Choose 310–350 gsm card stock with an aqueous or UV matte varnish for metallic foil or painted edges. Switch to anti-scuff matte when artwork uses heavy dark ink coverage, and reserve 400 gsm stock only for decks packaged in rigid two-piece or magnetic boxes engineered for the taller stack. Avoid thick soft-touch or heavy double-sided lamination films on gilded decks, as film edges resist foil adhesion and peel during edge-sanding and burnishing. Standard offset production starts at 200 decks (usual tiers: 200, 300, 500, 1,000+), while custom boxed sets and rigid tooling follow project and component minimums.
For base 78-card format options and trim sizing outside the gilding workflow, see the Standard Tarot Decks specification page.
78-Card Gilded-Edge Tarot BOM & Specifications
Card Deck Press coordinates 78-card gilded tarot production through specialist offset and tabletop manufacturing partners. Because tarot deck dimensions vary by edition, confirm your exact card trim dimensions before locking the dieline and box tooling; the stack-height and clearance calculations below apply to any 78-card tarot trim size.
Card Stock, Caliper, and 78-Card Stack Height
Paper weight in gsm measures grams per square meter directly. When converting to US pound weights, distinguish Cover LB (based on a 20 x 26 in sheet) from Text LB (based on a 25 x 38 in sheet): 300–400 gsm card stocks fall under Cover LB, whereas 80–120 gsm booklet interior stocks fall under Text LB.
Base stack height = 78 * single-card caliper
| Card Stock | Approximate Caliper (mm / in) | 78-Card Unlaminated Stack (mm / in) | Gilding Compatibility & Use Case |
|---|---|---|---|
| 300 gsm art / blue core | 0.28–0.31 mm / 0.011–0.012 in | 21.84–24.18 mm / 0.860–0.952 in | Lighter, flexible shuffle; compatible with thin varnish and gilding |
| 310 gsm black-core linen | 0.30–0.32 mm / 0.012–0.013 in | 23.40–24.96 mm / 0.921–0.983 in | Textured snap and opacity; pair with thin matte varnish for clean edge sanding |
| 330 gsm black core | 0.32–0.34 mm / 0.0126–0.0134 in | 24.96–26.52 mm / 0.983–1.044 in | Standard collector tarot weight; strong rigidity for metallic foil edges |
| 350 gsm art stock | 0.34–0.38 mm / 0.013–0.015 in | 26.52–29.64 mm / 1.044–1.167 in | Heavy premium feel; requires extra clamping pressure during gilding |
| 400 gsm art stock | 0.40–0.44 mm / 0.016–0.017 in | 31.20–34.32 mm / 1.228–1.351 in | Extra-thick collector stock; verify rigid box depth and corner die wear |
- Coating thickness: If a thin film is specified, double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card, adding 2.34–3.90 mm (0.092–0.154 in) across a 78-card deck. Thin matte or aqueous/UV varnish adds negligible caliper and prevents film-edge lifting during gilding.
- Dark artwork: Use anti-scuff matte rather than thick soft-touch film to prevent scuffing on dark card backs without compromising edge-foil bonding.
Prepress, Geometry, and Box BOM
- File formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4, with all fonts outlined or embedded.
- Color & resolution: CMYK at >= 300 DPI with separate spot layers for any face or back foil accents. Use 100% K for fine text, rich black C40–60 M30–40 Y30–40 K100 for deep solids, and keep Total Area Coverage (TAC) at <= 280%–300%.
- Bleed & safety: 3 mm (0.118 in) bleed per side; >= 3 mm (0.118 in) safety margin for borderless designs, and >= 4–5 mm (0.157–0.197 in) safety margin for bordered backs so minor die-cut or sanding variance does not expose uneven borders.
- Corners: R3–R3.5 mm (R0.118–R0.138 in) rounded corners.
- Box clearance: Allow 1.5–2.5 mm (0.059–0.098 in) clearance across card width and height, and 1.5–3 mm (0.059–0.118 in) clearance on stack height. If using a rigid two-piece or magnetic box, specify 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) greyboard with a 15–20 mm (0.591–0.787 in) wrap margin.
- Companion booklets & leaflets (optional): Folded leaflets use 4, 6, or 8 panels. Bound guidebook signatures run in multiples of four: saddle stitch (12–40 pages), perfect binding (28+ pages), or sewn binding (80–100+ pages recommended), using 80–120 gsm interior stock (about 0.08–0.13 mm / 0.0031–0.0051 in per sheet; US Text LB) and 200–300 gsm covers (US Cover LB).
