Standard offset sheet runs start at 200 units (usual tiers 200 / 300 / 500 / 1,000+), while bundled kits with custom sleeves, rigid boxes, or partner-sourced writing tools follow project and component minimums.


Bill of Materials & Component Specifications

A complete replacement kit consists of four functional layers: the writable surface, the rigid backer, the partner-sourced writing tool, and the outer retail wrap.

1. Writable Pad & Scoreboard Substrates

Component Type Stock & Weight Basis Sheet Distinction Caliper Surface & Edge Spec
Tear-off scorepad sheets 80–120 gsm uncoated offset paper 54–81 lb Text (25 × 38 in / 635 × 965.2 mm basis) 0.08–0.13 mm (0.0031–0.0051 in) per sheet Uncoated tooth for graphite pencil and ballpoint ink; top- or side-edge padding glue
Card-weight dry-erase boards 350–400 gsm art stock 130–148 lb Cover (20 × 26 in / 508 × 660.4 mm basis) 0.34–0.38 mm (0.0134–0.0150 in) at 350 gsm; 0.40–0.44 mm (0.0157–0.0173 in) at 400 gsm Double-sided gloss dry-erase film (+0.03–0.05 mm / 0.0012–0.0020 in); R3–R3.5 mm (0.118–0.138 in) corners
Plastic dry-erase boards Solid PVC N/A (extruded plastic) 0.30 mm (0.0118 in) Washable waterproof surface; R3–R3.5 mm (0.118–0.138 in) corners
Rigid wrapped scoreboards 1.5, 2, 2.5, or 3 mm greyboard + art wrap 200–300 gsm wrap (74–111 lb Cover, 20 × 26 in basis) 1.5–3 mm (0.059–0.118 in) core + wrap 15–20 mm (0.591–0.787 in) wrap margin; gloss dry-erase film on face
  • Trim sizing: Size pad and board trim dimensions to fit the target table footprint or existing core-game box cavity. Because scorepads and tally boards do not use a universal card format, define exact trim width and height in millimetres and inches (Inches = Millimetres / 25.4) based on the number of player columns, row height for handwriting, and whether writing tools pack alongside or on top of the pad.
  • Stack height and weight calculation (plain-text formulas):
    • Pad Stack Height (mm) = (Sheet Caliper (mm) * Sheet Count) + Backer Thickness (mm)
    • Stack Height (in) = Stack Height (mm) / 25.4
    • Paper Weight per Pad (kg) = (GSM / 1000) * (Width (mm) / 1000) * (Height (mm) / 1000) * Sheet Count
    • Weight (lb) = Weight (kg) * 2.2046

2. Chipboard Backers

  • Pad backers: Glue the bottom sheet of a tear-off pad to a rigid greyboard backer (1.5 mm / 0.059 in, 2 mm / 0.079 in, 2.5 mm / 0.098 in, or 3 mm / 0.118 in) when players write while holding the pad in hand. For pads used exclusively on a flat table or packed into tight tuck boxes, a 300–400 gsm (111–148 lb Cover, 20 × 26 in basis) board backer reduces stack height and unit weight.
  • Retail backing cards: When bundling loose dry-erase boards and markers in a polybag or shrink wrap without a box, include a 350–400 gsm (130–148 lb Cover) or 1.5 mm (0.059 in) greyboard stiffener behind the kit so tensioned wrap does not bow the contents.

3. Partner-Sourced Writing Tools

  • For tear-off pads: Mini wooden pencils (hexagonal or round barrels, pre-sharpened or unsharpened) pair with 80–120 gsm uncoated stock without drying time or cap-loss issues.
  • For dry-erase boards: Fine-tip dry-erase markers (with integrated cap erasers or paired with a small felt/foam wiper) are required for gloss-laminated or PVC boards.
  • Packaging clearance: Writing tools create localized thickness spikes. When kits are housed in a paper sleeve, tuck box, or two-piece rigid box, allow 1.5–2.5 mm (0.059–0.098 in) clearance across width and height and 1.5–3 mm (0.059–0.118 in) clearance for total stack height (measured over the marker barrel or bundled pencil diameter, unless recessed in a die-cut insert).

