For base card format choices and standalone deck options, see Standard Tarot Decks.


Bill of Materials and Structural Specifications

A magnetic-box tarot set combines four interdependent sub-assemblies: the 78-card deck, the bound guidebook, the inner well insert, and the rigid clamshell shell. Every dimension in the box BOM derives from the measured stack height of the cards and book rather than nominal paper weights.

1. 78-Card Deck Stack and Stock Caliper

Because 78 cards multiply small per-card thickness differences, stock and lamination choices directly dictate inner well depth.

Card Stock Approximate Base Caliper + Double-Sided Film (0.03–0.05 mm / 0.001–0.002 in) Estimated 78-Card Stack Height (Before Clearance)
300 gsm art / blue core 0.28–0.31 mm (0.011–0.012 in) 0.31–0.36 mm (0.012–0.014 in) 24.18–28.08 mm (0.952–1.106 in)
310 gsm black-core linen 0.30–0.32 mm (0.012–0.013 in) 0.33–0.37 mm (0.013–0.015 in) 25.74–28.86 mm (1.013–1.136 in)
330 gsm black core 0.32–0.34 mm (0.013–0.013 in) 0.35–0.39 mm (0.014–0.015 in) 27.30–30.42 mm (1.075–1.198 in)
350 gsm art stock 0.34–0.38 mm (0.013–0.015 in) 0.37–0.43 mm (0.015–0.017 in) 28.86–33.54 mm (1.136–1.320 in)
400 gsm art stock 0.40–0.44 mm (0.016–0.017 in) 0.43–0.49 mm (0.017–0.019 in) 33.54–38.22 mm (1.320–1.505 in)
PVC 0.30 mm (0.012 in) 0.30 mm (0.012 in) unlaminated 23.40 mm (0.921 in)

Plain-text stack formula: Deck Stack Height = 78 * (Card Base Caliper + Film Thickness per Card)

  • Corners and finishes: Die-cut cards use R3–R3.5 mm (R0.118–R0.138 in) corners. Anti-scuff matte lamination suits dark card backs and dark box wraps. Thick lamination can conflict with gilded edges, so edge-gilded decks require compatible thin film or varnish pairings confirmed on physical samples.
  • US LB vs. gsm: When specifying US paper weights alongside gsm, distinguish US Text LB (based on a 25 x 38 in / 635 x 965 mm basis sheet) from US Cover LB (based on a 20 x 26 in / 508 x 660 mm basis sheet), as identical pound ratings represent different sheet weights and calipers.

2. Magnetic Clamshell Shell, Hinge Geometry, and Magnets

  • Greyboard core: 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in). Larger side-by-side clamshells housing both a 78-card deck and a thick guidebook typically step up to 2–3 mm (0.079–0.118 in) greyboard to prevent lid bowing.
  • Wrap margin: 15–20 mm (0.591–0.787 in) turn-in allowance around all greyboard edges so the printed outer wrap seats cleanly onto the inner liner without peeling at the corners.
  • Hinge spine geometry: Book-style clamshells use V-grooved or scored hinge channels along the spine-to-cover and spine-to-base joints. The wrap paper bridges these hinge channels; the channel width must accommodate the greyboard thickness plus wrap caliper so the lid opens flat without stretching or cracking the outer wrap.
  • Magnet placement and retention: Concealed neodymium magnets sit inside routed pockets in the front flap and the fore-edge base wall, covered by the wrap and inner liner. Pockets must lock the magnets mechanically rather than relying solely on surface glue, and adhesive selection must hold under elevated transit container temperatures.

3. Cavity Layout and Inner Well Clearances

  • Well material: Recessed folded paperboard wells keep material construction mono-material and lighter, while die-cut EVA foam wells cushion heavier decks and provide tight perimeter friction.
  • Card well clearances: Add 1.5–2.5 mm (0.059–0.098 in) across the card width and height, and 1.5–3 mm (0.059–0.118 in) to the calculated 78-card stack height.
  • Extraction access: Recessed wells require a die-cut thumb notch in the paperboard/EVA wall or a glued satin ribbon pull anchored beneath the deck so cards lift out without bending the top edges.
  • Layout choice:
    • Side-by-side: Two adjacent wells (deck beside guidebook) keep overall box depth shallow and display both components on opening, increasing the footprint width.
    • Stacked: A stepped paperboard tray or deep EVA cavity places the deck beneath the guidebook, keeping the outer box footprint compact while increasing spine height and hinge wrap demand.