Production Workflow & Spoilage Overage
- Prepress & Dieline Lock: Verify PDF/X-1a or PDF/X-4 files, spot layers, 3 mm (0.118 in) bleed, bordered-back safety margins (>= 4–5 mm / 0.157–0.197 in), and R3–R3.5 mm (R0.118–R0.138 in) corner radii. Confirm box inner dimensions against the 78-card stacked caliper plus 1.5–3 mm (0.059–0.118 in) height clearance.
- Offset Printing with Gilding Overage: Print sheets on the chosen 300–400 gsm stock, building extra press-run spoilage overage into the sheet count. Edge-gilding is a secondary mechanical and heat/paint process after cutting; extra overage ensures that cards rejected for foil skips, paint bleed, or corner-sanding defects do not short the final 200 / 300 / 500 / 1,000+ deck count.
- Varnish or Anti-Scuff Matte Coating: Apply thin matte or varnish coatings and allow full curing before cutting so residual moisture or uncured ink does not cause cards to block (stick together) under gilding clamp pressure.
- Precision Die-Cutting & Corner Rounding: Die-cut all 78 cards with sharp steel rules to produce clean R3–R3.5 mm (R0.118–R0.138 in) corners without paper burrs or fuzz.
- Clamping, Sanding, and Edge-Gilding: Jog and clamp the 78-card stack tightly, sand the deck edges smooth to eliminate micro-steps between cards, and apply metallic foil (heat-stamped) or pigmented edge paint.
- Separation & Packaging: Flex and fan the cured deck to break any edge-bridging between adjacent cards, collate in exact 78-card sequence, and pack into the cleared tuck or rigid box alongside any leaflet or guidebook.
Sign-Off Criteria & Fan Inspection
Before releasing a gilded-edge tarot run to final packaging, verify these baseline sign-off criteria:
- Card count & sequence: Every deck contains all 78 cards in the approved order with no duplicates or missing cards from overage replacement.
- Corner & edge continuity: Metallic foil or paint covers straight edges and R3–R3.5 mm (R0.118–R0.138 in) corners evenly without bare paper spots or flaking.
- Clean card separation: Cards fan smoothly without sticking, tearing, or pulling foil off neighboring card edges.
- Box fit: The 78-card stack drops into and slides out of the box smoothly within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height tolerances.
For the full post-gilding fan inspection procedure, defect thresholds, and sampling steps, see Gilded and Foil Card Deck Inspection.
Concrete Failure Modes
- Film peeling and edge-foil bridging: Using thick soft-touch or heavy double-sided lamination causes the plastic film edge to fray during sanding and bridge foil across adjacent cards, leading to peeling when the deck is fanned. Fix: Specify thin matte or aqueous/UV varnish (or anti-scuff matte for dark artwork).
- Corner flaking on tight or burred cuts: Dull cutting dies or corner radii tighter than R3 mm (R0.118 in) leave fibers raised at the curve, causing foil or paint to chip during initial shuffling. Fix: Enforce sharp dies at R3–R3.5 mm (R0.118–R0.138 in) and inspect clamped stacks before gilding.
- Ink-to-edge bleed or blocking: Exceeding 280%–300% TAC near card borders leaves heavy ink wet or soft under clamping pressure, causing cards to stick together or contaminate light-colored edge paint. Fix: Cap TAC at <= 280%–300%, use 100% K for fine text, and allow full cure time before clamping.
- Shorted deck counts from unbudgeted spoilage: Running standard non-gilded overage leaves insufficient replacement cards to swap out decks damaged during edge sanding or foil transfer. Fix: Add dedicated gilding spoilage overage at the press-sheet stage.
- Crushed corners or bowed boxes: Calculating box depth from nominal stock gsm without accounting for caliper tolerance (e.g., 350 gsm at 0.38 mm / 0.015 in vs. 0.34 mm / 0.013 in) or thin coatings results in a tight fit. Fix: Measure physical dummy stacks and maintain 1.5–3 mm (0.059–0.118 in) stack-height clearance.
Regulatory & Packaging Compliance
When distributing gilded tarot decks into regulated markets, maintain the applicable assessment, testing, and packaging registration records for the target jurisdiction:
- EU Toy Safety (where applicable by age grading or product classification): Assessment and testing procedures under EN 71 are documented through the European Commission's EU Toy Safety framework.
- Germany Packaging Act (VerpackG): Producer participation and data reporting requirements for retail and shipping packaging are administered via LUCID / Verpackungsregister.
- France Sorting & Labeling (Triman / Info-tri): Consumer sorting signage rules for packaged decks and printed inserts are published by the French Ministry via Info-tri.
Parent guide Custom Standard Tarot Deck Printing