These targets apply to standard rigid two-piece boxes and folding tuck cartons holding unsleeved offset decks or multi-component tabletop games. Tighter 1.5 mm (0.059 in) clearances suit thin tuck boxes and single-deck rigid boxes where minimal rattle is needed; wider 2.5 to 3 mm (0.098 to 0.118 in) allowances accommodate linen-textured cards, double-sided film lamination, or multi-component trays containing booklets and punchboards.
Core Tolerance Specifications
| Dimension or Feature | Target Tolerance (mm) | Target Tolerance (in) | Governing Condition |
|---|---|---|---|
| Internal width and height clearance | 1.5–2.5 mm | 0.059–0.098 in | Total gap across card trim width and height |
| Internal stack-height allowance | 1.5–3.0 mm | 0.059–0.118 in | Extra depth above compressed deck or tray |
| Telescoping lid friction gap | 0.4–0.8 mm | 0.016–0.031 in | Clearance between wrapped base exterior and lid interior |
| Rigid greyboard thickness | 1.5 / 2.0 / 2.5 / 3.0 mm | 0.059 / 0.079 / 0.098 / 0.118 in | Selected by box footprint and total load |
| Wrap paper turn-in margin | 15–20 mm | 0.59–0.79 in | Overlap folded inside greyboard walls |
| Wrap and carton bleed | 3.0 mm per side | 0.118 in per side | Extends past die-cut trim and wrap edges |
| Artwork safety margin | >= 3.0 mm | >= 0.118 in | Minimum distance from fold scores and cut lines |
Internal Clearances and Stack-Height Calculation
Internal cavity dimensions are derived from the finished component stack rather than nominal sheet counts. Use these plain-text formulas to size the interior cavity before adding board or wrap thickness:
Internal Width = Content Width + 1.5 to 2.5 mm (0.059 to 0.098 in)Internal Height = Content Height + 1.5 to 2.5 mm (0.059 to 0.098 in)Internal Depth = Total Stack Height + 1.5 to 3.0 mm (0.059 to 0.118 in)
Card stack height shifts measurably by core stock and surface finish:
- 300 gsm art or blue-core stock: 0.28–0.31 mm (0.011–0.012 in) per card
- 310 gsm black-core linen stock: 0.30–0.32 mm (0.012–0.013 in) per card
- 330 gsm black-core stock: 0.32–0.34 mm (0.013–0.013 in) per card
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in) per card
- 400 gsm card stock: 0.40–0.44 mm (0.016–0.017 in) per card
- PVC stock: 0.30 mm (0.012 in) per card
- Double-sided film lamination: adds 0.03–0.05 mm (0.001–0.002 in) per card
When a box also holds booklets, include 0.08–0.13 mm (0.003–0.005 in) per interior sheet for 80–120 gsm text stock (roughly 54–80 lb US Text based on a 25 x 38 in / 635 x 965 mm basis sheet) plus 200–300 gsm cover stock (roughly 74–111 lb US Cover based on a 20 x 26 in / 508 x 660 mm basis sheet). For larger boxed games, verify the combined caliper of inserts, folded game boards, and die-cut punchboards—accounting for the 3–4 mm (0.118–0.157 in) die-cut kerf spacing around punchboard tokens—before locking internal depth.
Rigid Greyboard, Lid Friction, and Wrap Allowances
Two-piece rigid boxes build outward from the internal cavity. Greyboard walls are specified at 1.5 mm (0.059 in), 2.0 mm (0.079 in), 2.5 mm (0.098 in), or 3.0 mm (0.118 in) depending on box footprint and component weight.
Base Outer Width = Internal Width + (2 x Greyboard Thickness) + (2 x Wrap Thickness)Lid Inner Width = Base Outer Width + (0.4 to 0.8 mm [0.016 to 0.031 in] Telescoping Gap)
The 0.4–0.8 mm (0.016–0.031 in) telescoping gap controls how smoothly the lid slides over the base. Because wrap paper and lamination add bulk to both the outer base wall and the inner lid wall, thick matte or anti-scuff film requires targeting the upper end of the 0.4–0.8 mm (0.016–0.031 in) range to prevent binding.
Wrap sheets require 15–20 mm (0.59–0.79 in) turn-ins on all four sides so the paper wraps cleanly over the greyboard rim and anchors inside the box wall. Artwork files for wraps and folding cartons must be supplied in CMYK (with separate spot-color layers where used) at >= 300 DPI as PDF/X-1a or PDF/X-4, with 3.0 mm (0.118 in) bleed past the outer cut and >= 3.0 mm (0.118 in) safety from fold scores. Keep total area coverage (TAC) at <= 280%–300% and use 100% K for fine text to avoid cracking along tight 90-degree board folds.
Job-Specific Production Steps
- Measure the physical component stack: Sum the card caliper (including 0.03–0.05 mm / 0.001–0.002 in per card for double-sided film), booklet thickness, and insert or punchboard height under light hand pressure.
- Lock internal cavity dimensions: Add 1.5–2.5 mm (0.059–0.098 in) to content width and height, and 1.5–3.0 mm (0.059–0.118 in) to stack height.
- Calculate board and lid geometry: Select 1.5, 2.0, 2.5, or 3.0 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard, then size the lid interior with a 0.4–0.8 mm (0.016–0.031 in) telescoping clearance over the wrapped base.
- Generate the dieline and prepress layout: Add 15–20 mm (0.59–0.79 in) wrap turn-ins, 3.0 mm (0.118 in) bleed per side, and >= 3.0 mm (0.118 in) safety margins around scores and rims.
- Cut and test a white-sample dummy: Assemble an unprinted prototype using the exact production greyboard, wrap paper, and lamination, then test fit with full-weight production contents before releasing custom tooling or print runs.
Sign-Off Criteria
- Full-load insertion: Finished decks, booklets, and inserts drop into the cavity without forcing, bowing the cards, or leaving > 2.5 mm (0.098 in) of lateral play.
- Controlled lid release: Lifting the box by the lid allows the base to slide down smoothly under its own weight without sticking or dropping abruptly.
- Turn-in anchorage: Wrap margins of 15–20 mm (0.59–0.79 in) adhere flat inside the rim with no exposed greyboard corners or lifted edges.
- Score integrity: Laminated wraps and folding cartons show no ink cracking or paper splitting along 90-degree creases.
Concrete Failure Modes
- Lid binding or torn wrap corners: Caused by a telescoping gap below 0.4 mm (0.016 in) or failing to account for double-sided wrap lamination thickness on mating lid and base walls.
- Loose lid that separates in transit: Caused by a telescoping gap above 0.8 mm (0.031 in) or V-grooved board walls compressing slightly during wrapping.
- Crushed card corners or bowed tuck flaps: Caused by stack-height allowance below 1.5 mm (0.059 in), most often when 0.03–0.05 mm (0.001–0.002 in) per-card lamination bulk or linen embossing air gaps are omitted from the stack calculation.
- Edge ding and internal rattle: Caused by width or height clearance exceeding 2.5 mm (0.098 in) without an internal paperboard or molded insert to restrain movement.
- Peeling rim wraps: Caused by turn-ins shorter than 15 mm (0.59 in) or overly stiff wrap stock that pulls away from the inner greyboard wall as adhesive cures.
Guides in this section
Parent guide Card Box and Game Box Specifications