This construction changes when:
- Full-panel magnetic coverage vs. strip rail: A narrow initiative rail along the top edge allows a localized ferrous strip, whereas full-height tracker grids require a larger sheet inset from all four panel edges.
- Magnet strength vs. surface separation: Heavy resin or acrylic magnetic tokens need a ferrous layer directly beneath the printed wrap, while light magnetic strips tolerate a thin protective liner or heavier matte film.
- Panel thickness and weight: Adding steel or iron-filled interlayers increases panel mass and stiffness, which requires matching greyboard caliper and hinge-channel spacing so folded panels still lie flat.
Core Specifications and Structural Stack
Magnetic-receptive GM screen panels are built around rigid greyboard cores wrapped in printed paper, with the ferrous layer seated strictly inside the non-folding panel footprint.
| Component / Parameter | Specification |
|---|---|
| Core board caliper | Greyboard 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) |
| Wrap turn-in margin | 15–20 mm (0.591–0.787 in) folded onto the reverse face |
| Printed wrap bleed & safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety from edges and hinge lines |
| Artwork & color setup | CMYK with separate spot layers, ≥300 DPI, TAC ≤280%–300% |
| Black & fine text | 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100 |
| Prepress files | AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts |
| Surface finish | Anti-scuff matte lamination for dark artwork and frequent token sliding |
- Ferrous interlayer placement: Die-cut or shear the ferrous sheet (galvanized steel, tinplate, or flexible iron-polymer receptive sheet) smaller than the greyboard panel so a continuous greyboard perimeter frames the metal. Never bridge a hinge channel with the ferrous layer.
- Flush-face compensation: Because even thin metal creates a step under tensioned paper, either recess the ferrous zone into a multi-ply greyboard stack (for example, a thinner base ply laminated to a windowed top ply) or pair a flexible iron-receptive sheet with a compensating filler sheet across the non-magnetic area of the panel.
- Hinge channel clearance: Leave the hinge gap clear of metal and keep the wrap safety margin at least 3 mm (0.118 in) away from fold lines so tracker grid borders do not visually drift across the crease.
Production Steps
- Die-cut cores and ferrous inserts: Cut the greyboard panels to final size and shear or die-cut the ferrous tracker inserts with clean, burr-free edges. If using a stepped or windowed core to keep the face flush, laminate the backing greyboard ply to the windowed frame ply first.
- Bond the ferrous zone: Laminate the ferrous sheet into its designated panel zone using a high-tack contact or flexible PVA/hot-melt adhesive suitable for metal-to-board bonding. Press evenly so no air pockets remain beneath the metal.
- Print and finish the outer wrap: Print the outer wrap sheet in CMYK (plus any separate spot layers) at ≥300 DPI, apply anti-scuff matte lamination if the design uses dark artwork or heavy token movement, and trim with the 15–20 mm (0.591–0.787 in) turn-in margin intact.
- Mount and turn in: Align the printed tracker graphics to the embedded ferrous zone, laminate the wrap across the panel face and hinge channels, and fold the 15–20 mm (0.591–0.787 in) wrap margin cleanly onto the back.
- Channel creasing and counter-lining: Press the wrap into each hinge channel with a heated or shaped creasing rule, then mount the interior liner sheet over the back turn-ins to seal the edges and balance board warp.
- Flatness curing: Stack finished screens under even weight until adhesive moisture equalizes, preventing the metal-backed zones from bowing relative to adjacent panels.
Sign-Off Criteria
- Hinge articulation: Every panel folds smoothly through its full range without spring-back resistance, metal edge catch, or paper cracking along the hinge crease.
- Surface flushness: Under raking light, the transition between the ferrous tracker zone and the surrounding greyboard shows no visible ridge, step, or adhesive ripple through the printed wrap.
- Graphic-to-metal registration: Magnetic tokens snap cleanly to the printed initiative slots, confirming the embedded ferrous sheet aligns with the artwork's safety zone.
- Token retention: Test tokens hold position vertically when the screen stands upright and slide without scuffing or peeling the surface lamination.
- Warp and edge seal: Wrapped turn-ins of 15–20 mm (0.591–0.787 in) sit flat beneath the liner with zero edge lift, and assembled panels rest flat without twisting.
If the finished product includes loose magnets or targets users in age-regulated categories, compile material declarations and arrange EN 71 toy safety assessment and testing records for the complete screen and magnet assembly before release.
Concrete Failure Modes
- Metal bridging the hinge channel: Extending the ferrous sheet into or across a fold gap locks the joint, causing the screen to spring open, crease unevenly, or tear the wrap paper after repeated folding.
- Edge telegraphing through the wrap: Mounting a rigid metal strip directly onto solid greyboard without a recess or compensating filler creates a raised step that catches light, wears prematurely at the seam, and shifts printed lines.
- Differential warp and delamination: Rigid metal expands and contracts differently from greyboard and paper; insufficient adhesive coverage or unbalanced counter-lining causes panels to bow or bubbles to form over the tracker zone.
- Burred metal edges cutting the wrap: Unfinished sheared steel corners or raised burrs puncture the paper wrap during pressing or wear through the lamination during handling.
- Weak magnetic hold: Burying the ferrous layer behind an extra thick board ply or oversized film stack increases the air gap to the magnet, causing vertical tokens to slip down the tracker rail.
Parent guide GM Screen Construction