Pocket Materials, Panel Specs, and Prepress
Because clear pockets sit over finished GM screen boards, pocket dimensions and bonding methods must accommodate both the rigid greyboard core and the wrapped hinge channels.
| Parameter | Manufacturing Specification | Condition / Impact |
|---|---|---|
| Pocket Film | Clear PP or clear PVC (gloss or anti-glare matte) | PVC welds cleanly via high-frequency (HF) sealing and lies flat; PP resists cracking along repeated flex zones and pairs with ultrasonic welding or pressure-sensitive adhesive. |
| Core Greyboard | 1.5 mm (0.059 in), 2.0 mm (0.079 in), 2.5 mm (0.098 in), or 3.0 mm (0.118 in) | Thicker 2.5–3.0 mm (0.098–0.118 in) cores resist bowing from pocket adhesive tension better than 1.5 mm (0.059 in) boards. |
| Wrap Margin | 15–20 mm (0.591–0.787 in) | Printed liner wraps around the greyboard edges and across the hinge channels before pockets are applied. |
| Stepped Margin | Pocket outer seam set back from every hinge channel and outer panel edge | Keeps the rigid welded or bonded border strictly on the flat greyboard face, clear of the folded wrap trough. |
| Insert Stock Range | 80–120 gsm (Text weight) or 200–300 gsm (Cover weight) | US Text LB is measured on a 25 x 38 in (635 x 965 mm) basis sheet, whereas Cover LB is measured on a 20 x 26 in (508 x 660 mm) basis sheet; heavier cover-weight sheets require extra side clearance and a thumb notch for removal. |
| Underlying Wrap Print | CMYK + separate spot layers, >= 300 DPI, 3 mm (0.118 in) bleed per side, >= 3 mm (0.118 in) safety | Supply AI, PDF, or PSD in PDF/X-1a or PDF/X-4 with outlined or embedded fonts, 100% K fine text, rich black (C40–60 M30–40 Y30–40 K100), and TAC <= 280%–300%. |
| Surface Finish | Anti-scuff matte lamination on dark underlying wraps | Prevents dark ink abrasion when sheets slide in and out and reduces glare under overhead lighting. |
- Top-loading vs. side-loading orientation: Top-loading pockets allow sheet swaps without folding the screen, while side-loading pockets opening toward the outer edges or center channels rely on friction and the closed fold to retain sheets during transport.
- Thumb notches and corner reliefs: Die-cut half-moon thumb notches at the open edge let players grip flush-cut reference sheets without prying the pocket lip open.
Production Steps
- Print and wrap the base screen: Print the interior and exterior panel wraps with 3 mm (0.118 in) bleed per side and 15–20 mm (0.591–0.787 in) wrap margins, apply anti-scuff matte or gloss lamination, and mount onto the 1.5–3.0 mm (0.059–0.118 in) greyboard panels with open hinge channels.
- Form and weld the clear pockets: Die-cut the clear PP or PVC blanks with any required thumb notches, then seal three perimeter edges using HF welding (for PVC), ultrasonic welding (for PP), or narrow-width transfer adhesive, leaving one loading edge open.
- Register and bond to the flat panel face: Position each pocket inside a registration jig aligned to the individual greyboard panel edges, maintaining a stepped setback from all hinge channels and outer bevels so the pocket never bridges a fold.
- Press and cure: Apply flat, even pressure across the bonded perimeter until the adhesive sets, ensuring the pocket lies flush against the laminated interior wrap without trapped air pockets.
Sign-Off Criteria
- Full-arc hinge articulation: Panels fold completely closed and open flat to their standing angles without the pocket edge contacting, pinching, or lifting inside any hinge channel.
- Smooth sheet insertion and removal: Reference sheets at the target gsm (whether lighter Text LB or stiffer Cover LB stock) slide fully to the bottom seam without corner catching, bowing, or splitting the side welds.
- Flat panel lay: Bonded panels remain flat without inward cupping or warp caused by uneven film tension on the interior face.
- Optical clarity and seam integrity: Perimeter bonds show uniform contact with no adhesive squeeze-out into the pocket cavity, minimal glare or Newton rings over underlying artwork, and clean thumb-notch cuts.
Failure Modes
- Hinge binding and seam peel: Extending a pocket too close to or across a hinge channel forces the stiff perimeter weld to bend during folding, which prevents the screen from closing flat and peels the bond off the wrap.
- Sheet buckling and split seams: Undersized internal pocket width or adhesive bleeding into the cavity traps the inserted sheet, bowing the reference page and splitting the side welds when forced.
- Panel warp on thin cores: High-shrinkage adhesive or heavy PVC film applied to one face of a 1.5 mm (0.059 in) greyboard panel pulls the board concave; stepping up to 2.0–3.0 mm (0.079–0.118 in) greyboard and balancing wrap tension counters this pull.
- Newton rings and ink scuffing: Smooth gloss pockets pressed tight against gloss-laminated wraps trap optical interference rings and abrade dark artwork during repeated swaps; pairing anti-scuff matte panel lamination with matte or lightly textured pocket film eliminates both effects.
Parent guide GM Screen Construction