Bill of Materials and Baseline Specifications

Standard offset card production starts at 200 decks, with usual production tiers at 200, 300, 500, and 1,000+ decks.

Component Baseline Specification Alternatives & Conditions
Card format 63 x 88 mm (2.48 x 3.46 in), R3–R3.5 mm (0.118–0.138 in) corners 54–56 cards (52 standard + 2 jokers + up to 2 extra cards)
Card stock 310 gsm black-core linen (0.30–0.32 mm / 0.0118–0.0126 in) 300 gsm art/blue core (0.28–0.31 mm / 0.0110–0.0122 in); 330 gsm black core (0.32–0.34 mm / 0.0126–0.0134 in); double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card
Tuck box board 300–350 gsm SBS or grey-back folding carton 300 gsm suits lighter 54-card decks; 350 gsm SBS suits heavier 56-card decks or retail hang/shelf handling
Box internal clearance 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–2.5 mm (0.059–0.098 in) stack 1.5–3 mm (0.059–0.118 in) stack allowance if thick lamination or extra inserts are added
Outer overwrap Cellophane with horizontal tear-strip Omit only for non-retail bulk packs or inner-box components

When specifying paperboard weights in US units, use gsm alongside Cover LB (20 x 26 in / 508 x 660 mm basis sheet) rather than Text LB (25 x 38 in / 635 x 965 mm basis sheet), because folding carton and playing-card stocks are heavier cover-weight sheets.

For shipping and carton planning, calculate card stack mass using the plain-text formula:

Card stack mass (kg) = Card count x (0.063 m x 0.088 m) x (Card gsm / 1,000)

At 54–56 cards on 300–330 gsm stock (0.005544 m^2 per card), the cards weigh 0.090–0.102 kg (0.198–0.225 lb). Adding the 300–350 gsm tuck box and cellophane wrap brings a finished retail deck to roughly 0.105–0.125 kg (0.23–0.28 lb), or 105–125 kg (231–276 lb) per 1,000 decks before master shipping cartons.

Prepress and Color Defaults

  • File formats and color: Supply AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 at >=300 DPI in CMYK with separate spot layers for metallic inks, foils, or spot UV. Outline or embed all fonts.
  • Black builds and ink limits: Use 100% K for fine text and barcodes. Use rich black (C40–60 M30–40 Y30–40 K100) for large dark solids, keeping total area coverage (TAC) at <=280%–300%.
  • Bleed and safety: Include 3 mm (0.118 in) bleed per side on both cards and the tuck box dieline. Keep card face safety at >=3 mm (0.118 in) and bordered card-back safety at >=4–5 mm (0.157–0.197 in).
  • Surface finish: Pair dark tuck artwork with anti-scuff matte lamination or varnish to prevent rub marks during collation and overwrapping. If the deck uses gilded edges, avoid thick film lamination on the cards because thick film conflicts with edge gilding adhesion.

Stack Thickness, Clearances, and Grain Direction

Size the tuck box spine depth from the measured deck stack height rather than nominal gsm alone. Calculate total stack height with:

Stack height (mm) = Card count x (Base caliper + Double-sided film thickness)

Card Stock Base Caliper per Card 54-Card Stack (No Film) 56-Card Stack (No Film) Added Height for Double-Sided Film (0.03–0.05 mm/card)
300 gsm art/blue core 0.28–0.31 mm (0.0110–0.0122 in) 15.12–16.74 mm (0.595–0.659 in) 15.68–17.36 mm (0.617–0.683 in) +1.62–2.70 mm (+0.064–0.106 in) for 54; +1.68–2.80 mm (+0.066–0.110 in) for 56
310 gsm black-core linen 0.30–0.32 mm (0.0118–0.0126 in) 16.20–17.28 mm (0.638–0.680 in) 16.80–17.92 mm (0.661–0.706 in) +1.62–2.70 mm (+0.064–0.106 in) for 54; +1.68–2.80 mm (+0.066–0.110 in) for 56
330 gsm black core 0.32–0.34 mm (0.0126–0.0134 in) 17.28–18.36 mm (0.680–0.723 in) 17.92–19.04 mm (0.706–0.750 in) +1.62–2.70 mm (+0.064–0.106 in) for 54; +1.68–2.80 mm (+0.066–0.110 in) for 56

Add 1.5–2.5 mm (0.059–0.098 in) across the 63 mm (2.48 in) width and 88 mm (3.46 in) height, giving an internal box cavity of 64.5–65.5 mm (2.54–2.58 in) wide by 89.5–90.5 mm (3.52–3.56 in) tall. Add 1.5–2.5 mm (0.059–0.098 in) to the calculated stack height for standard retail tuck boxes, increasing to 3 mm (0.118 in) when accommodating thick film or slight deck curl.

