For custom punchboards and wrapped game boards produced through specialist offset and tabletop manufacturing partners, use identical or matched-weight coated face sheets on both sides of 1.5–3 mm (0.059–0.118 in) greyboard, align paper grain consistently, and apply balanced protective coatings to both faces. This choice changes when a board uses a turned-edge wrap rather than a flush-cut punchboard—requiring 15–20 mm (0.591–0.787 in) wrap margins instead of 3–4 mm (0.118–0.157 in) die gaps—or when dark, high-coverage artwork requires anti-scuff matte lamination to prevent rub marks during handling. For broader core and substrate context, see punchboard materials.
Specifications and Tolerances
Specify all face sheets and wraps in gsm rather than US pound (lb) weights alone. US Text LB is measured on a 25 x 38 in (635 x 965.2 mm) basis sheet, whereas US Cover LB is measured on a 20 x 26 in (508 x 660.4 mm) basis sheet, so the same LB number represents a substantially heavier sheet in Cover LB than in Text LB.
| Component or Parameter | Specification | Imperial / Equivalent | Notes |
|---|---|---|---|
| Greyboard core thickness | 1.5 / 2.0 / 2.5 / 3.0 mm | 0.059 / 0.079 / 0.098 / 0.118 in | Core stiffness scales with thickness |
| Lighter wrap / liner stock | 80–120 gsm | ~0.08–0.13 mm (0.0031–0.0051 in) per sheet | Text-range coated stock for wraps and liners |
| Heavy face / cover stock | 200–300 gsm | Cover-range basis | Used when extra surface rigidity is required |
| Double-sided film lamination | +0.03–0.05 mm total | +0.0012–0.0020 in total | Applied symmetrically to balance moisture |
| Wrap margin (turned-edge) | 15–20 mm | 0.591–0.787 in | Folded over greyboard edges |
| Punchboard die gap | 3–4 mm | 0.118–0.157 in | Minimum clearance between die-cut tokens |
| Bleed per side | 3 mm | 0.118 in | Extends artwork past trim or die line |
| Safety margin | >=3 mm | >=0.118 in | Keeps critical text and art clear of cuts |
Prepress and Ink Limits
- File format: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts.
- Resolution and color: >=300 DPI, CMYK with separate spot layers where needed.
- Black builds and coverage: 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100 for solid dark areas; total area coverage (TAC) <=280%–300%.
- Surface finish: Anti-scuff matte lamination suits dark artwork with heavy rich-black coverage.
Thickness and Weight Formulas
Calculate total mounted board thickness and convert sheet or stack weights using plain-text formulas:
total_thickness_mm = greyboard_mm + front_face_mm + back_face_mm + film_mm
inches = mm / 25.4
weight_lb = weight_kg * 2.205
For example, a 10 kg stack of mounted sheets equals 22.05 lb (10 * 2.205), and a 2.0 mm (0.079 in) greyboard core determines the primary rigidity while balanced face sheets and film keep both sides dimensionally symmetrical. Boxed games and custom die tooling follow project and component minimums.
Production Steps
- Prepress setup and grain planning: Prepare PDF/X-1a or PDF/X-4 files at >=300 DPI with 3 mm (0.118 in) bleed and >=3 mm (0.118 in) safety margins. Orient both front and back face sheets so their paper grain runs in the same direction relative to the greyboard core.
- Offset printing and balanced coating: Print CMYK and spot layers within <=280%–300% TAC. Apply identical protective coatings or lamination (such as double-sided anti-scuff matte film) to both face sheets so neither side absorbs or releases ambient humidity faster than the other.
- Mounting and flat pressing: Apply adhesive evenly across the 1.5–3.0 mm (0.059–0.118 in) greyboard and laminate both face sheets. Stack and press the mounted boards under flat weight (measured in kg/lb across the pallet) until moisture equalizes and the adhesive cures.
- Edge wrapping or die cutting: For wrapped boards, fold the 15–20 mm (0.591–0.787 in) wrap margins cleanly around the greyboard edges. For punchboards, die-cut the cured sheets with 3–4 mm (0.118–0.157 in) gaps between adjacent tokens so the face paper does not bridge-tear.
Sign-Off Criteria
- Flatness after curing: Mounted sheets lie flat without concave or convex bowing once removed from the press stack.
- Symmetrical construction: Front and back face sheets match in gsm weight, grain orientation, and lamination or coating type.
- Cut and wrap precision: All artwork and text sit >=3 mm (0.118 in) inside cut lines, punchboard die gaps hold 3–4 mm (0.118–0.157 in) without ragged fibers, and wrapped edges fully cover the 15–20 mm (0.591–0.787 in) turn-in zone.
- Surface durability: Dark rich-black areas (C40–60 M30–40 Y30–40 K100) show no scuffing or film lift along die-cut or folded edges.
Concrete Failure Modes
- Post-cut board curl: Caused by pairing different paper weights on the front and back faces, running face-sheet grain perpendicular to the opposing sheet, or laminating only one side. One face expands or contracts with humidity while the other stays locked, bowing the greyboard.
- Token edge peeling and delamination: Caused by die cutting before mounting adhesive has cured, insufficient adhesive near sheet perimeters, or brittle film lifting under blade compression along narrow 3–4 mm (0.118–0.157 in) die gaps.
- Wrap corner cracking or pull-back: Caused by wrap margins narrower than 15–20 mm (0.591–0.787 in), folding heavily inked paper (>300% TAC) against the grain, or using overly stiff cover-weight stock for tight edge turns.
- Scuffing on dark boards: Caused by running unlaminated or standard-finish dark solids (rich black C40–60 M30–40 Y30–40 K100) without anti-scuff matte film, leading to visible rub marks during die cutting, stacking, and packing.
Parent guide Punchboard Materials and Paperboard Cores