 / 166) Governing Weight (Air)
Compact Card Deck Carton 380 x 280 x 220 mm 14.96 x 11.02 x 8.66 in 50 decks 11.50 kg (25.35 lb) 0.0234 m³ 4.68 kg (10.32 lb) 3.90 kg (8.60 lb) Actual Weight (11.50 kg / 25.35 lb)
Heavy Multi-Deck / Expansion 420 x 320 x 260 mm 16.54 x 12.60 x 10.24 in 40 sets 14.80 kg (32.63 lb) 0.0349 m³ 6.99 kg (15.41 lb) 5.82 kg (12.83 lb) Actual Weight (14.80 kg / 32.63 lb)
Boxed Tabletop Game Carton 600 x 400 x 320 mm 23.62 x 15.75 x 12.60 in 8 games 12.00 kg (26.46 lb) 0.0768 m³ 15.36 kg (33.86 lb) 12.80 kg (28.22 lb) Dimensional Weight (15.36 kg or 12.80 kg)

Inches are derived from millimetres at 25.4 mm per inch. Ocean freight bookings report the carton CBM multiplied by total carton count separately from gross weight.


Moisture, Crush, and Pallet Specifications

Moisture and Crush Protection

  • Outer Carton Board: Use double-wall corrugated cartons (BC-flute or EB-flute) for boxed games and heavy deck runs exceeding 10 kg (22.05 lb). Single-wall board is limited to light inner cartons or air-express parcels with full internal void fill.
  • Internal Buffering: Line the top and bottom of master cartons with corrugated pad inserts to absorb strapping tension and cutter-blade damage during unpacking. Fill internal voids with kraft paper or corrugated dividers so decks and rigid boxes cannot shift under vibration.
  • Moisture Barrier: Shrink-wrap individual decks or game boxes, add an inner polybag liner inside the master carton for ocean transit, and place silica-gel desiccant sachets inside the sealed liner to control condensation during container temperature swings.
  • Sealing and Strapping: Apply H-tape sealing (center seam plus both edge seams) with reinforced packing tape. Add polypropylene strapping with plastic edge protectors on cartons over 15 kg (33.07 lb).

Pallet Planning

  • Standard Footprints:
    • North America / ISO Standard: 1,200 x 1,000 mm (47.24 x 39.37 in) or 1,219 x 1,016 mm (48.00 x 40.00 in).
    • Euro Pallet (EUR 1): 1,200 x 800 mm (47.24 x 31.50 in).
  • Stacking Height: Keep total pallet height (including the ~150 mm / 5.91 in pallet base) within 1,500–1,800 mm (59.06–70.87 in) for standard warehouse racking, or 1,200–1,400 mm (47.24–55.12 in) when double-stacking inside ocean containers or loading air-cargo ULDs.
  • Zero Overhang: Align cartons flush with or slightly inside the pallet perimeter. Even 15–25 mm (0.59–0.98 in) of overhang reduces vertical corner-crush strength and causes edge tearing during forklift handling.
  • Unitization: Interlock lower layers or stack column-aligned with slip sheets between tiers, apply vertical corner boards on all four corners, and machine-wrap with stretch film anchored to the pallet base.
  • Timber Compliance: Use heat-treated wooden pallets stamped with ISPM 15 marks or molded/injection-molded plastic export pallets to prevent customs quarantine holds.

Production, Packing, and Carrier Handoff Steps

  1. Lock Carton Spec Before Press: Confirm unit dimensions, units per carton, and target weight ceiling (≤20 kg / 44.09 lb) alongside final imposition so cartons fit the destination pallet footprint without wasted air space.
  2. Post-Inspection Unit Packing: After AQL release, seal finished decks or game boxes in shrink film or tamper seals, then pack into inner boxes or directly into lined master cartons with desiccant packs.
  3. Weigh and Measure Master Cartons: Weigh a packed master carton and measure outer L x W x H in both mm and in under load (accounting for slight bulge). Update the packing list with actual figures rather than theoretical estimates.
  4. Apply Carton Markings: Print or label each carton with item description, units per carton, carton number (1 of N), gross/net weight (kg and lb), and handling icons (keep dry, stack limit).
  5. Palletize and Unitize: Stack cartons onto ISPM 15 pallets with corner boards, strapping, and stretch wrap; apply pallet-level shipping labels on two adjacent sides.
  6. Assemble Export Paperwork and Destination Records:
    • Prepare the Commercial Invoice and Packing List showing exact carton counts, HS classifications, net/gross weights (kg and lb), and total CBM.
    • Issue the Bill of Lading (ocean) or Air Waybill (air) matching the carrier booking.
    • For shipments entering regulated markets, attach the required destination compliance records on request—such as packaging participation records under VerpackG for Germany, sorting-mark documentation under Triman for France, or applicable toy-safety assessment documentation under EN 71 for the EU.
  7. Carrier Handoff: Obtain a signed pickup receipt confirming pallet/carton count and intact seal/wrap condition at factory dock departure.

Sign-Off Criteria

Do not release the shipment to the carrier until all five checks pass:

  • Weight and Dimension Match: Measured carton gross weight and outer L x W x H match the packing list and stay within the agreed handling limit (≤20 kg / 44.09 lb standard manual ceiling).
  • Chargeable Weight Flagged: Air shipments have both actual weight and dimensional weight (5,000 / 139 or 6,000 / 166) calculated, with the larger value flagged on the booking brief; ocean shipments have total CBM reported separately.
  • Moisture and Crush Integrity: Desiccant packs and poly liners are sealed (for ocean/humid routes), top/bottom pad inserts are installed, and no carton shows bulging or crushed corners.
  • Pallet Stability: Zero carton overhang beyond the pallet deck, corner boards and stretch wrap secured to the pallet base, and ISPM 15 stamp visible on wood pallets.
  • Document Alignment: Physical carton count, pallet count, weights, and CBM match the Commercial Invoice, Packing List, and carrier Bill of Lading / Air Waybill.

Concrete Failure Modes

  • Moisture Warping in Ocean Transit: Unlined cartons or missing desiccants allow container condensation to penetrate tuck boxes and card edges, causing irreversible deck curl and board warping before arrival.
  • Bottom-Layer Carton Crush: Using single-wall corrugated board under heavy card stacks (>15 kg / 33.07 lb per carton) or leaving internal air gaps causes bottom cartons to buckle under multi-tier pallet loads.
  • Pallet Overhang Damage: Cartons extending past the 1,200 x 1,000 mm (47.24 x 39.37 in) or 1,200 x 800 mm (47.24 x 31.50 in) pallet edge lose column support and get sheared by dock forks and container walls.
  • Unplanned Dimensional Weight Surcharges: Estimating air freight using only actual scale weight on boxed games leads to unexpected billing jumps when the 5,000 or 6,000 divisor exceeds actual weight.
  • Customs and Quarantine Holds: Missing ISPM 15 heat-treatment stamps on wood pallets, mismatched carton counts between the Packing List and Bill of Lading, or missing destination packaging/safety records stall port release and incur demurrage.