Bill of Materials and Specifications
A complete standalone kit combines four physical components: the printed grid mat, dry-erase surface lamination, partner-sourced markers, and a flat-pack outer carton or sleeve.
| Component | Folding Greyboard Option | Flexible Synthetic Option |
|---|---|---|
| Mat Core / Substrate | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) greyboard | Tear-resistant, lay-flat synthetic sheet stock |
| Surface Wrap / Margin | Printed paper wrap with 15–20 mm (0.591–0.787 in) wrap margin folded over board edges | Direct-printed synthetic face (no separate paper wrap) |
| Erasable Coating | Gloss dry-erase PET/BOPP film laminated over printed wrap | Gloss dry-erase PET/BOPP film laminated over synthetic face |
| Corner Profile | Wrapped square or die-cut rounded corners | R3–R3.5 mm (0.118–0.138 in) rounded corners to resist dog-earing |
| Included Markers | Partner-sourced low-odor dry-erase markers (fine or bullet tip) | Partner-sourced low-odor dry-erase markers (fine or bullet tip) |
| Optional Care Leaflet | 4-, 6-, or 8-panel leaflet on 80–120 gsm interior stock (0.08–0.13 mm / 0.003–0.005 in per sheet) | 4-, 6-, or 8-panel leaflet on 80–120 gsm interior stock (0.08–0.13 mm / 0.003–0.005 in per sheet) |
| Outer Packaging | Two-piece rigid box (1.5–3 mm / 0.059–0.118 in greyboard, 15–20 mm / 0.591–0.787 in wrap) or folding carton | Printed belly band/sleeve or flat-pack folding carton |
Substrate, Paper Weight, and Minimums
- Mat trim sizing: Finished dimensions depend on the target table footprint, panel fold count, and outer carton geometry; lock the mat footprint and fold-hinge layout before finalizing the outer box dieline.
- Paper weight notation: Specify wrap and leaflet stocks in gsm alongside US basis weights—US Text LB is measured on a 25 × 38 in (635 × 965 mm) basis sheet, whereas US Cover LB is measured on a 20 × 26 in (508 × 660 mm) basis sheet (typical for 200–300 gsm card inserts or heavy sleeves).
- Order minimums: Boxed kits and custom cutting/folding tooling follow project and component minimums (including partner minimums for custom-branded or bulk-kitted markers). If the kit also bundles standard offset cards, those card decks start at 200 decks (usual tiers: 200, 300, 500, and 1,000+).
- Carton handling weight: Keep packed master shipping cartons within standard parcel-handling limits, typically 15–20 kg (33.1–44.1 lb) per master carton, by balancing board caliper against units per case.
Prepress and Color Setup
- File formats and resolution: Supply artwork in AI, PDF, or PSD exported to PDF/X-1a or PDF/X-4 with all fonts outlined or embedded and raster elements at ≥300 DPI.
- Bleed and safety: Include 3 mm (0.118 in) bleed per side. Keep grid numbers, borders, and critical markings at least ≥3 mm (0.118 in) inside the trim line, or ≥4–5 mm (0.157–0.197 in) for bordered edges.
- Color and ink limits: Build in CMYK with separate spot layers for metallic accents, registration, or dielines. Set fine grid lines and small key text to 100% K; build deep dark backgrounds in rich black (
C40–60 M30–40 Y30–40 K100) while keeping Total Area Coverage (TAC) at ≤280%–300%.
Flat-Pack Carton Clearances
- Width and height clearance: Size the inner cavity of a two-piece box or folding carton with 1.5–2.5 mm (0.059–0.098 in) clearance across both width and height relative to the folded mat footprint.
- Stack height clearance: Allow 1.5–3 mm (0.059–0.118 in) of vertical stack clearance over the combined thickness of the folded mat, care leaflet, and recessed marker channel or bag so the lid closes without bowing.
Production Steps
- Dieline and Fold-Map Lock: Confirm the open grid footprint, panel fold lines (bi-fold, tri-fold, or quad-fold), and outer box or sleeve dieline with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack clearance.
- Prepress Preflight: Verify PDF/X-1a or PDF/X-4 compliance, 3 mm (0.118 in) bleed, 100% K grid lines, TAC ≤280%–300%, and separate spot/dieline layers.
- Printing and Dry-Erase Lamination: Print the grid wrap or synthetic sheet in CMYK, then laminate with high-release gloss dry-erase PET/BOPP film.
- Board Wrapping or Die-Cutting:
- Folding greyboard: Wrap the laminated sheet around 1.5–3 mm (0.059–0.118 in) greyboard cores with a 15–20 mm (0.591–0.787 in) turn-in margin and controlled hinge gaps so the mat folds flat without stressing the film.
- Flexible synthetic: Die-cut to final perimeter with R3–R3.5 mm (0.118–0.138 in) rounded corners.
- Marker Kitting and Carton Assembly: Pair the finished mat and optional 4/6/8-panel leaflet with partner-sourced dry-erase markers inside a polybag or recessed tray, pack into the sleeve or two-piece box, and case-pack to master carton weight targets (kg/lb).
Sign-Off Criteria
Verify the following physical and compliance checkpoints on pre-production samples before releasing full production:
- Erasability and Ghosting Check: Mark the laminated grid with the exact partner-sourced dry-erase markers, leave the ink to dry, and wipe clean with a dry cloth; no pigment staining or haze may remain on light grid tiles.
- Fold-Hinge and Flatness Check: Cycle folding greyboard hinges open and closed to confirm the wrap and dry-erase film do not crack, bubble, or tent above the table surface.
- Fit and Clearance Check: Insert the folded mat, leaflet, and markers into the two-piece box or sleeve; verify smooth lid drop and zero bulging across the 1.5–3 mm (0.059–0.118 in) stack allowance.
- Regulatory and Packaging Records:
- If the kit is marketed or intended for children under 14, complete age-appropriate EN 71 mechanical and chemical assessment and testing—paying particular attention to marker ink migration and cap choking dimensions—and retain technical documentation per the EU Toy Safety framework.
- For EU distribution, maintain applicable packaging producer registrations and sorting marks, including Germany's LUCID Packaging Register under VerpackG and France's Triman / Info-tri labeling on outer cartons and sleeves.
Failure Modes and Mitigations
| Failure Mode | Physical Cause | Mitigation |
|---|---|---|
| Permanent marker ghosting or staining | Matte/textured lamination traps pigment, or marker ink solvent reacts with low-grade film | Specify smooth gloss dry-erase PET/BOPP film and test with the exact partner-sourced marker ink before sign-off |
| Hinge cracking or film lifting | Wrap grain runs perpendicular to the fold, or hinge gap is too tight for the board caliper | Align wrap grain parallel to primary fold lines and size hinge gaps to match 1.5–3 mm (0.059–0.118 in) greyboard thickness |
| Blurry or double-imaged grid lines | Fine grid lines built in 4-color rich black instead of 100% K | Set all thin grid lines and coordinates to 100% K only |
| Box lid binding or crushed markers | Stack clearance under 1.5 mm (0.059 in) or markers placed directly over folded mat seams | Reserve 1.5–3 mm (0.059–0.118 in) stack clearance and house markers in a dedicated side channel or recessed tray |
| Curled corners or split edges on synthetic mats | Sharp 90-degree corners catch during handling and sliding into sleeves | Die-cut synthetic mats with R3–R3.5 mm (0.118–0.138 in) rounded corners |
Parent guide Custom Tabletop Companion Sets