This guide sits within non-paper component inspection and covers lot-level checkpoints for cosmetic surface finish, dimensional balance, and sharp-edge removal.
Inspection Checkpoints by Component Type
| Component | Material & Process | Primary Checkpoints | Reference Baseline |
|---|---|---|---|
| Custom Dice | Cast resin or molded acrylic | Engraving depth, pip paint fill, mold seam flash, face flatness, opposing-face symmetry | Approved pre-production sample |
| Metal Coins | Die-cast zinc alloy | Plating coverage, antique wash match, edge burrs, relief crispness, coin flatness | Approved pre-production sample |
Custom Dice Specifications and Checkpoints
Engraving Depth and Paint Fill
- Recess depth: Engraved pips, numbers, and custom icons must be deep enough to hold paint below the outer face plane so normal table play does not abrade the pigment.
- Paint fill and wipe: Paint must fill the bottom and walls of each recess cleanly without air pinholes, missed corners, or excess pigment smeared across the surrounding face.
- Contrast and edge definition: Fine-line icons must remain legible at normal viewing distance without paint bridging across narrow gaps.
Mold Seam Flash and Surface Finish
- Parting lines: Check along edges and corners where mold halves meet for raised flash, stepped ridges, or over-sanded flat spots created while removing flash.
- Resin and acrylic clarity: On translucent or transparent dice, inspect under direct light for trapped air bubbles, swirl streaks outside the intended pattern, or cloudy polish marks.
- Tumbling and polish: Verify that matte, frosted, or high-gloss surfaces match the approved sample consistently across every face of the die.
Dimensional Balance
- Opposing-face symmetry: Measure across all three opposing face pairs to confirm uniform thickness and squareness rather than skewed or tapered faces.
- Corner and edge uniformity: Rounded or chamfered edges should be consistent around all faces so one edge does not catch or favor a specific resting face.
- Sink marks: Check the center of large flat faces for concave depressions caused by uneven cooling or curing, which distort both light reflection and resting stability.
Metal Coin Specifications and Checkpoints
Plating Coverage and Antique Wash Match
- Base plating continuity: Inspect both faces and the outer rim for bare zinc-alloy spots, pinholes, flaking, or thin plating along sharp relief edges.
- Antique wash distribution: On antiqued finishes, verify that darkened wash sits evenly inside recessed textures and lettering while raised surfaces remain clean and consistent in tone with the approved sample.
- Tarnish and spotting: Check for water spots, fingerprints sealed under lacquer, or uneven clear-coat pooling in deep recesses.
Edge Burrs and Sharp-Edge Removal
- Rim and gate trim: Run a finger lightly around the entire outer edge and any pierced cutouts to detect casting gate stubs, sharp burrs, or rough grinding marks.
- Relief edges: High-relief lettering and reeded rims must feel crisp visually without razor-sharp metal fins that can scratch cards, boards, or players' hands.
Dimensional and Weight Consistency
- Flatness: Place sample coins on a flat reference surface and press opposite edges to check for bowing or warping from die ejection.
- Weight and feel: Compare sample coin weights against the approved golden sample to catch hollow casting voids or alloy inconsistencies.
Lot Inspection Steps
- Pull the approved golden sample: Place the signed pre-production die or coin next to the production lot under neutral, diffused lighting before reviewing individual pieces.
- Sort by visual surface defects: Screen random pulls from multiple cartons for paint voids, plating skips, antique wash mismatch, and surface scratches.
- Perform a tactile edge and seam check: Handle each pulled piece to detect mold seam flash on dice and casting burrs or sharp rims on metal coins.
- Verify dimensional balance and flatness: Check opposing dice faces for uniformity and test metal coins on a flat surface for rocking or warp.
- Check packaging contact: Confirm that dice and coins packed in polybags, trays, or paperboard dividers do not rub against each other or scuff adjacent printed components during transit.
Sign-Off Criteria
- Cosmetic match: Finish, color tone, gloss or antique level, and paint fill align with the approved pre-production sample across pulls from different cartons.
- Clean edges: No sharp metal burrs, protruding gate stubs, or raised mold flash remain on handling surfaces.
- Functional geometry: Dice sit flat without rocking from sink marks or uneven seams, and coins lie flat without visible warp.
- Compliance documentation link: When a tabletop game is intended for children or falls under toy safety requirements, physical sharp-edge and small-part checks connect to formal assessment and testing records under EU Toy Safety (EN 71) rather than relying on visual lot inspection alone.
Concrete Failure Modes
- Shallow engraving with paint rub-off: Insufficient recess depth causes surface wiping during production—or normal handling afterward—to pull paint out of pips and icons.
- Over-sanded mold seams: Aggressive manual removal of parting-line flash flattens one edge or rounds one corner more than the others, unbalancing the die.
- Unremoved zinc-alloy gate burrs: Incomplete tumbling or hand-deburring leaves sharp metal tabs on coin rims that cut paper sleeves, damage game boards, or create handling hazards.
- Antique wash mismatch across batches: Variations in dip time or brushing pressure leave one batch overly dark and muddy while another looks bright and washed out against the golden sample.
- Plating blistering or flaking: Poor surface preparation before electroplating traps residue under the metallic layer, causing peeling along coin rims and high-relief edges.
- Transit abrasion: Loose bulk packing without dividers lets metal coins chip their own plating or scratch acrylic dice faces before the lot reaches final assembly.
Parent guide Non-Paper Tabletop Component Lot Inspection