Concrete Choice and Changing Conditions
Pack remote prototype kits in rigid, step-sequenced sub-packs inside a cushioned outer mailer rather than shipping loose components in a single polybag or unreinforced folding carton. Remote handling feedback only isolates real ergonomic and fit issues when testers know which materials are temporary stand-ins and when parts arrive undamaged.
Three conditions change how a prototype kit is built and packed:
- Stock substitution: When short-run digital or hand-trimmed sheets stand in for offset card stock, surface friction, snap, and stack height shift. Label every substitute pack with both its prototype stock and the target production stock.
- Hand-cut vs. die-cut construction: Hand-scored boxes, trays, and 4/6/8-panel leaflets lack the compression strength of steel-rule die-cut and machine-glued production pieces. Reinforce corners and tray walls before parcel transit.
- Component mix and weight: Kits combining paper decks with heavy partner-sourced pieces or 1.5–3 mm (0.059–0.118 in) greyboard punchboards require internal dividers so dense parts do not dent card edges under courier sorting loads.
For broader proof sign-off and pre-production workflow stages, align kit dispatch with the prototyping and proof approval sequence.
Prototype Kit Specifications and Tolerances
Record exact basis weight, basis sheet size, and caliper on every prototype label. Distinguish US Text LB (25 x 38 in / 635 x 965 mm basis sheet) from US Cover LB (20 x 26 in / 508 x 660 mm basis sheet) alongside gsm so testers and production teams do not confuse sheet weights across components.
Reference Stock Weights and Calipers
| Component Role | Production Target (gsm & US Basis) | Approximate Caliper | Lamination / Finish Allowance |
|---|---|---|---|
| Standard art / blue-core cards | 300 gsm (~111 lb US Cover) | 0.28–0.31 mm (0.011–0.012 in) | +0.03–0.05 mm (0.001–0.002 in) per card for double-sided film |
| Black-core linen cards | 310 gsm (~115 lb US Cover) | 0.30–0.32 mm (0.012–0.013 in) | +0.03–0.05 mm (0.001–0.002 in) per card if filmed |
| Heavy black-core cards | 330 gsm (~122 lb US Cover) | 0.32–0.34 mm (0.0126–0.0134 in) | +0.03–0.05 mm (0.001–0.002 in) per card if filmed |
| Art-stock cards | 350 gsm (~129 lb US Cover) | 0.34–0.38 mm (0.013–0.015 in) | Anti-scuff matte film suits dark artwork |
| Heavyweight cards | 400 gsm (~148 lb US Cover) | 0.40–0.44 mm (0.016–0.017 in) | Thick film can conflict with gilded edges |
| Waterproof plastic cards | PVC | 0.30 mm (0.012 in) | No film allowance required |
| Leaflet / booklet interiors | 80–120 gsm (~54–81 lb US Text) | 0.08–0.13 mm (0.003–0.005 in) per sheet | Uncoated or matte coated; 4/6/8 panels or multiples of 4 pages |
| Booklet covers | 200–300 gsm (~74–111 lb US Cover) | 0.19–0.31 mm (0.007–0.012 in) | +0.03–0.05 mm (0.001–0.002 in) if double-side filmed |
Structural Clearances and Transit Tolerances
- Box and tray clearances: Maintain 1.5–2.5 mm (0.059–0.098 in) across interior width and height, and 1.5–3 mm (0.059–0.118 in) for total stack height.
- Plain-text stack height formula:
Minimum interior box height = (Card count * Single card caliper) + (Card count * Film thickness if laminated) + 1.5 to 3 mm (0.059 to 0.118 in) stack clearance - Rigid board and wraps: Prototype rigid boxes and boards use 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) greyboard with 15–20 mm (0.591–0.787 in) wrap margins.
- Punchboards: Keep 3–4 mm (0.118–0.157 in) die gaps between punchable tokens so hand-cut or laser-cut prototype sheets do not tear into adjacent pieces during transit.
- Hand-trimmed card geometry: Match production corner rounding at R3–R3.5 mm (0.118–0.138 in). When trimming from press sheets, preserve 3 mm (0.118 in) bleed per side and ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in for bordered backs) so edge-shift feedback reflects real trim tolerances.
- Kit weight and outer protection: Keep individual remote tester kits between 0.5 kg and 2.5 kg (1.10 lb to 5.51 lb) per inner carton where practical, surrounded by at least 15–20 mm (0.591–0.787 in) of crushable dunnage on all six faces inside the outer corrugated shipper.
Job-Specific Assembly, Labeling, and Packing Steps
- Measure and label every substitute component.
