Choose 1.5 mm (0.059 in) greyboard for compact 78-card sets with thin saddle-stitched booklets, and step up to 2.0 mm (0.079 in) greyboard when pairing 350 gsm cards with a perfect-bound or sewn guidebook. Switch from standard matte to anti-scuff matte lamination on dark box wraps, and omit thick film lamination if the 78-card deck specifies gilded edges. Card trim dimensions and core deck options follow the standard tarot decks specification; this guide covers the complete bill of materials, internal tray geometry, and assembly tolerances for the finished rigid-box set.

Bill of Materials and Component Specifications

Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+), while two-piece rigid boxes, custom inner trays, and bound guidebooks follow project and component minimums.

Component Default Specification Dimensions & Caliper Conditions That Change It
78-Card Deck 330 gsm black-core or 350 gsm art stock; R3–R3.5 mm (R0.118–R0.138 in) corners 330 gsm black core: 0.32–0.34 mm (0.0126–0.0134 in); 350 gsm art stock: 0.34–0.38 mm (0.0134–0.0150 in); double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card Use anti-scuff matte for dark card backs; avoid thick lamination when specifying gilded edges
Companion Guidebook Multiples of 4 pages; 12–40p saddle-stitched or 28p+ perfect-bound Interior: 80–120 gsm (~54–81 lb US Text, 25 × 38 in basis sheet), 0.08–0.13 mm (0.0031–0.0051 in) per sheet; Cover: 200–300 gsm (~74–111 lb US Cover, 20 × 26 in basis sheet) Step up to sewn binding for 80–100+ pages so the spine opens flat without cracking
Two-Piece Rigid Box Telescoping lid-and-base greyboard wrapped in coated art paper 1.5–2.0 mm (0.059–0.079 in) greyboard; 15–20 mm (0.591–0.787 in) wrap turn-in margin Use 2.5–3.0 mm (0.098–0.118 in) greyboard for oversized formats or heavy multi-deck sets; specify anti-scuff matte on dark wraps
Inner Tray & Divider Die-cut paperboard well, stepped insert, or foam/EVA cradle 1.5–2.5 mm (0.059–0.098 in) width/height clearance around card and booklet footprints Add a stepped shoulder or removable divider when the guidebook footprint exceeds the card trim
Ribbon Lift Satin or grosgrain pull ribbon anchored beneath the card well Anchored under the base liner or tray floor with free pull tab Required whenever the card stack sits flush inside a deep tray well without finger cutouts

Basis Weight and Stack-Height Calculation

Paper weights for the guidebook distinguish US Text LB (measured on a 25 × 38 in / 635 × 965 mm basis sheet) from US Cover LB (measured on a 20 × 26 in / 508 × 660 mm basis sheet). When sizing the rigid box depth, calculate the combined stack height of the physical deck, the bound guidebook, and any internal tray floor before cutting greyboard:

Combined Stack Height = (78 × single-card caliper with film) + ((guidebook pages / 2) × interior sheet caliper) + (2 × guidebook cover caliper) + tray floor thickness + 1.5–3.0 mm (0.059–0.118 in) stack clearance

For example, 78 cards on 330 gsm black-core stock (0.33 mm / 0.0130 in) with double-sided film (+0.04 mm / 0.0016 in) produce a 28.86 mm (1.136 in) deck stack. Pairing that deck with a 64-page perfect-bound guidebook on 100 gsm interior stock (~0.10 mm / 0.0039 in per sheet, 3.20 mm / 0.126 in text block) and a 250 gsm cover (~0.25 mm / 0.010 in per cover face, 0.50 mm / 0.020 in total) adds 3.70 mm (0.146 in) plus spine glue swell, requiring a minimum interior box depth of 34.06–35.56 mm (1.341–1.400 in) before adding tray floor thickness.

Prepress and File Setup

Prepare print-ready files in Adobe Illustrator (AI), PDF, or Photoshop (PSD) exported to PDF/X-1a or PDF/X-4 at ≥300 DPI.

  • Color and Ink Limits: Build artwork in CMYK with separate spot layers for foil stamping, spot UV, or edge gilding. Set fine body text to 100% K only. Use rich black (C40–60 M30–40 Y30–40 K100) for large dark solids on box wraps and card backs, keeping Total Area Coverage (TAC) at ≤280%–300%.
  • Bleed and Safety Margins: Apply 3 mm (0.118 in) bleed per side on cards, guidebook pages, and box wraps. Maintain ≥3 mm (0.118 in) safety inside the trim line for standard artwork, and increase safety to ≥4–5 mm (0.157–0.197 in) for bordered card backs.
  • Fonts and Box Wrap Turn-Ins: Outline or embed all fonts. Extend the rigid-box wrap artwork 15–20 mm (0.591–0.787 in) past the outer board score lines so the wrap folds cleanly over the greyboard edges without exposing raw board at the corners.

