The sampling plan and inspection rigor shift based on four conditions:
- Order volume and tier: Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks), while boxed games and custom tooling follow project and component minimums. Larger lots and multi-press runs require proportional sampling across pallets and cartons rather than pulling only from the top layer.
- Component complexity: A single shrink-wrapped card deck requires fewer structural checks than a boxed game combining greyboard boxes, punchboards, booklets, inserts, and partner-sourced game pieces.
- Edition and assortment mix: Multi-language editions, Kickstarter/retail variants, or mixed-case assortments must be stratified so every variant is represented in the sample.
- Finish sensitivity and compliance scope: Dark solid artwork, bordered card backs, gilded edges, and projects subject to EN 71 assessment and testing require targeted visual, dimensional, and documentation checks before release.
Lot Definition and AQL Parameters
A production lot is a homogeneous quantity of finished goods produced under uniform press, finishing, and assembly conditions—typically one edition or one SKU within a single manufacturing run. If a batch splits across different card stocks, lamination lines, or assembly shifts, divide it into separate lots for sampling.
Defect Classification
Every non-conformance observed against the signed physical or digital proof is classified into one of three tiers:
- Critical: Defects that make the product unusable, misrepresent the edition, or create safety/compliance issues (e.g., missing cards or components, mixed-edition decks inside the wrong box, unreadable rules text, unsealed packs where tamper-evidence is required, or missing required compliance markings). Zero tolerance applies.
- Major: Functional, structural, or visual defects that degrade playability or perceived retail quality (e.g., off-center bordered backs exceeding safety margins, mismatched spot UV or foil registration, warped greyboard lids, tight box stack clearance, split shrink-wrap seams, or scuffed dark artwork).
- Minor: Cosmetic blemishes that do not affect function or core presentation (e.g., slight edge fuzzing within tolerance, minor dust specks in non-critical ink areas, or faint carton scuffing on outer master shippers).
Lot-Size Ranges, Sample Selection, and Acceptance Structure
Parent-level lot sizing groups production runs by tier and maps each lot to a random sample size drawn proportionally across master cartons, paired with separate Accept (Ac) and Reject (Re) thresholds for Critical, Major, and Minor defects:
| Lot Scope / Tier | Lot Stratification | Sample Selection Basis | Acceptance Threshold Structure |
|---|---|---|---|
| Small offset runs (200–300 decks) | Single lot per SKU/edition | Pull randomly across all master cartons and inner packs | Critical Ac = 0; tighter Major/Minor Ac / Re limits per project spec |
| Mid-tier runs (500–1,000+ decks) | Separate lots if split across press forms or shifts | Stratified pull from top, middle, and bottom cartons across pallets | Critical Ac = 0; scaled sample size with defined Major and Minor Ac / Re cutoffs |
| Boxed games & multi-component sets | One lot per assembled edition/assortment | Inspect full assembled sets plus sub-samples of loose inserts and pieces | Critical Ac = 0; component-level checks for cards, boards, punchboards, and booklets |
Plain-text disposition rule:
Release if Critical = 0 AND Major <= Ac(Major) AND Minor <= Ac(Minor)
Hold / Reject if Critical >= 1 OR Major >= Re(Major) OR Minor >= Re(Minor)
Inspection Specifications Against Signed Proofs
Inspectors compare sampled units directly against the signed proof (approved wet proof, press sheet, or pre-production sample) and the job's dimensional and print specifications:
| Inspection Area | Target Specification | Tolerance / Verification Check |
|---|---|---|
| Card Stock & Caliper | 300 gsm art/blue core: 0.28–0.31 mm (0.011–0.012 in) 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in) 330 gsm black core: 0.32–0.34 mm (0.0126–0.0134 in) 350 gsm art stock: 0.34–0.38 mm (0.0134–0.0150 in) 400 gsm art stock: 0.40–0.44 mm (0.0157–0.0173 in) PVC: 0.30 mm (0.012 in) |
Verify stock core type (blue core, black core, art, or PVC) and micrometer caliper. Account for double-sided film adding 0.03–0.05 mm (0.0012–0.0020 in) per card. Note: gsm is metric weight per square meter; if converting to US paper weights, distinguish Text LB (25 × 38 in / 635 × 965.2 mm basis) from Cover LB (20 × 26 in / 508 × 660.4 mm basis). |
| Trim, Safety & Corners | 3 mm (0.118 in) bleed per side; >= 3 mm (0.118 in) safety margin (>= 4–5 mm / 0.157–0.197 in for bordered backs); R3–R3.5 mm (0.118–0.138 in) corners | Check die-cut centering against the signed proof. Confirm no white bleed edge or clipped text/borders and uniform corner rounding. |
| Print & Color | CMYK + separate spot layers; >= 300 DPI source; 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; TAC <= 280%–300% | Compare color density and gray balance to signed proof. Check fine text for 100% K sharpness (no CMYK registration halo) and inspect dark solids for scuffing or ink set-off. |
| Surface Finish & Edges | Anti-scuff matte for dark artwork; lamination paired with edge treatment | Check matte/gloss/linen texture uniformity, spot UV/foil registration, and edge smoothness—especially where thick lamination meets gilded edges. |
| Boxes, Boards & Punchboards | Greyboard: 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in); wrap margin: 15–20 mm (0.591–0.787 in); punchboard die gap: 3–4 mm (0.118–0.157 in) | Verify box clearance of 1.5–2.5 mm (0.059–0.098 in) across width/height and 1.5–3 mm (0.059–0.118 in) for stack height. Test punchboard tokens for clean release without tearing paper wrap. |
| Booklets & Leaflets | Leaflets: 4, 6, or 8 panels Bound signatures (multiples of 4): saddle stitch 12–40 pages, perfect binding 28+ pages, sewn binding 80–100+ pages recommended Interior: 80–120 gsm (about 0.08–0.13 mm / 0.0031–0.0051 in per sheet); covers: 200–300 gsm |
Verify page count, signature sequence, binding integrity (staples, glue spine, or sewn signatures), and fold alignment on multi-panel leaflets. |
Job-Specific Inspection Steps
- Quarantine and Carton Verification: Confirm the entire production lot is staged, labeled by SKU/edition, and segregated from other runs. Count master cartons and verify inner pack quantities against the packing list.
