Several project conditions change how this template is built and produced:

  • Ringed or bordered backs: Concentric borders amplify slight die-cut drift, requiring a 4–5 mm (0.157–0.197 in) safe inset instead of 3 mm (0.118 in).
  • Custom trim diameters: Unlike standard rectangular tabletop card sizes that use existing dies with R3–R3.5 mm (0.118–0.138 in) corners, circular cards require dedicated round trim die tooling that follows project and component minimums alongside standard offset card runs starting at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks).
  • Dark artwork and edge finishes: Dark full-bleed designs require anti-scuff matte lamination to prevent rub marks during die cutting and handling, and thick lamination can conflict with gilded edges.

Template Geometry and 300 DPI Bleed Calculator

Round card print files are supplied on a square artboard rather than a circular crop. Let D be your target finished trim diameter in millimetres.

Trim Diameter (in)      = D / 25.4
Bleed Canvas (mm)       = D + 6
Bleed Canvas (in)       = (D + 6) / 25.4            (D_in + 0.236 in)
300 DPI Canvas (px)     = round((D + 6) / 25.4 * 300)
Standard Safe Dia (mm)  = D - 6                     (3 mm / 0.118 in radial inset)
Ringed Safe Dia (mm)    = D - 8 to D - 10           (4–5 mm / 0.157–0.197 in radial inset)
Safe Area at 300 DPI    = round(Safe_Dia_mm / 25.4 * 300)
Template Zone Diameter / Dimension (mm) Diameter / Dimension (in) Layer & Alignment Rule
Square Bleed Canvas D + 6 (D / 25.4) + 0.236 Full-bleed artwork fills the entire square
Circular Trim Line D D / 25.4 Centered circle on a non-printing spot layer
Standard Safe Area D - 6 (D / 25.4) - 0.236 Concentric circle; keeps text/icons ≥3 mm (0.118 in) inside trim
Ringed / Bordered Safe Area D - 8 to D - 10 (D / 25.4) - 0.315 to 0.394 Concentric circle; keeps ringed backs ≥4–5 mm (0.157–0.197 in) inside trim

Card Stock, Caliper, and Packaging Clearances

Specify card stock by metric weight (gsm) and approximate caliper rather than generic pound weight alone. In US paper grading, Cover LB is weighed on a 20 × 26 in (508 × 660.4 mm) basis sheet, whereas US Text LB is weighed on a 25 × 38 in (635 × 965.2 mm) basis sheet; card stocks fall under Cover grades, while lighter interior booklets (80–120 gsm, about 0.08–0.13 mm / 0.003–0.005 in per sheet) fall under Text grades.

Card Stock Approximate Caliper (mm) Approximate Caliper (in) Notes
300 gsm art / blue core 0.28–0.31 mm 0.011–0.012 in Standard opaque core for tabletop decks
310 gsm black-core linen 0.30–0.32 mm 0.012–0.013 in Embossed linen texture with black-core opacity
330 gsm black core 0.32–0.34 mm 0.013 in Higher snap and stiffness for frequent shuffling
350 gsm art stock 0.34–0.38 mm 0.013–0.015 in Rigid feel without core layer
400 gsm stock 0.40–0.44 mm 0.016–0.017 in Heavyweight board-like card feel
PVC 0.30 mm 0.012 in Waterproof plastic substrate
  • Lamination thickness: Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card to total deck height.
  • Box and insert clearances: Size rigid box cavities (typically built with 1.5, 2, 2.5, or 3 mm / 0.059, 0.079, 0.098, or 0.118 in greyboard) with 1.5–2.5 mm (0.059–0.098 in) clearance across the circular diameter and 1.5–3 mm (0.059–0.118 in) clearance over the finished stack height.

Prepress Specifications and Production Steps

Card Deck Press coordinates round-card production with specialist offset and tabletop manufacturing partners using the following prepress standards:

  • File formats and resolution: Supply layered AI, PDF, or PSD source files exported as PDF/X-1a or PDF/X-4 at ≥300 DPI.
  • Color and ink limits: Build artwork in CMYK with separate spot layers for the circular die line and any foil or spot UV masks. Set fine text to 100% K, use rich black at C40–60 M30–40 Y30–40 K100, and keep total area coverage (TAC) at ≤280%–300%.
  • Typography: Outline or embed all fonts before export.

Job-Specific Production Steps

  1. Build the square artboard: Set the document width and height to D + 6 mm (D_in + 0.236 in) at ≥300 DPI.
  2. Place the circular die line: Draw a centered circle of exact diameter D on a dedicated non-printing spot layer set to overprint.
  3. Extend full-bleed artwork: Run background colors, patterns, and textures all the way to the square bleed edges (D + 6 mm). Do not clip or mask background art to the trim circle.
  4. Center concentric safe zones: Keep all typography, card numbers, and circular icons inside D - 6 mm (or D - 8 to D - 10 mm for ringed backs).
  5. Confirm tooling and box fit: Verify circular die dimensions and box/insert cavity clearances (D + 1.5–2.5 mm / 0.059–0.098 in) against the selected card stock caliper and lamination thickness before press sign-off.

Sign-Off Criteria

  • Canvas and resolution: Artboard pixel dimensions equal round((D + 6) / 25.4 * 300) square at ≥300 DPI.
  • Die-line separation: Circular trim path of diameter D is centered on its own spot layer and does not knock out underlying ink.
  • Radial bleed coverage: Background artwork extends a full 3 mm (0.118 in) past the circular trim path in every direction.
  • Safe-area margin: All critical text and graphics sit ≥3 mm (0.118 in) inside trim, or ≥4–5 mm (0.157–0.197 in) for ringed backs.
  • Ink and font compliance: Fonts are outlined or embedded, fine text is 100% K, rich black is within C40–60 M30–40 Y30–40 K100, and TAC does not exceed 280%–300%.

Concrete Failure Modes

  • White edge slivers from circular clipping: Masking artwork to diameter D leaves unprinted paper arcs along one side when the circular die shifts within normal press tolerance. Always extend bleed across the full D + 6 mm square canvas.
  • Visibly off-center ringed backs: Placing a thin concentric ring 3 mm (0.118 in) from the trim edge exaggerates minor registration variance. Increase the safe inset to 4–5 mm (0.157–0.197 in) or use a full-bleed borderless back.
  • Edge scuffing on dark backgrounds: Uncoated or standard varnish finishes on dark rich-black round cards show rub marks from circular die ejection and shuffling. Specify anti-scuff matte lamination, and avoid combining thick lamination with gilded edges.
  • Cards binding in box cavities: Calculating tray or tuck diameter from D alone without the 1.5–2.5 mm (0.059–0.098 in) width/height clearance—or omitting the 0.03–0.05 mm (0.001–0.002 in) per-card film thickness from stack-height calculations—prevents smooth deck insertion and removal.