When to adjust the margin: Use the lower end near 15 mm (0.59 in) on thinner 1.5 mm (0.059 in) greyboard or shallow box walls where adhesive tack sets quickly and excess flap would interfere with interior liners. Increase toward 20 mm (0.79 in) on thicker 2.5 to 3 mm (0.098 to 0.118 in) greyboard walls, taller box sides, or laminated wraps where added film stiffness requires a wider glue area inside the wall to hold the fold flat. These allowances sit within the broader wrap and die-cut allowances for rigid box construction.
Wrap and Corner Specifications
The wrap sheet must cover the exterior panel, rise up the outer wall height, cross the top edge of the greyboard, and fold down inside the wall.
| Parameter | Metric | Imperial | Role in Wrap Fit |
|---|---|---|---|
| Turn-in margin | 15 to 20 mm | 0.59 to 0.79 in | Interior wall overlap for adhesive hold |
| Greyboard thickness | 1.5 / 2 / 2.5 / 3 mm | 0.059 / 0.079 / 0.098 / 0.118 in | Sets edge-wrap distance and corner relief gap |
| Outer bleed | 3 mm per side | 0.118 in per side | Extends print past the die-cut wrap perimeter |
| Artwork safety margin | ≥3 mm from folds | ≥0.118 in from folds | Keeps critical text and borders off 90-degree edges |
Wrap Sheet Sizing Formula
Calculate the flat wrap span before die-cutting by accounting for every surface the sheet crosses, including the greyboard edge thickness on both sides:
Flat Wrap Span = Exterior Base Span + (2 * Wall Height) + (2 * Greyboard Thickness) + (2 * Turn-In Margin)
For prepress files (AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4), keep artwork in CMYK with separate spot layers at ≥300 DPI, fonts outlined or embedded, 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) at ≤280%–300%. Anti-scuff matte lamination suits dark wrap artwork, though added film increases spring-back tension along the turn-in fold.
Corner Miter Geometry
Unmitered square corners double up four layers of paper when folded over a 90-degree greyboard corner, creating ridges that prevent tight lid-to-base closure. Die-cutting a mitered relief removes the corner triangle while leaving a small tab or allowance equal to the greyboard thickness (1.5 to 3 mm / 0.059 to 0.118 in) so the folded wrap completely covers the raw board corner before meeting the adjacent flap inside the wall.
Production Steps
- Lay out the flat wrap dieline: Build the dieline using the flat wrap span formula, adding 15 to 20 mm (0.59 to 0.79 in) turn-in flaps on all four sides and 3 mm (0.118 in) print bleed beyond the outer cut line.
- Set corner miter relief: Notch each corner of the wrap dieline so the adjacent turn-in flaps clear each other inside the box wall without overlapping, while retaining enough corner tab to wrap around the greyboard thickness.
- Prepare and laminate the printed sheet: Print CMYK and spot layers within the ≤280%–300% TAC limit, apply anti-scuff matte or gloss film if specified, and die-cut the outer perimeter and corner miters.
- Apply adhesive and position greyboard: Coat the back of the wrap sheet evenly with adhesive and register the assembled greyboard shell onto the center panel.
- Fold and press turn-ins: Wrap the side walls upward, tuck the corner relief tabs tightly over the board corners, and fold the 15 to 20 mm (0.59 to 0.79 in) turn-in flaps flat against the interior walls under firm roller pressure.
Sign-Off Criteria
- Full inner-wall adhesion: All four turn-in flaps bond flat against the interior greyboard walls with no edge lift or air pockets.
- Covered board corners: Raw greyboard is completely concealed at every exterior and interior corner seam.
- Flush corner seams: Adjacent turn-in flaps meet cleanly inside the wall without overlapping layers, ridges, or paper bunching.
- Intact fold lines: Ink and lamination remain unbroken along the 90-degree outer and inner wall edges, with no cracking or whitening.
- Aligned graphics: Logos, borders, and type maintain ≥3 mm (0.118 in) clearance from wall folds and stay centered on the lid or base face.
Failure Modes
- Turn-in under 15 mm (0.59 in): Reduces the bonded surface area inside the wall, causing the wrap edge to peel or lift away from the greyboard, especially on laminated sheets with high fold tension.
- Turn-in over 20 mm (0.79 in) without liner compensation: Excess flap depth collides with interior box liners or crowds the inner wall cavity, creating uneven interior walls.
- Insufficient or omitted corner miters: Overlapping paper layers bunch at the corners, thickening the outer wall profile and interfering with telescoping lid fit.
- Over-trimmed corner miters: Cutting too close to the board fold leaves a triangular gap that exposes raw greyboard at the box corners.
- High ink density over folds: Exceeding 280%–300% TAC without compatible lamination causes ink cracking and flaking along the sharp 90-degree greyboard edges during wrapping.
Parent guide Panel Wrap Allowances and Die-Cut Registration Tolerances