Check scope changes with project structure and finish choices. Standalone card decks starting at 200 decks (usual tiers of 200, 300, 500, and 1,000+ decks) focus on card caliper, shuffle wear, corner radius, and tuck or rigid box stack height. Multi-component boxed games, which follow project and component minimums, add greyboard hinge stress, punchboard die-gap release, booklet binding flex, and combined insert pack-up. Dark full-bleed artwork, bordered card backs, double-sided film lamination, and gilded edges each introduce specific physical failure points that digital proofs cannot expose. For broader prototype staging and proof sequencing, see the prototyping overview.
Component Specifications and Tolerance Targets
Physical prototypes must match production material calipers, board thicknesses, and clearance allowances rather than substitute office papers or unlaminated digital prints. When specifying paper weights in US units alongside gsm, distinguish US Text LB (based on a 25 × 38 in / 635 × 965 mm basis sheet) from US Cover LB (based on a 20 × 26 in / 508 × 660 mm basis sheet), because identical LB numbers represent different densities across the two basis sizes.
Cardstock, Core, and Finish Allowances
| Component Spec | Metric Caliper / Dimension | Inch Equivalent (25.4 mm/in) | Physical Check Focus |
|---|---|---|---|
| 300 gsm art / blue core | 0.28–0.31 mm | 0.011–0.012 in | Snap recovery and opacity under light |
| 310 gsm black-core linen | 0.30–0.32 mm | 0.012–0.013 in | Linen texture drag and ink scuffing |
| 330 gsm black core | 0.32–0.34 mm | 0.013–0.013 in (0.0126–0.0134 in) | Flex stiffness and edge-wear resistance |
| 350 gsm art stock | 0.34–0.38 mm | 0.013–0.015 in | Bend creasing in heavy riffle shuffles |
| 400 gsm stock | 0.40–0.44 mm | 0.016–0.017 in | Stack height growth and riffle stiffness |
| PVC card stock | 0.30 mm | 0.012 in | Static cling and edge sharpness |
| Double-sided film addition | +0.03–0.05 mm per card | +0.001–0.002 in per card | Cumulative deck height and gilding bond |
| Corner radius | R3–R3.5 mm | R0.118–R0.138 in | Pocket-catch and corner-split resistance |
| Standard safety margin | ≥3 mm | ≥0.118 in | Text and icon clearance from trim |
| Bordered-back safety margin | ≥4–5 mm | ≥0.157–0.197 in | Visual framing symmetry after die-cut |
Boards, Punchboards, Booklets, and Box Clearances
| Component Group | Production Spec | Metric Target | Inch Equivalent (25.4 mm/in) |
|---|---|---|---|
| Folding boards & punchboards | Greyboard thickness | 1.5 / 2 / 2.5 / 3 mm | 0.059 / 0.079 / 0.098 / 0.118 in |
| Wrapped boards & boxes | Wrap margin | 15–20 mm | 0.591–0.787 in |
| Punchboards | Die-cut gap between tokens | 3–4 mm | 0.118–0.157 in |
| Boxes & inserts | Width and height clearance | 1.5–2.5 mm | 0.059–0.098 in |
| Boxes & inserts | Stack height clearance | 1.5–3 mm | 0.059–0.118 in |
| Leaflets | Folded panel count | 4, 6, or 8 panels | — |
| Bound booklets | Signature structure | Multiples of 4 pages | — |
| Saddle-stitch booklets | Page range | 12–40 pages | — |
| Perfect-bound booklets | Page range | 28+ pages | — |
| Sewn-bound booklets | Recommended page range | 80–100+ pages | — |
| Booklet interior stock | 80–120 gsm (US Text LB basis) | 0.08–0.13 mm per sheet | 0.003–0.005 in per sheet |
| Booklet cover stock | 200–300 gsm (US Cover LB basis) | — | — |
Calculate expected deck stack height and box cavity height using plain-text formulas before cutting prototype boxes:
Stack height (mm) = Card count * (Base card caliper + Film addition)Stack height (in) = Stack height (mm) / 25.4Target box cavity height (mm) = Stack height (mm) + 1.5 to 3 mmTarget box cavity height (in) = Target box cavity height (mm) / 25.4
Job-Specific Physical Check Steps
- Shuffle, fan, and inspect card edges. Run riffle, overhand, and mash shuffles on the full card count using the target core and finish. Check dark solid artwork for scuffing, where anti-scuff matte suits dark coverage better than standard matte. If the deck uses gilded edges, verify that edge foil adheres cleanly without peeling against double-sided film lamination, as thick lamination conflicts with gilded edges. Inspect bordered backs against the ≥4–5 mm (0.157–0.197 in) safety margin to confirm trim variation does not expose uneven borders.
- Cycle folding boards and inspect wrap seams. Fold and unfold the prototype board repeatedly along every score line. Verify that the 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard lies flat without bowing and that the 15–20 mm (0.591–0.787 in) wrap margin stays bonded around corners and hinges without lifting or cracking ink along the crease.
