Card Deck Press produces custom decks and molded-case assemblies with specialist offset and tabletop manufacturing partners. Standard offset card production starts at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks), while custom-tooled plastic cases or specialized molded trays follow project and component minimums.
Finished Deck and Molded Case Specifications
Card Stock, Caliper, and Stack Height
Match the card substrate and finish to the fixed internal depth of the chosen PP or PS snap case. In US paper specifications, distinguish Cover LB (measured on a 20 x 26 in basis sheet) from Text LB (measured on a 25 x 38 in basis sheet) alongside metric gsm values so insert and card weights are not confused.
| Component / Stock | Weight / Basis | Single-Card Caliper | Notes for Molded Snap Cases |
|---|---|---|---|
| PVC plastic card stock | — | 0.30 mm (0.0118 in) | Consistent caliper; resists moisture and warping inside tight PP/PS cavities |
| Black-core linen paper | 310 gsm (Cover LB, 20 x 26 in) | 0.30–0.32 mm (0.0118–0.0126 in) | Matches standard poker snap-case depth at 52–54 cards |
| Art / blue-core paper | 300 gsm (Cover LB, 20 x 26 in) | 0.28–0.31 mm (0.0110–0.0122 in) | Slightly thinner stack; leaves extra vertical play unless padded |
| Black-core paper | 330 gsm (Cover LB, 20 x 26 in) | 0.32–0.34 mm (0.0126–0.0134 in) | Near the upper limit for standard-depth snap cases at 54 cards |
| Heavy art / board stock | 350–400 gsm (Cover LB, 20 x 26 in) | 0.34–0.44 mm (0.0134–0.0173 in) | Exceeds standard shallow snap-case depth at 54 cards; requires fewer cards or a deep cavity |
| Double-sided film lamination | — | +0.03–0.05 mm (+0.0012–0.0020 in) | Add per laminated card; conflicts with gilded edges when thick film is used |
Calculate total stack height before locking the mold cavity:
Total stack height = Card count * (Base card caliper + Double-sided film thickness)
As a baseline, a 54-card deck on 0.30 mm (0.0118 in) PVC measures 16.20 mm (0.638 in). A 54-card deck on 310 gsm black-core linen measures 16.20–17.28 mm (0.638–0.680 in) uncoated, or 17.82–19.98 mm (0.702–0.787 in) with double-sided film.
Cavity Clearances and Insert Tolerances
- Internal cavity clearance: Maintain 1.5–2.5 mm (0.059–0.098 in) total clearance across deck width and height, and 1.5–3 mm (0.059–0.118 in) clearance above the stack height. Molded PP/PS walls are rigid; tighter clearances bind on draft angles or corner radii, while excess clearance lets cards rattle and chip edges.
- Corner radius: Die-cut poker cards to R3–R3.5 mm (R0.118–R0.138 in) and verify that the molded case's internal corner radius is equal to or larger than the card corner radius at the base of the draft angle.
- Header and wrap inserts: Printed paper wraps or top/bottom header cards use 200–300 gsm Cover LB (20 x 26 in basis) for rigid headers or 80–120 gsm Text LB (25 x 38 in basis; approximately 0.08–0.13 mm / 0.0031–0.0051 in per sheet) for thin wraparound bands and folded 4/6/8-panel inserts. Trim inserts to the exact flat-panel recess of the mold with 0.5 mm (0.020 in) maximum cumulative trim tolerance so the insert sits flat without bowing the snap latch.
Prepress and Finishing Rules
- File format and color: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts. Set artwork in CMYK at ≥300 DPI with separate spot layers for foil, spot UV, or die lines.
- Black ink and coverage: Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for solid dark fields, and keep Total Area Coverage (TAC) at ≤280%–300%.
- Bleed and safety: Include 3 mm (0.118 in) bleed per side on both cards and printed inserts. Keep text and critical graphics at ≥3 mm (≥0.118 in) inside the trim line, and ≥4–5 mm (≥0.157–0.197 in) for bordered card backs.
- Surface protection: Use anti-scuff matte varnish or lamination on dark artwork to prevent rubbing against the interior plastic walls during transit.
Production Steps and Sign-Off Criteria
- Cavity measurement and BOM lock: Measure the exact internal length, width, corner radius, and depth of the selected PP or PS snap case at the narrowest draft point. Lock the card count, substrate (0.30 mm / 0.0118 in PVC or 310 gsm paper), and insert stock (Cover LB vs. Text LB) using the stack-height formula.
- Prepress and dieline check: Verify PDF/X-1a or PDF/X-4 compliance, 3 mm (0.118 in) bleeds, ≥3 mm (≥0.118 in) or ≥4–5 mm (≥0.157–0.197 in) safety margins, 100% K fine text, TAC ≤280%–300%, and exact insert die lines matched to the case recess.
- Card printing, coating, and die-cutting: Print offset sheets (or UV-offset on PVC), apply anti-scuff matte or specified finish, and die-cut cards to R3–R3.5 mm (R0.118–R0.138 in) corners.
- Insert trimming and folding: Guillotine-trim header cards or fold 4/6/8-panel inserts to fit the molded recess without interfering with the hinge or snap clasp.
- Casing and master-carton packing: Seat the collated deck and insert into the molded case, snap-close, and pack into master cartons with gross weights recorded in both kg and lb.
Sign-Off Criteria
- Physical fit: The snap clasp closes with uniform resistance, no lid bowing, and no card corner pinching against the case's internal corner radii.
- Stack play: When shaken gently, the deck stays within the 1.5–3 mm (0.059–0.118 in) stack-height allowance and 1.5–2.5 mm (0.059–0.098 in) width/height allowance without rattling hard enough to dent card edges.
- Print and finish: Dark solids show no scuffing against the plastic shell, bordered backs remain centered within tolerance, and insert edges sit flush inside the case recess.
- Regulatory and packaging records (where applicable): If distributed in markets with toy-safety or packaging-EPR rules, compile the relevant technical and registration records—such as EN 71 toy safety assessment and testing for children's decks in the EU, LUCID / VerpackG participation and data reporting for German packaging weights (in kg and lb), and Triman sorting-information rules for French market packaging.
Concrete Failure Modes
- Snap latch pops open or lid bows: Caused by pairing a standard-depth snap case with 350–400 gsm stock or adding 0.03–0.05 mm (0.0012–0.0020 in) double-sided film across 54+ cards without recalculating stack height. Fix by switching to 0.30 mm (0.0118 in) PVC or 310 gsm linen, reducing card count, or moving to a deeper mold.
- Corner crushing at the base of the case: Caused by card corners (R3–R3.5 mm / R0.118–R0.138 in) being sharper than the molded case's internal corner radius or by draft-angle taper narrowing the bottom of the cavity below the 1.5 mm (0.059 in) minimum clearance.
- Header or wrap insert buckling: Caused by insert trim oversized by >0.5 mm (0.020 in) or by grain direction running perpendicular to a wrap fold, forcing the insert out of the recess and fouling the snap clasp.
- Scuff marks on dark card backs: Caused by glossy or uncoated dark ink (high TAC >300%) rubbing directly against rigid PS or PP walls during shipping vibration. Fix by enforcing TAC ≤280%–300% and applying an anti-scuff matte finish.
- Gilded-edge flaking or delamination: Caused by combining thick double-sided film lamination with metallic edge gilding; thick film prevents clean edge adhesion and flakes when cards flex inside a tight plastic cavity.
Parent guide Custom Poker Deck Printing