4. Bound Guidebook Specifications

Guidebook page counts must run in multiples of four for bound signatures.

Binding Method Page Count Range Interior Stock Cover Stock
Saddle stitch 12–40 pages 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in per sheet) 200–300 gsm
Perfect binding 28+ pages 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in per sheet) 200–300 gsm
Sewn binding 80–100+ pages recommended 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in per sheet) 200–300 gsm

Plain-text guidebook thickness formula: Guidebook Thickness = (Page Count / 2) * Interior Sheet Caliper + 2 * Cover Caliper

(Note: 4/6/8-panel folded leaflets can replace a bound book for minimal inserts, though standard magnetic tarot sets pair a bound guidebook sized to match the deck cavity or lid recess.)

5. Prepress and Print File Requirements

  • File formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
  • Resolution and color: >=300 DPI raster artwork in CMYK, with separate named spot layers for foil stamping, spot UV, or embossing.
  • Black ink and coverage: 100% K for fine body text; rich black C40–60 M30–40 Y30–40 K100 for solid dark areas; Total Area Coverage (TAC) <=280%–300%.
  • Bleed and safety: 3 mm (0.118 in) bleed per side on cards, box wraps, and guidebook pages. Maintain >=3 mm (0.118 in) safety margin from trim on borderless cards, and >=4–5 mm (0.157–0.197 in) safety margin on bordered card backs.

Job-Specific Production Steps and Sign-Off Criteria

  1. Stack and BOM Lock: Finalize card stock, film finish, edge gilding, and guidebook page count. Calculate exact 78-card stack height and guidebook thickness, then lock the cavity layout (side-by-side vs. stacked) and inner well dimensions with 1.5–2.5 mm (0.059–0.098 in) XY clearance and 1.5–3 mm (0.059–0.118 in) Z clearance.
  2. Dieline Engineering: Generate the clamshell greyboard dieline, hinge groove positions, 15–20 mm (0.591–0.787 in) wrap turn-ins, magnet pocket coordinates, and well/ribbon-pull cutouts.
  3. White Dummy (Structural Sample) Sign-Off: Assemble an unprinted dummy using the exact greyboard caliper, wrap paper weight, EVA or paperboard well, and 78-card blank deck + blank guidebook.
    • Sign-off criteria: The lid opens smoothly without wrap tension or spine creasing; the 78-card deck and guidebook drop in and lift out cleanly via the thumb notch or ribbon; the magnetic flap snaps shut without lifting under the weight of the lid.
  4. Prepress and Wet/Digital Proofing: Verify PDF/X-1a or PDF/X-4 output, spot layers, >=4–5 mm (0.157–0.197 in) bordered-back safety, and TAC <=280%–300%. Confirm anti-scuff matte adhesion on dark wraps and edge-gilding compatibility on laminated card samples.
  5. Mass Production and Transit Heat Verification: Inspect early production boxes for magnet pocket seating, adhesive cure, and flap pull strength after elevated-temperature conditioning before full carton packing.

Concrete Failure Modes

  • Hinge Wrap Cracking or Tenting: Insufficient spine channel width for 2–3 mm (0.079–0.118 in) greyboard causes the outer wrap to split along the hinge crease or lift away from the inner liner when opened.
  • Magnet Detachment or Flap Pop-Open in Transit: Surface-glued magnets without recessed greyboard pockets can shift or detach when container temperatures rise, and undersized magnets fail to hold heavy 2.5–3 mm (0.098–0.118 in) lids closed during vibration.
  • Tight or Crushed Card Well: Calculating well depth from base card caliper while omitting the 0.03–0.05 mm (0.001–0.002 in) double-sided film thickness adds 2.34–3.90 mm (0.092–0.154 in) across 78 cards, forcing the deck to bow or preventing the magnetic flap from seating flush.
  • Scuffing on Dark Wraps and Gilding Delamination: Standard matte lamination on rich-black clamshell wraps scuffs during transit and handling; thick card lamination can peel or blister along the edges when paired with metallic gilding.
  • Guidebook Spine Splitting: Specifying perfect binding instead of sewn binding on 80–100+ page guidebooks causes pages to crack or detach when readers press the book flat during use.

Regulatory and Packaging Compliance Records

Applicable compliance steps depend on the target sales channel, age grading, and destination market: