Choose collar-struck reeding or knurling when crisp, repeating perimeter texture is central to the piece and tooling budgets support a grooved retaining collar. Choose a smooth or chamfered edge when using two-piece spin casting or die casting, because a cast perimeter carries a horizontal mold parting seam that cannot be ground cleanly out of fine vertical grooves. For alloy selection, blank thickness, and core forming trade-offs, see metal coin casting and striking.
Edge Profiles and Forming Conditions
| Edge Profile | Primary Forming Method | Parting-Seam Behavior | Plating and Finish Interaction | Best-Fit Conditions |
|---|---|---|---|---|
| Reeded (vertical grooves) | Collar-struck | No perimeter parting seam; collar forms grooves during the strike | High-contrast antique wash settles in troughs; sharp groove peaks can build thicker plating | Struck coins needing tactile grip, easy stacking alignment, and classic perimeter definition |
| Knurled (angled or diamond texture) | Collar-struck or post-strike rolled | No mold seam on struck blanks; rolled knurling can displace metal at rim corners | Textured facets catch light and hold patina; deep pockets require thorough rinsing before plating | Thick-rimmed tokens or coins where non-slip handling and ornamental side texture are priorities |
| Chamfered (beveled rim) | Die-formed on struck blanks or ground on cast blanks | Ideal for cast coins: beveling blends the horizontal parting seam during cleanup | Softens high-current-density rim corners, reducing plating burn and chipping | Cast coins requiring clean seam removal, or struck coins needing snag-free handling |
Three physical conditions govern edge selection:
- Forming process: In coining, a retaining collar surrounds the blank so obverse and reverse dies push metal radially into the collar's internal grooves in one stroke. In casting, liquid metal fills a two-part cavity, leaving a raised parting line around the circumference that must be abraded away.
- Rim thickness and groove pitch: Shallow, wide-pitched reeds eject cleanly and accept uniform electroplating. Narrow, deep grooves require higher ejection force and risk uneven plating coverage between the groove peak and root.
- Handling and surface wear: Unchamfered 90-degree rim corners concentrate impact and electroplating current, making them prone to rough buildup or edge chipping during tumbling and tabletop play.
Job-Specific Production Steps
Collar-Struck Reeded and Knurled Edges
- Collar machining: Cut the internal reed or knurl pattern into a hardened retaining collar matched to the blank diameter and target stroke depth.
- Blank seating and strike: Center the blank inside the collar cavity so radial metal flow fills the perimeter grooves completely without overflowing between the die face and collar wall.
- Vertical ejection: Push the struck coin straight out of the collar to preserve groove walls without smearing the reed crests.
- Rim deburring and tumbling: Run struck coins through light media tumbling to knock down micro-burrs at the face-to-edge transition before electroplating and patina application.
Cast Coin Edges and Parting-Seam Removal
- Mold separation and gate trim: Remove cast coins from the two-piece mold and shear or clip the feed gate vestige from the perimeter.
- Parting-seam grinding: Grind the horizontal mold seam flush around the full circumference using progressive abrasive belts or wheels.
- Chamfering (when specified): Cut or grind a consistent bevel along the upper and lower rim corners to remove sharp edges left by flat perimeter grinding.
- Vibratory tumbling and plating: Tumble ground blanks in ceramic or steel media to erase directional grinding scratches, then clean, electroplate, and apply antique wash or protective lacquer.
Sign-Off Criteria
Inspect pre-production samples under raking light across the entire circumference before approving bulk finishing:
- Struck reeding and knurling: Uniform groove depth and spacing around the full perimeter, clean tooth crests with no drag marks, and consistent patina or plating coverage at the groove roots.
- Cast and chamfered edges: Complete removal of the mold parting seam with no raised ridge, hairline shadow, or coarse abrasive scratches telegraphing through the plated finish.
- Circularity and feel: Even rim contour with no flat spots from over-grinding and no sharp wire burrs at the face-to-edge transition.
Concrete Failure Modes
- Parting-seam ghosting: Incomplete seam grinding or coarse belt marks on cast edges remain visible as a dull band or hairline ridge after electroplating.
- Perimeter flat-spotting: Heavy-handed manual grinding to clear a thick mold flash flattens an arc of the edge, making the coin visibly out-of-round.
- Smeared or torn reeds: Galling, tight collar clearance, or misaligned ejection drags across the groove crests and tears the perimeter teeth.
- Starved or bridged plating: Overly deep, narrow knurling or reeding traps processing solution or receives thin plating in the troughs while building rough deposits on the peaks.
- Sharp rim burrs: Omitting a light chamfer or post-grind tumble leaves a cutting edge that snags fingers, card sleeves, or storage trays.
Parent guide Metal Coin Casting and Die-Striking Construction