Specifications and Geometry Limits
- Coined relief height limits: Hydraulic striking compresses and displaces solid metal rather than filling a molten cavity. Cold metal resists deep vertical flow, so die-struck construction is suited to 2D stepped levels and low-3D relief rather than high-relief sculptural forms. Deeper relief requires higher hydraulic tonnage, harder die steel, and wider draft angles on vertical walls so the struck blank releases cleanly without tearing.
- 2D and low-3D geometry: Flat recessed fields, raised flat-top lettering, crisp bevels, and fine linework reproduce sharply because upper and lower dies compress the blank between parallel faces. Minimum line widths and groove spacing must leave enough steel mass on the die face to withstand repeated hydraulic impacts without chipping.
- Blank annealing: Rolled metal sheet work-hardens during slitting and blanking, which resists plastic flow into fine die recesses. Partner toolmakers anneal blanks—heating them to a controlled recrystallization temperature and cooling them before pressing—to soften the grain structure so metal fills sharp corners and raised rims at lower press tonnage without splitting. Multi-strike coins with deeper low-3D relief may require intermediate annealing between strikes.
- Blank dimensions and edge profile: Blanks are punched from solid sheet or strip (such as brass, bronze, copper, or iron) to maintain uniform thickness across the coin face and predictable stack height inside game trays. Specify coin diameter and thickness in
mm(in) and unit or batch weight inkg(lb) so insert cavities and shipping cartons match actual tolerances. Edge profiles—smooth, chamfered, or reeded—depend on whether the blank is struck inside a retaining collar or trimmed after striking.
Production Steps
- Vector and relief separation: Prepare clean 2D vector artwork with closed paths separating raised metal, recessed fields, and stepped low-3D bevels. Supply distinct layers for obverse, reverse, collared edge reeding (if used), and plating or antique finish zones.
- Die engraving and collar setup: Specialist manufacturing partners machine and harden the upper and lower steel dies from the approved vector or low-3D relief file, polishing flat fields and adding a retaining collar when reeding or tight diameter control is required.
- Blanking and annealing: Solid metal blanks are stamped from rolled strip to the target diameter and thickness, deburred, and annealed to restore ductility prior to pressing.
- Hydraulic striking: Each annealed blank is seated between the dies and compressed under hydraulic pressure so metal flows into the engraved recesses while the collar (when present) restrains outward spread and forms the rim.
- Trimming, tumbling, and finishing: Excess flash on uncollared strikes is trimmed; coins are tumbled or brushed to clean edges, plated or patinated for contrast, and sealed with a protective clear coat when specified.
- Compliance and packaging records (where applicable): When coins are included in children's games or toy-graded tabletop products, schedule EN 71 assessment and testing (including small-parts and chemical migration checks) with an accredited laboratory under the European Commission toy safety framework. Maintain material and packaging declarations where regional rules such as VerpackG or Triman apply to the finished retail box.
Sign-Off Criteria
- Pre-production sample review: Confirm obverse-to-reverse alignment (medallic or coin rotation), sharp flat lettering, complete fill on raised rims, and consistent recessed contrast.
- Dimensional and weight check: Verify coin diameter and thickness in
mm(in) and pack weight inkg(lb) against tray and box insert clearances so stacks sit flat without binding. - Edge and surface inspection: Confirm clean rims free of sharp burrs, parting-line flash, radial stress cracks, or galling marks along vertical relief walls.
Concrete Failure Modes
- Incomplete fill (short strike): Under-annealed blanks, insufficient hydraulic tonnage, or overly deep relief prevents metal from reaching the top of raised lettering and rims, leaving soft, rounded high points.
- Rim cracking and radial splits: Work-hardened blanks or excessive perimeter relief stretches the metal beyond its ductility limit during compression.
- Die chipping and blurred fine lines: Excessively thin raised walls or acute internal angles on the die steel fracture under repeated strikes, transferring rough burrs onto subsequent blanks.
- Off-center strike and heavy flash: Poor blank seating or omission of a retaining collar produces uneven rim widths, slight oval distortion, and excess perimeter flash that requires heavy trimming.
- Galling and surface drag: Steep vertical relief walls without sufficient draft angle or die lubrication tear metal along the sidewalls as the dies retract.