The production specification depends on three concrete choices:

  • Sleeve construction: Choose clear matte sleeves when card backs must remain visible or glare must be minimized; choose art-backed sleeves when uniform opaque backs, custom graphics, or dark full-bleed artwork are required.
  • Box construction: Choose a folding cardstock box (300–400 gsm) for single-deck retail kits and lower unit weight; choose a wrapped rigid greyboard box (1.5–3 mm / 0.059–0.118 in) for multi-deck, heavy-sleeved, or collector kits.
  • Retail presentation: Choose a printed header card over a polybag for hanging pegboard displays; choose a die-cut window tuck box when the sleeved deck or divider tab must be visible in a rigid retail footprint.

Bill of Materials and Component Specifications

A complete companion kit BOM pairs partner-sourced sleeves with offset-printed dividers, a custom-sized deck box, and retail outer packaging. All cavity dimensions are derived from the target card's trim size plus sleeve allowances—never from bare card dimensions.

Component Material & Weight Spec Caliper / Thickness Sizing & Clearance Rules
Card Sleeves Partner-made clear matte film or printed art-backed film Two film walls per card plus perimeter weld seam Sized to target card trim plus insertion clearance; art backs require 3 mm (0.118 in) bleed per side
Deck Dividers 300–400 gsm cardstock (US Cover LB, 20 × 26 in / 508 × 660 mm basis sheet) or 0.30 mm (0.012 in) PVC 300 gsm: 0.28–0.31 mm (0.011–0.012 in); 350 gsm: 0.34–0.38 mm (0.013–0.015 in); 400 gsm: 0.40–0.44 mm (0.016–0.017 in); double-sided film adds 0.03–0.05 mm (0.001–0.002 in) Match outer sleeve width; R3–R3.5 mm (R0.118–R0.138 in) corner radius; tab height must clear sleeve top without hitting box lid
Deck Box (Folding) 300–400 gsm art/core cardstock (Cover LB) 0.28–0.44 mm (0.011–0.017 in) plus 0.03–0.05 mm (0.001–0.002 in) for double-sided film Internal cavity: 1.5–2.5 mm (0.059–0.098 in) width/height clearance; 1.5–3 mm (0.059–0.118 in) stack-height clearance
Deck Box (Rigid) 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard with wrapped paper Greyboard thickness plus 15–20 mm (0.591–0.787 in) wrap margin Same internal cavity clearances as folding boxes, measured after wrap turn-in
Retail Header / Window Pack 200–350 gsm cardstock (Cover LB) or 80–120 gsm (US Text LB, 25 × 38 in / 635 × 965 mm basis sheet) inner leaflet Header/window board: 0.20–0.38 mm (0.008–0.015 in); leaflet: 0.08–0.13 mm (0.003–0.005 in) per sheet Window cutout requires die setback from crease lines; header card includes hang-hole safety margin

Note on paper weight standards: Specify heavy dividers, folding boxes, and header cards in gsm alongside US Cover LB (20 × 26 in / 508 × 660 mm basis sheet). Use US Text LB (25 × 38 in / 635 × 965 mm basis sheet) only when specifying thin 80–120 gsm pack-in leaflets or instruction sheets.

Sleeved-Stack Sizing Formulas

Because sleeve film adds two wall thicknesses per card and traps slight air volume between cards, calculate internal box dimensions from a physical sleeved stack rather than bare card caliper alone:

Internal Box Width  = Outer Sleeve Width + 1.5 to 2.5 mm (0.059 to 0.098 in)
Internal Box Height = Max(Outer Sleeve Height, Divider Tab Height) + 1.5 to 2.5 mm (0.059 to 0.098 in)
Internal Box Depth  = Measured Sleeved-Deck Stack Height + (Divider Count * Divider Caliper) + 1.5 to 3.0 mm (0.059 to 0.118 in)

For reference, common bare card cores range from 300 gsm art/blue core at 0.28–0.31 mm (0.011–0.012 in), 310 gsm black-core linen at 0.30–0.32 mm (0.012–0.013 in), and 330 gsm black core at 0.32–0.34 mm (0.013 in), up to 400 gsm at 0.40–0.44 mm (0.016–0.017 in) or 0.30 mm (0.012 in) PVC. Double-sided film lamination on cards adds 0.03–0.05 mm (0.001–0.002 in) per card before sleeving.