Weigh and micrometer-check the actual prototype deck, booklet, and board before packing. Apply a printed label directly on each resealable bag or paper band stating:
- Prototype material (for example,
350 gsm / 129 lb US Cover digital matte, 0.36 mm / 0.014 in). - Target offset material (for example,
310 gsm / 115 lb US Cover black-core linen, 0.31 mm / 0.012 in). - Caliper delta per card and total stack-height delta across the deck.
- Prototype material (for example,
- Reinforce hand-cut folds, trays, and punchboards.
- Pre-score hand-cut folding cartons and 4/6/8-panel leaflets along the grain direction to prevent fiber cracking on the spine.
- Insert temporary corrugated or chipboard stiffeners inside empty tray cavities and under thin 1.5 mm (0.059 in) greyboard trays so courier compression does not bow tray walls inward.
- Sandwich hand-cut punchboards between two rigid backing boards sized at least 5 mm (0.197 in) wider than the punchboard perimeter.
- Pack pieces by assembly step, not by material type.
- Group components into numbered bags or belly-banded bundles matching the tester's sequence (for example,
Step 1: Box & Insert Fit,Step 2: Main Deck Shuffle & Fan,Step 3: Punchboard & Token Extraction,Step 4: Booklet & Leaflet Fold Check). - Place dense or sharp-edged pieces (dice, metal or acrylic tokens, thick boards) in separate cushioned compartments away from unlaminated card edges.
- Include a one-page physical manifest listing part counts, expected clearances, and the exact handling questions tied to each numbered step.
- Group components into numbered bags or belly-banded bundles matching the tester's sequence (for example,
- Immobilize the kit inside the outer parcel.
- Wrap moisture-sensitive uncoated decks and booklets in a sealed poly sleeve to prevent humidity curl during multi-day transit.
- Fill all internal voids around the prototype box so the kit cannot slide or rattle when shaken.
- Tape outer corrugated seams in an H-pattern and mark the inner lid with the kit version ID and dispatch date.
Sign-Off Criteria Before Dispatch
Verify each kit against these physical checks before sealing the outer carton:
- Label accuracy: Every substitute deck, cover, and booklet carries a readable label showing gsm, US Text or US Cover basis weight, and measured caliper in both mm and in.
- Zero-rattle fit: Shaking the sealed inner prototype box produces no shifting of trays, dividers, or loose tokens.
- Clearance verification: Card stacks drop into their tray or tuck box with 1.5–2.5 mm (0.059–0.098 in) side clearance and 1.5–3 mm (0.059–0.118 in) height clearance without forcing or bending corners.
- Intact folds and edges: Hand-cut scores show no white cracking, R3–R3.5 mm (0.118–0.138 in) corners are clean, and punchboard 3–4 mm (0.118–0.157 in) bridges remain unbroken.
- Step completeness: All numbered bags match the packing manifest and total parcel weight is recorded in kg and lb for carrier tracking.
Concrete Failure Modes
| Failure Mode | Physical Cause | Impact on Tester Feedback | Prevention |
|---|---|---|---|
| Misleading stiffness or snap ratings | Unlabeled digital 350 gsm (0.34–0.38 mm / 0.013–0.015 in) sheet sent in place of 310 gsm black-core linen (0.30–0.32 mm / 0.012–0.013 in) | Testers reject or approve card feel based on the wrong stock | Label both prototype and target gsm, US Cover LB, and caliper on the deck band |
| Crushed tray walls and jammed decks | Hand-cut tuck box or unreinforced tray shipped without internal stiffeners | Testers report box fit as too tight when transit crush caused the bind | Add temporary corrugated cavity fillers and keep 15–20 mm (0.591–0.787 in) outer dunnage |
| Pre-punched or torn tokens | Punchboards with 3–4 mm (0.118–0.157 in) die gaps packed loose under heavy decks | Tokens arrive detached, preventing evaluation of punch-out force | Sandwich punchboards between oversized rigid backing boards |
| Corner dings and edge nicking | Loose tokens or sharp tray corners packed in the same bag as unlaminated cards | Testers mistake transit damage for poor die-cut or corner rounding quality | Bag heavy parts separately and sleeve decks before boxing |
| Incomplete or out-of-order assembly notes | All parts dumped into one bulk bag without step numbering | Testers skip insert-fit checks or force components into the wrong slots | Kit every sub-assembly into numbered step bags tied to a printed manifest |
Parent guide Card and Tabletop Prototypes
Related guides
- Checking Multilingual Text Expansion on Prototype Cards and Booklets
- Temporary Prototype Substitutes for Partner-Made Components
- Physical Handling and Assembly Checks for Prototypes
- Locking Prototype Dimensions and Counts Before Production Proofing
- What a Print-and-Play Prototype Must Verify Before Proofing
- Home-Cut, Sleeved-Insert, and Digital Short-Run Build Methods