- Stratified Sample Pull: Draw the AQL sample across the full pallet footprint (top, middle, bottom, and multiple carton numbers) rather than from a single opened case.
- Edition, Assortment, and Completeness Check: Open sampled units and verify card counts, deck order, booster/assortment ratios, partner-sourced game pieces, and language edition of boxes, leaflets, and booklets.
- Pack Seal and Structural Check: Inspect shrink-wrap seams, tamper seals, tuck-box flaps, and rigid box wrap margins (15–20 mm / 0.591–0.787 in). Confirm decks slide smoothly into boxes within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height clearances.
- Proof Comparison and Dimensional Measurement: Measure card caliper, corner radius (R3–R3.5 mm / 0.118–0.138 in), and border symmetry against the signed proof. Check CMYK/spot color match, 100% K fine text, and surface scuff resistance.
- Compliance and Release Documentation Check: Where applicable, confirm that required assessment and testing records (such as EN 71 documentation via European Commission Toy Safety procedures, or market-specific packaging/sorting marks where specified in the job brief) match the batch records before signing off.
Batch Disposition and Sign-Off Criteria
Record all defect counts on the lot inspection sheet and assign one of four dispositions:
| Disposition | Trigger Condition | Required Action |
|---|---|---|
| Release | Critical defects = 0, and Major/Minor counts are at or below Ac |
Apply release stamp/label to lot pallets and clear for outbound packing and freight. |
| Hold | Any Critical defect >= 1, Major/Minor counts >= Re, or missing/mismatched proof or compliance records |
Quarantine the entire lot immediately; do not ship. Issue a non-conformance report for engineering or client review. |
| Rework | Isolated, correctable defect (e.g., damaged outer shrink-wrap, mislabeled outer cartons, missing loose insert, or sortable collation error) | Segregate affected cartons, perform 100% sorting or re-packing under supervisor sign-off, and route back to reinspection. |
| Reinspect | Completed rework, or borderline lot where a secondary sample is authorized | Draw a fresh, independent AQL sample from the reworked lot. Release only if Critical = 0 and Major/Minor meet Ac. |
Concrete Failure Modes
- Bordered-back die-cut shift: Printing or cutting drift pushes a bordered card back past the 4–5 mm (0.157–0.197 in) safety margin, creating visibly uneven borders that reveal card orientation during play.
- Stack-height bind after lamination: Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card; across a full deck, uncompensated film thickness consumes the 1.5–3 mm (0.059–0.118 in) box stack clearance, bowing tuck boxes or preventing rigid lids from seating flush.
- Thick lamination conflicting with gilded edges: Heavy film lamination lifts or chips along the card edge during foil gilding, leaving ragged edge seams or peeling film.
- Scuffed dark artwork: High-ink-coverage dark backs (near the 280%–300% TAC limit) printed without anti-scuff matte varnish show rub marks and ink transfer from collation and transit vibration.
- Punchboard tear-out: Die-cut gaps narrower than 3–4 mm (0.118–0.157 in) or dull cutting rules leave nicked bridges that tear the printed face paper when players punch tokens.
- Mixed edition or assortment contamination: Cards, leaflets, or booklets from an adjacent print run or alternate language edition enter the collation line, creating a Critical defect that requires 100% lot sorting or reprint.
Guides in this section
- Failed Lot Disposition, Sorting, and Re-Inspection
- Game Board and Punchboard Lot Inspection
- Booklet, Puzzle, and Printed Extras Inspection
- Inspecting Booster Packs, Assortment Ratios, and Seals
- Box and Insert Lot Inspection Checkpoints
- Card Deck Lot Inspection Checkpoints
- Channel-Specific Pre-Shipment Lot Checks
- Edition Collation and Box Completeness Audits
- Lot Definition, Defect Classes, and AQL Sampling
- Non-Paper Tabletop Component Lot Inspection
- Verifying Production Lots Against Signed Proofs
Parent guide Card and Tabletop Production and Delivery