Prepress and Print Specifications

All printed components—art-backed sleeves, cardstock dividers, deck boxes, and retail header or window cartons—follow offset prepress standards:

  • File formats: Supply AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
  • Color and resolution: CMYK with separate spot layers for white underbase (on clear/metallic sleeve film), Pantone spots, or foil/varnish masks at ≥300 DPI.
  • Black ink and coverage: Set fine text to 100% K. Use rich black (C40–60 M30–40 Y30–40 K100) for large dark solids, keeping total area coverage (TAC) at ≤280%–300%.
  • Bleed and safety: Extend artwork 3 mm (0.118 in) beyond trim on all sides. Keep critical text and graphics ≥3 mm (0.118 in) inside trim, increasing to ≥4–5 mm (0.157–0.197 in) on bordered sleeve backs or divider faces.
  • Surface finishes: Apply anti-scuff matte lamination on dark deck box and divider artwork to prevent rub marks during retail transit. Avoid thick lamination on components paired with gilded edges, as thick film can conflict with edge gilding.

Production Steps and Tooling Minimums

Standard offset card and divider components start at 200 decks (usual tiers: 200, 300, 500, and 1,000+), while boxed kits, custom sleeve runs, and dedicated die-cutting or rigid-box tooling follow project and component minimums.

  1. Lock target card trim and sleeve style: Confirm the exact card dimensions to be protected and select clear matte or art-backed sleeves.
  2. Measure sleeved-stack height: Sleeve the full target card count using partner sample sleeves, compress lightly to simulate packed tension, and measure total stack height in mm and in.
  3. Generate dielines: Build the divider die (with R3–R3.5 mm / R0.118–R0.138 in corners) and deck box dieline using the sleeved-stack formulas above. If using a rigid greyboard box, verify the 15–20 mm (0.591–0.787 in) wrap margin on all outer faces.
  4. Prepress and proofing: Export PDF/X-1a or PDF/X-4 files with separate spot/dieline layers and verify TAC ≤280%–300%.
  5. Component manufacturing: Specialist manufacturing partners produce the sleeves while offset presses run the dividers, deck boxes, and retail headers or window cartons.
  6. Kitting and retail pack-out: Collate the sleeved pack, dividers, and deck box into the polybag with stapled header card or into the window carton.

Sign-Off Criteria

Before approving bulk production or shipment, verify each kit against four physical gates:

  • Sleeved-fit check: Insert a full sleeved deck plus all cardstock dividers into the production box sample. Confirm the deck slides in without catching and sits within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) depth clearance windows.
  • Lid and tab clearance: Close the box lid completely and verify divider tabs do not bend or prevent the tuck flap or rigid lid from seating flush.
  • Print and finish inspection: Check dark solids for scuffing (confirming anti-scuff matte performance), verify 100% K fine text sharpness, and inspect window film adhesion along die-cut frames.
  • Weight and pack verification: Measure and record finished unit kit weight and master carton gross weight in both kg and lb on the final packing specification.

Regulatory and Packaging Compliance Records

When kits are distributed into regulated markets, maintain the applicable assessment, registration, and labeling records for the target jurisdictions:

  • Toy safety assessment: Where kits are marketed or intended for use by children under 14, maintain applicable assessment and testing documentation per EU Toy Safety (EN 71).
  • Packaging producer responsibility (Germany): Register retail packaging (boxes, polybags, header cards) and report material weights per Zentrale Stelle Verpackungsregister (VerpackG).
  • Sorting and recycling markings (France): Include required sorting symbols and material separation instructions on retail header cards and window cartons per French Triman and Info-tri rules.

Failure Modes

  • Box sized to bare cards instead of sleeved stack: Calculating internal box depth from bare card caliper omits two sleeve walls per card and trapped air, causing the lid to bulge or split at the seams.
  • Divider tabs colliding with box closure: Designing divider tabs without accounting for sleeve height plus 1.5–2.5 mm (0.059–0.098 in) lid clearance causes tabs to fold over when the tuck flap or rigid lid closes.
  • Ink setoff and scuffing on dark boxes: Exceeding 280%–300% TAC or omitting anti-scuff matte lamination on dark rich-black boxes and dividers leads to visible rub marks inside window packs and transit cartons.
  • Window cutout too close to crease lines: Placing a retail window die-cut within the score-to-fold margin weakens the carton corner, causing the window frame to tear during kitting.
  • Asymmetric borders on art-backed sleeves or dividers: Using less than 4–5 mm (0.157–0.197 in) safety margin on bordered backs exposes die-cut shift and makes borders appear uneven.