Board-Gauge Specifications
| Core Gauge | Inch Equivalent | Typical Applications | Stiffness & Shear Behavior | Die-Cutting Pressure |
|---|---|---|---|---|
| 1.5 mm | 0.059 in | Standard tokens, small chits, dense counters | Moderate stiffness; cleanest vertical shear on tight curves | Low to moderate platen tonnage |
| 2.0 mm | 0.079 in | Standard game tiles, medium tokens, player boards | High stiffness-to-thickness ratio; clean shear with minimal bevel | Moderate platen tonnage |
| 2.5 mm | 0.098 in | Large modular tiles, heavy chits, long track pieces | Rigid against bowing; noticeable edge bevel on tight radii | High platen tonnage |
| 3.0 mm | 0.118 in | Structural punch-outs, slotted standees, heavy boards | Maximum rigidity; highest edge-compression and beveling risk | Maximum platen tonnage |
Density, Caliper, and Finished Thickness
- Stiffness vs. caliper: Bending stiffness scales rapidly with thickness, so stepping from 1.5 mm (0.059 in) to 2.0 mm (0.079 in) substantially increases rigidity. High-density greyboard (tightly compressed recycled pulp fibers) resists denting and corner mushrooming better than lower-density chipboard of the same caliper.
- Edge shear and beveling: As core caliper increases toward 2.5–3.0 mm (0.098–0.118 in), the steel-rule blade must displace more compressed fiber before reaching the cutting plate. Thicker cores produce a slightly more tapered edge profile unless paired with high-density stock and sharp, tall-profile steel rules.
- Liner and film stack-up: Printed wrap liners—typically 80–120 gsm art paper (approximately 54–81 lb US Text on a 25 x 38 in basis sheet, distinct from Cover LB which uses a 20 x 26 in basis sheet)—add about 0.08–0.13 mm (0.003–0.005 in) per face. Double-sided film lamination adds another 0.03–0.05 mm (0.001–0.002 in) to the total finished board caliper.
- Layout and box clearances: Maintain a 3–4 mm (0.118–0.157 in) die gap between adjacent punchboard pieces, 3 mm (0.118 in) bleed per side on artwork, and a 15–20 mm (0.591–0.787 in) wrap margin on wrapped edges. Size the outer game box with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance to accommodate the total laminated caliper of all punchboard frames.
Production Steps
Card Deck Press produces custom punchboards through specialist tabletop manufacturing partners following five controlled stages:
- Core conditioning: Select the 1.5, 2.0, 2.5, or 3.0 mm (0.059, 0.079, 0.098, or 0.118 in) high-density greyboard sheets and acclimatize them to pressroom humidity to limit post-lamination curl.
- Offset printing and mounting: Print the face and back liners (CMYK, >=300 DPI, PDF/X-1a or PDF/X-4), apply any protective film, and laminate both liners onto the greyboard core with balanced adhesive tension.
- Pressing and curing: Stack and weight the laminated boards during adhesive cure so moisture equalizes evenly across both faces.
- Steel-rule die-cutting: Mount the custom die with 3–4 mm (0.118–0.157 in) spacing between cut lines and calibrated nicking bridges to hold tokens in the frame. Set platen impression depth and tonnage to match the core's density and caliper.
- Inspection and boxing: Check punch-out release, edge shear cleanly, and total frame stack height against box tolerances before packing.
Sign-Off Criteria
- Finished caliper: Measured total thickness (greyboard core + front/back liners + film) falls within target tolerance and clears the 1.5–3 mm (0.059–0.118 in) box stack-height allowance.
- Clean punch-out release: Tokens separate from nicking bridges under light thumb pressure without tearing the back liner or pulling surface ink.
- Vertical edge shear: Cut edges show uniform fiber separation along the steel-rule path without crushed top-sheet shoulders or delaminated paper edges.
- Sheet flatness: Unpunched frames lie flat without directional bowing across the sheet width or length.
Concrete Failure Modes
- Edge crushing and mushrooming: Low-density greyboard or excessive platen pressure compresses the top edge before the blade shears through, leaving rounded, soft shoulders on 2.5–3.0 mm (0.098–0.118 in) tiles. Prevent this by specifying high-density greyboard and calibrating kiss-cut/through-cut impression depth.
- Back-liner tearing ("haloing"): Insufficient die-cutting pressure or oversized nicking bridges leave uncut fibers on the bottom liner, which rip paper away from the token back when punched. Increase platen tonnage at the die bed and minimize nick width.
- Frame bridge collapse: Placing cut lines closer than the 3–4 mm (0.118–0.157 in) minimum die gap causes the steel rules to pinch and fracture the narrow greyboard web between tokens. Enforce >=3–4 mm (0.118–0.157 in) gaps in the dieline layout.
- Board warping: Asymmetric moisture absorption or mismatched paper/film tension between the front and back faces pulls the core into a bow. Match liner weights on both sides and press sheets under weight during adhesive curing.
- Slotted-component bind: Cutting interlocking slots to the raw greyboard gauge without adding liner (0.08–0.13 mm / 0.003–0.005 in per face) and film (0.03–0.05 mm / 0.001–0.002 in) thickness causes standees and dividers to bind or split the slot edges during assembly. Size slot widths from the finished laminated caliper.
Parent guide Punchboard Materials and Paperboard Cores