4. Retail Wraps & Sleeves

  • Shrink wrap: Holds a pad, backing board, and loose pencils/markers together as a single retail SKU. Specify low-tension heat shrink when wrapping thin pads without a rigid backer.
  • Printed belly bands and sleeves: Wrap around the pad and tool bundle, leaving the pad edges visible while providing barcode, branding, and component callouts. Use 200–300 gsm (74–111 lb Cover, 20 × 26 in basis) art stock; apply anti-scuff matte lamination on dark-ink sleeves to resist transit rubbing.

Prepress & Print File Requirements

  • File formats: Submit print-ready files in AI, PDF, or PSD, exported to PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
  • Color & ink limits: Build artwork in CMYK with separate spot layers for custom Pantone colors or finish masks (such as selective dry-erase zones vs. matte borders). Keep Total Area Coverage (TAC) at ≤280%–300%.
  • Resolution: Minimum 300 DPI at 100% print scale for all raster graphics.
  • Typography & grid lines: Set fine grid lines, score boxes, and small body text on scorepads to 100% K (black only) to prevent multi-plate registration blur. Use rich black (C40–60 M30–40 Y30–40 K100) only for large solid dark areas on sleeves or scoreboard borders.
  • Bleed & safety margins: Include 3 mm (0.118 in) bleed per side on all printed sheets, boards, and sleeves. Keep critical text and score-grid outer rules at least 3 mm (0.118 in) inside the trim line, increasing to ≥4–5 mm (0.157–0.197 in) on bordered backs or wrap-around sleeves.

Production Steps & Sign-Off Criteria

  1. Substrate & Tool Pairing Sign-Off: Confirm paper weight (80–120 gsm uncoated for pads) or board/PVC spec (350–400 gsm + gloss dry-erase film or 0.30 mm PVC) alongside partner-sourced pencil or marker barrel dimensions.
  2. Prepress Proofing: Verify PDF/X-1a or PDF/X-4 files for 3 mm (0.118 in) bleed, 100% K grid lines, TAC ≤280%–300%, and wrap margins (15–20 mm / 0.591–0.787 in for wrapped greyboard).
  3. Offset Printing & Finishing: Print pad sheets, scoreboard faces, and sleeves. Apply gloss dry-erase film to scoreboards (or anti-scuff matte to non-writable dark sleeves) and die-cut R3–R3.5 mm (0.118–0.138 in) corners where specified.
  4. Collation & Padding: Jog pad sheets square against the chipboard backer, clamp, and apply flexible padding adhesive along the bound edge. Verify clean single-sheet tear-off without pulling fibers from the next sheet.
  5. Kitting, Wrapping & Compliance Documentation: Collate pads/boards with pencils or markers, apply retail shrink wrap or printed sleeves, and record exact component weights (in kg and lb) for packaging compliance.
    • EN 71 (EU Toy Safety): If the kit is marketed for children or includes small parts such as marker caps, mini pencils, or erasers, conduct EN 71 mechanical, physical, and chemical migration assessment and testing per EU Toy Safety.
    • Packaging & Sorting Records (EU): Document packaging material weights (shrink film, paper sleeves, backing cards) in kg and lb to support registration and reporting under ZSVR Verpackungsregister (Germany VerpackG) and sorting-label requirements under French Info-Tri / Triman where applicable.

Failure Modes & Prevention

  • Ink and pencil smearing on scorepads: Printing tear-off pads on coated art paper prevents graphite adhesion and smears ballpoint ink. Use 80–120 gsm uncoated offset stock for all writable paper pads.
  • Dry-erase ink ghosting or staining: Applying dry-erase markers to uncoated paper, standard varnish, or matte lamination leaves permanent residue. Specify gloss dry-erase film lamination or 0.30 mm (0.0118 in) PVC for erasable tally boards.
  • Padding glue tearing or block-splitting: Over-penetrating or brittle adhesive rips the top of the next sheet during tear-off, while under-applied glue causes the pad to split mid-stack. Match flexible padding compound to the sheet gsm and verify clean peel on a bound sample before full kitting.
  • Shrink-wrap curling and corner crush: High shrink tension over thin pads or unbacked boards bows the stack and crushes exposed corners. Pair shrink-wrapped kits with a 1.5–3 mm (0.059–0.118 in) greyboard or 350–400 gsm stiffener and calibrate tunnel heat for the wrap gauge.
  • Sleeve or box splitting around writing tools: Sizing sleeves or tuck boxes to the flat pad thickness alone causes bulging or torn seams once a marker or pencil bundle is inserted. Measure total stack height over the writing tool diameter and enforce 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack clearance.