Conditions that shift the baseline:

  • Thicker greyboard (2.5 to 3 mm / 0.098 to 0.118 in): Requires the upper end of the 15 to 20 mm (0.59 to 0.79 in) turn-in range so the wrap clears the thicker edge and anchors securely on the interior face.
  • Laminated or heavy-ink wraps: Dark artwork finished with anti-scuff matte lamination resists abrasion during forming, though added film stiffness demands sharper corner pleating and firm pressing along the turn-in.
  • Thumb notches and window cutouts: Any die-cut opening in the board reduces local gluing area and requires tighter wrap-to-board registration so the wrap edge neither overhangs the opening nor leaves greyboard visible.
  • Telescoping lids and tight trays: Box clearances of 1.5 to 2.5 mm (0.059 to 0.098 in) across width and height leave little room for bunched turn-ins or bowed V-grooved walls.

Core Specifications and Allowances

Rigid boxes built by specialist offset and tabletop manufacturing partners combine die-cut or V-grooved greyboard cores with offset-printed wrap sheets.

Parameter Specification Fabrication Role
Wrap turn-in margin 15–20 mm (0.59–0.79 in) Anchors the wrap around the board edge onto the inner wall
Greyboard thickness 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) Sets wall rigidity, outer wrap span, and V-groove cut depth
Box clearance (width/height) 1.5–2.5 mm (0.059–0.098 in) Accommodates wrap thickness and corner turn-ins around contents
Box clearance (stack height) 1.5–3 mm (0.059–0.118 in) Prevents lid binding or proud stack edges
Wrap bleed 3 mm (0.118 in) per side Extends background artwork past the outer wrap trim edge
Wrap safety margin >=3 mm (0.118 in) Keeps critical text and borders clear of fold lines and cutouts

Wrap Sheet Sizing Formula

Because the wrap sheet covers the exterior panel, wraps over the board thickness on all sides, and folds inward, calculate total flat wrap dimensions in plain text as:

Wrap sheet width = Flat board width + (2 * Board thickness) + (2 * Wrap turn-in margin)

Wrap sheet height = Flat board height + (2 * Board thickness) + (2 * Wrap turn-in margin)

With standard 15 to 20 mm (0.59 to 0.79 in) turn-ins, the turn-in allowance alone adds 30 to 40 mm (1.18 to 1.57 in) to each axis before accounting for board caliper.

Prepress and Surface Requirements for Wrap Sheets

  • File format and color: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts, CMYK builds plus separate spot layers, and >=300 DPI resolution.
  • Black builds and ink limits: Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for solid dark areas, and keep total area coverage (TAC) at <=280%–300% so heavy ink does not crack along 90-degree V-grooves or turn-in folds.
  • Protective finish: Anti-scuff matte lamination suits dark artwork, preventing rub marks as sheets pass through gluing and wrapping rollers.

Job-Specific Production Steps

  1. Lay out the wrap dieline around board caliper: Map the outer panel faces, V-groove fold lines, 15 to 20 mm (0.59 to 0.79 in) turn-in flaps, and corner notches onto the flat wrap sheet. Apply 3 mm (0.118 in) bleed on the outer perimeter and keep logos or borders >=3 mm (0.118 in) away from V-groove bends and cutout edges.
  2. Cut and V-groove the greyboard: Blank the 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard to net panel dimensions. Cut V-grooves at a calibrated depth that leaves a thin hinge at the bottom of the groove so panels fold to crisp 90-degree corners without splitting.
  3. Die-cut board and wrap openings: Punch thumb notches, window cutouts, or ribbon slots in the greyboard and match the corresponding relief cuts in the printed wrap. Corner reliefs in the wrap must clear the board thickness so overlapping paper does not stack at the interior corners.
  4. Glue, register, and turn in: Coat the wrap sheet with adhesive, register the folded or flat greyboard skeleton to the wrap marks, and press the panels down. Fold and wipe the 15 to 20 mm (0.59 to 0.79 in) turn-ins tightly over the board edges and into any cutout recesses, then seat the corner pleats flat.

Sign-Off Criteria

Verify pre-production samples against these physical checks before approving full offset and box-making runs:

  • Turn-in bond and depth: All four turn-in flaps measure within 15 to 20 mm (0.59 to 0.79 in), lie flat against the interior board face, and show zero edge lift at corners or along thumb notches.
  • Corner geometry: V-grooved edges form square 90-degree corners without bowed sidewalls, fractured board hinges, or cracked ink and lamination along the fold.
  • Cutout registration: Wrap reliefs align cleanly with greyboard thumb notches and windows, leaving no exposed greyboard edge and no overhanging paper lip that snags components.
  • Clearance and fit: Finished inner tray and outer lid dimensions maintain 1.5 to 2.5 mm (0.059 to 0.098 in) width and height clearance and 1.5 to 3 mm (0.059 to 0.118 in) stack-height clearance around packed decks, boards, or inserts.

Concrete Failure Modes

Failure Mode Physical Cause Production Outcome
Turn-in edge peel Margin cut below 15 mm (0.59 in) or insufficient pressing on laminated stock Wrap pulls away from the inner wall, exposing raw greyboard
Corner bunching and lid bind Turn-in exceeds 20 mm (0.79 in) or corner reliefs are undersized Paper overlaps at interior corners, consuming the 1.5–2.5 mm (0.059–0.098 in) clearance
Bowed walls or split corners V-groove cut too shallow or too deep for the selected board caliper Shallow grooves round the corner; over-deep grooves tear the hinge under handling
Exposed board at cutouts Wrap-to-board registration drift or missing cutout bleed/relief Greyboard edge shows inside thumb notches or window openings
Cracked or scuffed wrap folds TAC above 280%–300% or unlaminated dark solids on sharp folds Ink fractures along the 90-degree box edge and scuffs during assembly