Both finishes reduce glare compared with gloss coatings, so the decision turns on how the component is handled, how dark the artwork is, and whether secondary finishing is planned. For broader finish options beyond these two films, see the finish comparisons.
When the Choice Changes
- Switch to matte lamination (anti-scuff matte): Dark solid artwork, heavy ink coverage, and components handled repeatedly in play. Anti-scuff matte resists burnishing and surface marks better than standard soft-touch film.
- Keep soft-touch lamination: Rigid box wraps, collector display decks, and presentation covers where first-touch feel matters more than high-cycle shuffling.
- Avoid thick film on edge-gilded decks: Thick lamination can conflict with gilded edges. Use the film-selection criteria below and review soft-touch lamination and edge finishing before locking the spec.
Specifications and Component Fit
Card Deck Press coordinates custom card and tabletop printing with specialist offset and tabletop manufacturing partners. Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks), while boxed games and tooling follow project and component minimums.
Always specify paper weights in gsm and distinguish US Text LB from US Cover LB by basis sheet size, because the same pound rating represents different sheet thicknesses across Text and Cover categories.
| Attribute | Soft-Touch Lamination | Matte Lamination |
|---|---|---|
| Surface feel and look | Velvety, low-glare tactile finish | Smooth, low-glare satin-matte finish |
| Best-fit components | Rigid boxes, display decks, presentation covers | Play decks, dark-artwork wraps, booklet covers |
| Shuffling and hand oils | Shows hand-oil buildup faster under heavy shuffling | Holds up better to frequent shuffling and handling |
| Dark artwork durability | More prone to visible rub marks on dark solids | Anti-scuff matte suits dark artwork |
| Edge-gilding compatibility | Thick film can conflict with gilded edges | Safer baseline when planning gilded edges |
| Double-sided film caliper | Adds 0.03–0.05 mm (0.0012–0.0020 in) per card |
Adds 0.03–0.05 mm (0.0012–0.0020 in) per card |
Substrate Caliper and Box Clearance Allowances
Film thickness changes total deck stack height, which directly affects rigid box sizing:
- Card stocks (uncoated/base caliper before film):
300 gsmart / blue core:0.28–0.31 mm(0.0110–0.0122 in)310 gsmblack-core linen:0.30–0.32 mm(0.0118–0.0126 in)330 gsmblack core:0.32–0.34 mm(0.0126–0.0134 in)350 gsmart stock:0.34–0.38 mm(0.0134–0.0150 in)400 gsmboard:0.40–0.44 mm(0.0157–0.0173 in)PVC:0.30 mm(0.0118 in)
- Double-sided lamination addition: Add
0.03–0.05 mm(0.0012–0.0020 in) per card to the base caliper when calculating total deck height. - Booklets and covers: Covers use
200–300 gsmstock; interior sheets use80–120 gsmstock at roughly0.08–0.13 mm(0.0031–0.0051 in) per sheet. - Rigid boxes and clearance: Greyboard walls run
1.5,2,2.5, or3 mm(0.059,0.079,0.098, or0.118 in) with a15–20 mm(0.591–0.787 in) wrap margin. Allow1.5–2.5 mm(0.059–0.098 in) clearance across width and height, and1.5–3 mm(0.059–0.118 in) for stack height.
Edge-Gilding Selection Criterion
When a deck includes gilded edges, treat film thickness as a selection gate: thick lamination can conflict with gilded edges, so favor matte lamination or adjust edge-finishing plans early. For clamp scuffing, heat damage, and edge adhesion mechanics, see soft-touch lamination and edge finishing.
Production Steps
- Prepare prepress files for dark and laminated surfaces: Export
AI,PDF, orPSDfiles asPDF/X-1aorPDF/X-4inCMYKwith separate spot layers,>= 300 DPIresolution, and outlined or embedded fonts. Set3 mm(0.118 in) bleed per side,>= 3 mm(0.118 in) safety margin, and>= 4–5 mm(0.157–0.197 in) safety for bordered backs. Use100% Kfor fine text, build rich black atC40–60 M30–40 Y30–40 K100, and keep total area coverage (TAC) at<= 280%–300%. - Pair stock weight and film to component role: Assign soft-touch film to rigid box wraps (
15–20 mm/0.591–0.787 inwrap margin over1.5–3 mm/0.059–0.118 ingreyboard) and display decks. Assign matte or anti-scuff matte film to shuffled card decks, dark-ink layouts, and200–300 gsmbooklet covers. - Calculate laminated stack height before tooling: Multiply the chosen card caliper plus
0.03–0.05 mm(0.0012–0.0020 in) per card by the deck count, then verify the1.5–3 mm(0.059–0.118 in) stack-height box clearance andR3–R3.5 mm(0.118–0.138 in) corner rounding before cutting.
Sign-Off Criteria
- Film selection matches component use: soft-touch for rigid boxes and display decks; matte or anti-scuff matte for frequent shuffling, hand oils, dark artwork, or edge-gilded projects.
- Prepress files pass
PDF/X-1aorPDF/X-4,>= 300 DPI, bleed and safety margins, andTAC <= 280%–300%. - Box dimensions account for the
0.03–0.05 mm(0.0012–0.0020 in) per-card film addition and preserve1.5–2.5 mm(0.059–0.098 in) width/height clearance and1.5–3 mm(0.059–0.118 in) stack-height clearance.
Concrete Failure Modes
- Scuffing and burnishing on dark artwork: Standard matte or soft-touch film over heavy dark ink shows rub marks during packing and handling. Switch to anti-scuff matte film and keep
TAC <= 280%–300%. - Hand-oil buildup on high-shuffle decks: Soft-touch film on frequently shuffled cards absorbs skin oils and loses its uniform velvet surface. Specify matte lamination for play decks.
- Gilded-edge conflicts: Applying thick lamination to a deck scheduled for edge gilding can interfere with the edge finish. Select a compatible matte film or review soft-touch lamination and edge finishing before production.
- Tight box fit from uncounted film caliper: Sizing a rigid box from base card stock alone omits
0.03–0.05 mm(0.0012–0.0020 in) per card, which can consume the1.5–3 mm(0.059–0.118 in) stack-height clearance across a full deck.