Three conditions change the pairing:
- Double-sided vs. single-sided artwork: If the back of the board or GM screen carries full-color art, replace the plain counter-liner with a printable coated back liner carrying the same film lamination as the face.
- Core thickness: Thicker 2.5 mm and 3 mm (0.098 in and 0.118 in) grayboard cores require the full 15–20 mm (0.591–0.787 in) wrap margin to tuck cleanly around the edges without pulling back.
- Fold count and panel width: Multi-panel folding boards and GM screens concentrate stress along the hinges, requiring long-grain alignment parallel to the fold lines and flexible wrap adhesives.
Face Wrap Stocks and Counter-Liner Specifications
Paper weights in print production are specified in grams per square meter (gsm) alongside US pound weights. US Text (Book) LB and US Cover LB are not interchangeable because they use different basis sheet sizes: US Text LB is weighed on a 25 × 38 in (635 × 965 mm) 500-sheet ream, whereas US Cover LB is weighed on a 20 × 26 in (508 × 660 mm) 500-sheet ream. For example, a 500-sheet ream weighing 100 lb (45.4 kg) equals about 148 gsm in US Text LB, but about 270 gsm in US Cover LB.
| Component | Material Type | Typical Weight (gsm / US Basis) | Finish & Surface Behavior | Primary Use |
|---|---|---|---|---|
| Face Wrap (Standard) | Coated Art Paper (C1S or C2S) | ~128–157 gsm (~86–106 lb US Text; 25 × 38 in / 635 × 965 mm) | Smooth clay coating for sharp halftone dots and clean film lamination | Full-color game boards and printed GM screen exteriors |
| Face Wrap (Tactile) | Linen-Embossed or Textured Paper | ~120–150 gsm (~81–101 lb US Text; 25 × 38 in / 635 × 965 mm) | Embossed micro-texture diffuses overhead glare and resists finger marks | Classic board surfaces and textured GM screens |
| Counter-Liner (Plain) | Uncoated or Matte-Calendered Liner | ~120–157 gsm (~81–106 lb US Text; 25 × 38 in / 635 × 965 mm) | High-friction or neutral matte back surface; balances face curl | Single-sided game boards with unprinted backs |
| Counter-Liner (Printed) | Coated Art Liner | ~128–157 gsm (~86–106 lb US Text; 25 × 38 in / 635 × 965 mm) | Matches face wrap coating and film lamination to equalize tension | Double-sided boards and interior-printed GM screens |
Heavier Cover-weight stocks (200–300 gsm, or ~74–111 lb US Cover at 20 × 26 in / 508 × 660 mm) are reserved for unmounted covers and rigid cards rather than turned-edge board wraps, because thick sheets resist folding cleanly around 90-degree grayboard edges.
Prepress and Wrap Layout Tolerances
- File formats: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color and resolution: Build raster artwork at ≥300 DPI in CMYK with separate spot layers for metallic inks or spot UV. Use 100% K for fine black text, rich black at C40–60 M30–40 Y30–40 K100 for large dark fills, and keep Total Area Coverage (TAC) at ≤280%–300%.
- Bleed and wrap margin: Extend artwork by at least 3 mm (0.118 in) bleed per side beyond the finished board face, and keep critical text and icons inside a ≥3 mm (0.118 in) safety zone from the board edge and fold hinges. For full-wrap production, the physical wrap sheet extends 15–20 mm (0.591–0.787 in) past each board edge to form the turn-in flaps.
- Surface film: Pair dark wrap artwork with anti-scuff matte lamination to prevent burnishing and rub marks during packing and play.
Grain Direction, Lamination, and Production Steps
- Match grain direction across all three layers: Cut the face wrap paper, grayboard core, and counter-liner so their machine grain runs parallel to the primary fold axis of the board or GM screen.
- Print and laminate the wrap and printed liner: Offset-print the face sheet (and printed counter-liner, if double-sided), allow ink to cure, and apply protective matte, gloss, or anti-scuff matte film before mounting.
- Coat and mount the face wrap: Apply water-based or hot-melt mounting adhesive evenly across the face wrap, position the grayboard core(s) onto the sheet, and press to eliminate trapped air.
- Miter corners and fold turn-in margins: Trim or nick the four corners of the 15–20 mm (0.591–0.787 in) wrap margin, fold the top, bottom, and side flaps over the grayboard edges, and press them flat onto the reverse face.
- Apply the counter-liner: Center the counter-liner on the back of the board, inset slightly from the outer perimeter so it covers the exposed grayboard center and overlaps the turned-in face wrap edges without overhanging the board edge.
- Press and condition: Stack finished boards under flat weight during adhesive curing so moisture from the wet glue equalizes evenly across both faces.
Sign-Off Criteria
Verify these physical checkpoints on wet proofs and pre-production board samples before full run sign-off:
- Turn-in coverage: All four edges are wrapped with 15–20 mm (0.591–0.787 in) margins, with tight corner tucks and zero exposed grayboard at edges or mitered corners.
- Counter-liner registration: The back liner sits squarely over the turned-in wrap seams with uniform edge reveal and no lifted edges.
- Panel flatness: Conditioned boards and GM screen panels lie flat on a level table without concave or convex bowing toward either face.
- Hinge and film integrity: Folding along scored hinges does not crack the wrap paper, split the surface film, or pull the counter-liner loose.
- Dark-area scuff resistance: High-TAC dark solids coated with anti-scuff matte film show no shiny rub streaks after normal handling.
Failure Modes
- Board cupping or bowing (warp): Caused by pairing a laminated face wrap with an unlaminated or lighter counter-liner, or by running the counter-liner grain perpendicular to the face wrap grain. Balance both sides in gsm, grain direction, and surface film.
- Corner dog-earing or exposed grayboard: Caused by wrap margins narrower than 15 mm (0.591 in) or insufficient corner-tuck pressure on 2.5–3 mm (0.098–0.118 in) cores. Maintain the 15–20 mm (0.591–0.787 in) turn-in allowance and miter corners to match core thickness.
- Turn-in seam telegraphing or liner lift: Caused by an overly thin counter-liner or dry adhesive along the perimeter where the liner bridges the turned-in wrap step. Use a ~120–157 gsm (~81–106 lb US Text) counter-liner with full perimeter adhesive wet-out.
- Hinge cracking along folds: Caused by grain running across the fold line or brittle film lamination over heavy ink coverage. Align paper grain parallel to the primary fold and keep TAC ≤280%–300%.
- Scuffing on dark artwork: Caused by standard matte or unlaminated varnish on dark fills. Specify anti-scuff matte film on dark-ground boards and GM screens.
Guides in this section
Parent guide Game Board and GM Screen Materials