- Punch out tokens from the prototype punchboard. Press every token shape out by hand across the 3–4 mm (0.118–0.157 in) die-cut gaps. Check that nick points break cleanly without tearing the printed face sheet, delaminating the greyboard layers, or leaving ragged pulp burrs on small or curved pieces.
- Read and flex leaflets and bound booklets. Refold 4-, 6-, or 8-panel leaflets to verify panel nesting order and crease cracking. Open saddle-stitched (12–40 pages), perfect-bound (28+ pages), or sewn-bound (80–100+ pages recommended) booklets flat across central spreads to confirm inner margins remain readable and signatures in multiples of four hold without spine splitting across 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in per sheet) interiors and 200–300 gsm covers.
- Pack the full game and check box tolerances. Load all cards, folded boards, punched or unpunched sheets, booklets, paper extras, and partner-sourced game pieces into the box and insert. Confirm 1.5–2.5 mm (0.059–0.098 in) clearance across width and height and 1.5–3 mm (0.059–0.118 in) clearance for stack height so components slide out without forcing and the lid closes flush. Weigh the packed unit in kg and lb (using 1 kg = 2.205 lb) to confirm handling durability during transit.
- Run applicable physical safety assessments. Where the finished product falls under toy safety rules, schedule EN 71 physical assessment and testing on prototype parts for small-part geometry, sharp points, and accessible edges in line with the European Commission Toy Safety framework.
Sign-Off Criteria
A physical prototype passes pre-proofing handling checks only when all applicable component gates are met:
- Cards: Shuffling completes without corner splitting on R3–R3.5 mm (R0.118–R0.138 in) corners, dark ink shows no immediate scuff lines, gilded edges remain intact against lamination, and bordered backs stay balanced within ≥4–5 mm (0.157–0.197 in) safety.
- Boards: Hinges open flat after repeated fold cycles with intact 15–20 mm (0.591–0.787 in) wraps and no exposed greyboard at seams.
- Punchboards: Tokens release cleanly across 3–4 mm (0.118–0.157 in) die gaps without face-paper tearing.
- Booklets: Folded leaflets nest flat without buckling; bound signatures (multiples of four) open without glue cracking or obscured gutter text.
- Box and Insert Fit: Packed components sit within 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack clearance, allowing effortless removal and flush lid closure.
Concrete Failure Modes and Spec Corrections
| Failure Mode | Physical Cause | Specification Correction |
|---|---|---|
| Box lid bows or fails to close flush | Stack calculation omitted the +0.03–0.05 mm (+0.001–0.002 in) per card from double-sided film | Recalculate stack height with film added and restore 1.5–3 mm (0.059–0.118 in) stack clearance |
| Cards jam in tuck box or rigid tray | Cavity width/height matches card trim with zero tolerance | Add 1.5–2.5 mm (0.059–0.098 in) clearance across width and height |
| Gilded edges flake or peel off | Thick film lamination prevents clean edge-foil adhesion | Reduce film thickness or remove lamination conflict before gilding |
| Dark card backs show white rub marks | Standard finish scuffs under shuffle friction | Switch to anti-scuff matte finish |
| Bordered card backs look off-center | Artwork placed inside the 3 mm (0.118 in) standard safety zone | Expand bordered-back safety margin to ≥4–5 mm (0.157–0.197 in) |
| Punchboard tokens tear face paper on release | Die-cut gap narrower than 3–4 mm (0.118–0.157 in) or oversized nicks | Widen die gap to 3–4 mm (0.118–0.157 in) and adjust nick size |
| Board wrap lifts at corners or hinges | Wrap margin cut narrower than 15–20 mm (0.591–0.787 in) | Extend wrap margin to 15–20 mm (0.591–0.787 in) |
| Booklet spine cracks or pages detach | Thick page count placed in perfect binding without sewn signatures | Move 80–100+ page books from perfect binding to sewn binding, keeping signatures in multiples of four |
Guides in this section
- Booklet, Leaflet, and Scorepad Handling Checks on Prototypes
- Booster Pack Opening and Opacity Checks on Prototypes
- Prototype Box Opening, Display, and Pack-Up Checks
- Card Handling, Shuffling, and Border Checks on Prototypes
- Board Folding, Seam, and Dual-Layer Checks on Prototypes
- Two-State Insert and Loose-Piece Storage Checks on Prototypes
- Punch-Out Token, Standee, and Dial Checks on Prototypes
- Puzzle Assembly and Paper-Extra Checks on Prototypes
Parent guide Card and Tabletop Prototypes
Related guides
- Mocking Up Coatings, Foil, and Colored Edges on Early Prototypes
- Packing Durable Prototype Kits for Remote Physical Testing
- Preparing Small-Batch Prototypes for Previews and Crowdfunding
- Checking Multilingual Text Expansion on Prototype Cards and Booklets
- Temporary Prototype Substitutes for Partner-Made Components
- Locking Prototype Dimensions and Counts Before Production Proofing