Specify grain direction on both the carton and the cards:

  • Tuck box grain: Run paperboard grain parallel to the vertical 88 mm (3.46 in) height of the box. Vertical grain keeps the four main body scores and the side glue seam folding smoothly without ink cracking, while providing rigidity along the top and bottom tuck flaps.
  • Card grain: Keep all cards in the deck cut to a single grain direction (commonly parallel to the 88 mm / 3.46 in long edge) so the deck flexes uniformly and does not fan unevenly inside the tuck box.

Cellophane Tear-Strip Overwrap and Production Steps

  1. Lock dieline from physical stack: Confirm card stock, coating/film, and 54–56 card count, then set the tuck box spine depth (Stack height + 1.5–2.5 mm / 0.059–0.098 in) and 3 mm (0.118 in) bleed on the flat dieline.
  2. Offset print and finish: Print cards and tuck box sheets in CMYK (+ spot layers if specified). Apply anti-scuff matte or protective varnish to the tuck box exterior, keeping glue flaps free of varnish and lamination.
  3. Cut, round, and collate cards: Guillotine or die-cut cards to 63 x 88 mm (2.48 x 3.46 in), round corners to R3–R3.5 mm (0.118–0.138 in), and collate 54–56 cards per deck.
  4. Die-cut and glue tuck boxes: Crease and die-cut 300–350 gsm SBS or grey-back board with vertical grain, then fold and glue the side seam.
  5. Insert and overwrap: Load the collated deck into the tuck box, close the dust flaps and main tuck flap, and apply cellophane overwrap with a horizontal tear-strip positioned around the upper third of the box. Place the longitudinal heat-seal seam on a side spine or bottom panel away from the barcode and front artwork.

Sign-Off Criteria and Retail Compliance Records

Verify these criteria on pre-production or first-article samples before full run release:

  • Fit and clearance: The 54–56 card stack slides into the 64.5–65.5 mm x 89.5–90.5 mm (2.54–2.58 in x 3.52–3.56 in) cavity without catching on the side-seam flap or bowing the front/back panels.
  • Crease and finish integrity: Vertical body folds and horizontal tuck-flap scores show no fiber cracking or ink flaking, and dark solids pass scuff inspection.
  • Tear-strip function: Pulling the cellophane tear-strip tab cleanly severs the wrap around the upper perimeter without snagging or tearing the underlying carton print.

When distributing retail tuck-box decks into regulated markets, maintain the applicable compliance records alongside the bill of materials:

  • EU Toy Safety (EN 71): If the deck is marketed or intended for use by children under 14, plan for EN 71 safety assessment and laboratory testing covering physical/mechanical properties and chemical migration as outlined by the European Commission Toy Safety framework.
  • Germany Packaging (VerpackG): For retail distribution in Germany, the tuck box and cellophane overwrap require producer registration and system participation data reporting under the ZSVR Verpackungsregister.
  • France Sorting Marks (Triman): For retail distribution in France, reserve print space on the carton or packaging artwork for the applicable sorting instructions defined in French Ministry Info-Tri.

Concrete Failure Modes

  • Omitted film allowance in spine depth: Calculating spine depth from base caliper without adding 0.03–0.05 mm (0.0012–0.0020 in) per laminated card reduces clearance below 1.5 mm (0.059 in), causing bowed carton walls, popped side seams, and pinched card corners during insertion.
  • Cross-grain tuck box layout: Nesting the tuck dieline with grain perpendicular to the 88 mm (3.46 in) height cracks the ink and board fibers along the four main vertical folds on 300–350 gsm stock.
  • Excessive heat-seal tension or misaligned tear-strip: Over-tensioned cellophane warps the tuck box inward and crushes the top corners; a tear-strip placed too close to the top fold fails to open the upper cap cleanly.
  • Narrow safety on bordered card backs: Keeping less than 4–5 mm (0.157–0.197 in) safety on bordered backs exposes die-cut registration shifts as visibly uneven margins on 63 x 88 mm (2.48 x 3.46 in) cards.
  • High TAC on dark tuck solids without anti-scuff matte: Exceeding 300% TAC or skipping anti-scuff matte on dark cartons leads to ink set-off, rub marks on the collating line, and cracking along the tuck-flap crease.