For broader board core and liner options, see Game Board Materials.
Specifications and Board Construction
A magnetic-receptive panel replaces standard single-step paper-to-board mounting with a three-layer sandwich on the active face: greyboard core, ferrous interlayer sheet, and outer printed wrap paper.
| Specification Area | Manufacturing Standard | Design & Fit Impact |
|---|---|---|
| Greyboard core thickness | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) | Thicker cores resist bow from ferrous sheet tension; 2 mm (0.079 in) and 2.5 mm (0.098 in) balance rigidity and folded stack height. |
| Interlayer placement | Laminated between the greyboard core and outer wrap paper | Keeps the ferrous surface close to the face for reliable magnetic hold while hiding raw metal behind printed paper. |
| Hinge-channel exclusion | Interlayer stopped short of all fold lines and V-grooves | Prevents metal fatigue, cracking, and hinge tenting when boards or multi-panel GM screens fold. |
| Wrap margin (turn-in) | 15–20 mm (0.591–0.787 in) | Wraps cleanly over the board perimeter and anchors the outer paper to the back liner, sealing the ferrous sheet edges. |
| Box fit clearance | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Accounts for added interlayer caliper so folded boards and GM screens slide into rigid boxes without binding. |
| Wrap paper weight basis | Specified in gsm (distinct from US Text LB at 25 x 38 in and Cover LB at 20 x 26 in) | Lighter Text-basis wraps conform tightly over stepped edges; heavier Cover-basis wraps mask slight surface telegraphing but resist tight turn-ins. |
| Prepress & surface finish | CMYK with separate spot layers, >=300 DPI, 3 mm (0.118 in) bleed per side; anti-scuff matte for dark artwork | PDF/X-1a or PDF/X-4 with outlined or embedded fonts, 100% K fine text, rich black C40–60 M30–40 Y30–40 K100, and TAC <=280%–300%. |
Weight, Caliper, and Wrap Paper Basis
Adding a ferrous sheet increases panel mass in kg (lb) relative to all-paper greyboard construction, which raises per-unit carton weight and shifts center-of-gravity balance on upright GM screens. Because each active panel adds ferrous caliper on top of the 1.5–3 mm (0.059–0.118 in) greyboard core, total folded stack height must be verified against the outer box depth using:
Folded board height + 1.5–3 mm (0.059–0.118 in) clearance = minimum box interior depth
When specifying the outer wrap paper, distinguish metric gsm from US basis weights by sheet size: US Text LB is weighed on a 25 x 38 in (635 x 965.2 mm) basis sheet, whereas US Cover LB is weighed on a 20 x 26 in (508 x 660.4 mm) basis sheet. A wrap stock specified in gsm ensures consistent thickness across offset runs regardless of regional paper naming.
Job-Specific Production Steps
- Panel Mapping and Hinge Exclusion: Define separate die-line layers in AI/PDF/PSD for the greyboard cut, wrap paper bleed (3 mm / 0.118 in per side), and ferrous interlayer islands. Offset each ferrous island back from every fold channel and outer board edge so the wrap paper bonds directly to bare greyboard along all hinges and turn-ins.
- Tooling and Blanking: Boxed game boards, GM screens, and custom interlayer dies follow project and component minimums. Blank or die-cut the ferrous sheets per panel island so no raw metal spans a hinge line.
- Core-to-Interlayer Lamination: Bond the ferrous islands to the active face of the 1.5–3 mm (0.059–0.118 in) greyboard core using a metal-compatible adhesive, pressing flat to eliminate air pockets before wrap mounting.
- Wrap Mounting and Turn-In: Mount the printed wrap sheet (and backing liner) over the laminated face, folding the 15–20 mm (0.591–0.787 in) wrap margin onto the reverse side. Apply anti-scuff matte lamination to dark wrap artwork to prevent rub marks from sliding magnetic tokens.
- Hinge Pressing and Conditioning: Press fold channels and stack finished boards under flat weight during adhesive cure to counter asymmetric curl between the ferrous-backed face and the paper-only back.
- Regulatory Assessment for Paired Magnets: While the ferrous interlayer itself is non-magnetized, pairing a magnetic-receptive board or GM screen with loose magnetic tokens or clips for children's products requires EN 71 assessment and testing for magnet flux and small-part hazards. Maintain test records and technical documentation per the EU Toy Safety framework.
Sign-Off Criteria
Before approving full production from pre-production white dummies or wet proofs:
- Hinge actuation: All fold channels open and close smoothly to 180 degrees (or the intended GM screen standing angle) without resistance, cracking, or metal ridge telegraphing through the wrap.
- Magnetic hold through wrap: Production magnetic tokens and initiative clips hold securely across the active panel face without sliding under normal tabletop handling, and without scratching the matte finish.
- Perimeter adhesion: The 15–20 mm (0.591–0.787 in) wrap margin and backing liner show continuous bond around all four edges with zero delamination over the ferrous step-down.
- Flatness and box fit: Panels lie flat on the table and fit inside the rigid box with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance.
- Recorded weight: Finished board or GM screen weight is logged in kg and lb for carton-pack and freight calculations.
Concrete Failure Modes
- Hinge tenting or crease cracking: Occurs when the ferrous interlayer extends into or across a fold channel, preventing the wrap and backing paper from hinging cleanly and causing the board to spring open.
- Edge lift and wrap bubbling: Occurs when standard water-based paper glue is used directly over an untreated ferrous surface, or when the interlayer runs too close to the board edge and starves the 15–20 mm (0.591–0.787 in) wrap margin of direct paper-to-greyboard bond.
- Panel warp (bowing): Occurs when the rigid ferrous sheet on one side of a 1.5 mm (0.059 in) greyboard core shrinks or expands at a different rate than the unreinforced paper liner on the back, pulling the board into a concave or convex arc.
- Step-edge telegraphing: Occurs when a thick ferrous sheet ends abruptly beneath thin, high-gloss wrap paper, creating a visible ridge inside the board margin.
- Box binding: Occurs when box depth is calculated from standard greyboard thickness without adding the ferrous interlayer caliper across every folded panel in the stack.
Parent guide Game Board and GM Screen Materials