When a coin design relies on flat fields and crisp, shallow lettering, cold striking is typically the better fit; see Metal Coin Casting and Striking for the full comparison between casting and striking. Choose centrifugal spin-casting in rubber molds for lower-volume runs, multi-cavity flexibility, or deeper undercuts, and choose steel-cavity die-casting for higher-volume runs that require tighter dimensional repeatability and crisper edge definition. Tooling and component minimums follow project and partner manufacturing requirements.
Specifications and Tooling Structure
- Material: Molten zinc alloy formulated for fluid cavity fill, high-relief detail retention, and substantial hand weight without requiring high-tonnage coining presses.
- Relief and Rim Geometry: Supports multi-level 3D sculptural relief, stepped or beveled rims, and undercut contours that cannot release from rigid striking dies.
- Pierced-Coin Tooling: Internal apertures and center holes are formed directly in the mold using core pins or shut-off bosses that block molten metal flow, avoiding secondary punching stress.
- Parting Line and Gating: Two-part (or multi-part) mold cavities meet along a defined parting line at the rim perimeter, with feed gates and air vents positioned on non-focal edge segments for clean removal.
- Draft Angles: Vertical relief walls and pierced-hole interiors require slight draft angles so solidified castings release cleanly from the mold without galling or tearing.
Production Steps
- Master Pattern and Mold Creation: Build a 3D master model incorporating draft angles and alloy shrinkage allowance, then form the vulcanized rubber mold (centrifugal casting) or machine the hardened steel die (die-casting) with core pins for any pierced holes.
- Gating and Venting: Cut or machine sprues, runners, feed gates, and air vents so molten zinc alloy reaches deep sculptural pockets and thin rim transitions before solidifying.
- Molten Zinc-Alloy Casting: Spin or inject molten zinc alloy into the closed cavity, packing metal into fine 3D recesses and around pierced-hole cores.
- De-molding and Gate-Sprue Trimming: Extract the solidified casting tree or individual coin blanks, then break or trim the gates and sprues close to the outer rim contour.
- Parting-Line Cleanup and Deburring: Grind, file, or barrel-tumble the coin perimeter and pierced-hole edges to remove parting-line flash, gate stubs, and sharp burrs before plating or antique finishing.
Sign-Off Criteria
- Cavity Fill: High-relief peaks, stepped rims, and recessed textures are fully formed with no voids or cold-shut seams.
- Rim and Parting-Line Finish: Gate stubs are trimmed flush and the parting line blends smoothly around the outer edge without flat spots or raised flash.
- Pierced-Hole Integrity: Center holes and internal cut-outs are properly centered, free of thin metal webbing, and smooth along the inner wall.
- Structural Soundness: Thin web sections around pierced holes show no stress cracks, and finished coins sit cleanly in any paired trays or inserts.
- Regulatory Documentation (When Applicable): For games or components subject to toy-safety rules, maintain applicable assessment records, small-parts and edge evaluations, and chemical/heavy-element test documentation in accordance with the EU Toy Safety framework.
Failure Modes
- Incomplete Fill and Cold Shuts: Molten zinc alloy solidifies before reaching high-relief peaks or thin stepped rims, leaving rounded or missing detail due to insufficient venting, undersized gates, or low casting temperature.
- Heavy Parting-Line Flash or Mold Mismatch: Worn or misaligned mold halves allow metal to seep along the seam or create an offset step around the rim and pierced holes that tumbling alone cannot correct.
- Gate-Trimming Scars: Gates placed over detailed rim features or broken off aggressively leave gouges, flat spots, or protruding nubs on the coin edge.
- Pierced-Hole Webbing or Core Tear: Misaligned core pins leave thin flash bridging the center hole, while insufficient draft on a core pin tears the inner hole wall during ejection.
- Subsurface Porosity: Trapped air in deep sculptural recesses forms pinholes beneath the skin that later blister or pit during plating and surface finishing.
Parent guide Metal Coin Casting and Die-Striking Construction