Production Steps and Sign-Off Criteria

  1. White Dummy and Stack-Height Verification: Build an unprinted structural dummy using the exact 1.5–2.0 mm (0.059–0.079 in) greyboard, inner tray, and ribbon lift alongside a physical 78-card dummy deck and bound guidebook dummy. Measure the combined stack height with calipers and verify the 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3.0 mm (0.059–0.118 in) height clearance.
  2. Prepress and Wet Proofing: Run preflight checks for TAC ≤280%–300%, spot-layer separation, and bordered-back safety margins. Sign off on color proofs for the cards, guidebook, and box wrap under the same lighting conditions, paying close attention to dark rich-black consistency.
  3. Printing, Lamination, and Finishing: Print cards, guidebook signatures, and box wraps via offset lithography. Apply anti-scuff matte lamination to dark box wraps and card backs; if the deck includes gilded edges, substitute a compatible varnish or thin coating rather than thick film lamination.
  4. Card Die-Cutting and Guidebook Binding: Die-cut and round corners to R3–R3.5 mm (R0.118–R0.138 in). Fold and bind guidebook signatures in multiples of four (12–40p saddle stitch, 28p+ perfect binding, or 80–100p+ sewn binding) and trim flush to the tray recess dimensions.
  5. Greyboard Grooving, Wrapping, and Lid Friction Tuning: V-groove and stay-tape the rigid base and telescoping lid. Wrap with the laminated art paper using the 15–20 mm (0.591–0.787 in) turn-in margin. Test lid-to-base friction damping so the lid descends smoothly under its own weight without binding or dropping abruptly.
  6. Tray Insertion, Ribbon Anchoring, and Pack-Out: Anchor the ribbon lift beneath the inner tray or base liner, seat the 78-card deck and guidebook into their respective wells, and shrink-wrap or sleeve the finished box. Keep master shipping cartons within ergonomic handling limits (typically ≤15–20 kg / 33.1–44.1 lb per carton) with corner protectors to prevent crushed rigid-box edges in transit.

Sign-Off Criteria

  • Combined Stack Fit: The 78-card deck and bound guidebook sit inside the tray with 1.5–3.0 mm (0.059–0.118 in) vertical clearance; the lid closes completely without resting on the guidebook spine or card stack.
  • Lid Friction Damping: Holding the lid at the top edges allows the base to slide out smoothly in 2–4 seconds without sticking (vacuum lock) or falling freely.
  • Dark-Box Surface Integrity: Anti-scuff matte lamination shows no visible white rub marks or gloss burnishing after carton-pack vibration testing.
  • Ribbon Lift Function: Pulling the ribbon tab lifts the full 78-card stack cleanly above the tray lip without tearing the anchor or creasing the bottom card.

Concrete Failure Modes

  • Lid Seizure or Loose Drop: Omitting wrap-paper and lamination thickness from the lid-to-base gap calculation causes either tight corner binding that tears the wrap or a loose lid that separates during retail handling.
  • Bowed Lid or Crushed Guidebook Spine: Calculating stack height from nominal paper gsm without accounting for double-sided card film (+0.03–0.05 mm / 0.0012–0.0020 in per card) or perfect-bound spine swell leaves the lid resting on the contents.
  • Whitening and Scuffing on Dark Boxes: Using standard matte lamination or unlaminated dark rich-black wraps leads to visible fingernail scratches and edge whitening during assembly and shipping.
  • Gilded-Edge Flaking: Pairing thick film lamination on 330–350 gsm cards with metallic edge gilding prevents clean foil adhesion along the card edge, causing flakes to peel during shuffling.
  • Trapped Deck in Flush Tray: Designing a deep paperboard or EVA well with 1.5–2.5 mm (0.059–0.098 in) side clearance but no ribbon lift or finger notch forces users to invert and shake the rigid box to remove the cards.
  • Miscut Bordered Card Backs: Using a standard 3 mm (0.118 in) safety margin instead of ≥4–5 mm (0.157–0.197 in) on bordered tarot backs makes normal die-cut register shifts visibly uneven.

Conditional Regulatory and Packaging Records

Documentation and testing requirements depend on the target market, age grading, and distribution channel:

  • Toy Safety Assessment (EU/EEA): If a tarot set is marketed for children or falls within toy-safety scope, maintain technical documentation, risk assessment, and applicable EN 71 physical, flammability, and chemical testing records in line with European Commission Toy Safety (EN 71).
  • German Packaging Registration (VerpackG): When placing packaged sets onto the German market, register the brand/producer and report packaging material weights (kg/lb of paperboard, greyboard, and film) through the LUCID Packaging Register (VerpackG).
  • French Sorting Labeling (Triman / Info-tri): For sets distributed to consumers in France, apply the required sorting signage and material separation instructions on the outer packaging or insert according to French Info-tri / Triman guidelines.