Choose cellophane tear-strip overwrap when using heat-sensitive PVC, thick double-sided lamination, or dark anti-scuff matte coatings that risk blocking in a heat tunnel. Choose low-temperature shrink wrap when tight film conformance over a paper belly band or irregular stack height is required. If your distribution requires individual shelf display or retail drop protection, use the standard boxed configuration on the Poker Decks page instead. Standard offset card production starts at 200 decks (usual tiers: 200 / 300 / 500 / 1,000+); omitting individual tuck boxes removes carton die tooling from the job while keeping card-sheet setup unchanged.


Specifications & Bill of Materials

Card Stock, Caliper & Finishes

Card Deck Press coordinates production with specialist offset and tabletop manufacturing partners. Specify card and band stocks by gsm alongside US basis weight, keeping US Text LB (25 × 38 in basis sheet) distinct from Cover LB (20 × 26 in basis sheet):

  • 300 gsm art / blue core: 0.28–0.31 mm (0.011–0.012 in) caliper
  • 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in) caliper
  • 330 gsm black core: 0.32–0.34 mm (0.013–0.013 in) caliper
  • 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in) caliper
  • 400 gsm stock: 0.40–0.44 mm (0.016–0.017 in) caliper
  • PVC: 0.30 mm (0.012 in) caliper
  • Double-sided film lamination: Adds 0.03–0.05 mm (0.001–0.002 in) per card. Anti-scuff matte suits dark artwork; thick lamination can conflict with gilded edges.

Prepress & Trim Tolerances

Trim dimensions follow the poker-deck format specified on the Poker Decks parent page. All refill deck files must meet these prepress tolerances:

  • Color & Resolution: CMYK with separate spot layers, ≥300 DPI, 100% K for fine text, rich black C40–60 M30–40 Y30–40 K100, Total Area Coverage (TAC) ≤280%–300%.
  • File Format: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts.
  • Bleed, Safety & Corners: 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered backs); R3–R3.5 mm (0.118–0.138 in) corner radius.

Shrink-Wrap Enclosures & Heat Limits

For general shrink-film mechanics and tunnel equipment behavior, see Shrink-Wrap Enclosures. Because refill poker decks have no tuck carton acting as a thermal buffer, film contacts the top card, bottom card, and exposed deck edges directly:

  • Low-temperature shrink wrap: Requires reduced tunnel temperature and shorter dwell time to prevent coating softening, card-to-card blocking, and inward corner curl on thin art stocks or 0.30 mm (0.012 in) PVC.
  • Cellophane tear-strip overwrap: Seals with localized heat at the fold seam rather than full-deck tunnel exposure, preserving edge flatness on coated or laminated decks while providing a clean pull-tab opening.

Belly-Band Placement & Stock

An optional paper belly band carries barcodes, batch codes, or deck identifiers that cannot be printed on clear film:

  • Stock: 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in per sheet) text stock or 200–300 gsm cover stock (distinguishing Text LB from Cover LB by basis sheet size).
  • Placement: Wrapped dry around the collated deck before film overwrapping so the outer film holds the band flush without glue touching the card faces. Position the band's overlap seam on the deck face or edge away from the film's primary heat-seal bar.

Partitioned Brick Master Cartons & Compliance Records

Without tuck boxes, corner protection depends entirely on inner brick boxes and corrugated master cartons:

  • Partitioned Grid: Full-height corrugated dividers isolate each wrapped deck or tight brick stack, eliminating deck-to-deck corner impact and film scuffing during transit.
  • Clearance: Size brick cells to the wrapped deck stack with minimal lateral play so rounded R3–R3.5 mm (0.118–0.138 in) corners cannot rattle against carton walls.
  • Conditional Regulatory Documentation: When shipping into regulated markets, record packaging material compositions and applicable marks on the belly band or master carton per official process requirements—such as German packaging registration under VerpackG or French sorting signage under Triman. Where the deck is marketed for children or falls under toy safety scope, coordinate EN 71 assessment and testing records prior to shipment.

Production Steps

  1. Prepress & Imposition: Verify PDF/X-1a or PDF/X-4 card files, 3 mm (0.118 in) bleeds, bordered-back safety margins (≥4–5 mm / 0.157–0.197 in), and optional belly-band artwork.
  2. Offset Printing, Coating & Die-Cutting: Print sheets, apply aqueous, UV, anti-scuff matte, or double-sided film, then die-cut and round corners to R3–R3.5 mm (0.118–0.138 in). Allow full ink and coating cure before stacking.
  3. Collation & Belly-Band Wrapping: Collate each deck in exact card sequence and apply the dry paper belly band flush to the stack, keeping adhesives off card surfaces.
  4. Overwrapping & Tunnel Calibration: Apply cellophane tear-strip overwrap or run low-temperature shrink wrap calibrated to the deck's core stock and coating thermal limit.
  5. Partitioned Brick Packing: Load cooled, wrapped decks into partitioned brick inner boxes and corrugated master cartons with void fill as needed to immobilize stacks.

Sign-Off Criteria

  • Collation & Trim: Exact card count and sequence verified; corners uniformly cut to R3–R3.5 mm (0.118–0.138 in) with no nicked or fuzzy edges.
  • Wrap Integrity: Film lies flat against the deck without bowing the stack or curling card corners; tear strip opens cleanly without snagging the belly band.
  • Surface Condition: Zero card-to-card blocking, coating tackiness, or heat-scorch marks on the top and bottom cards after cooling.
  • Belly-Band Alignment: Band sits square and centered on the deck with no adhesive bleed onto cards and no torn overlap at the heat-seal seam.
  • Brick Carton Fit: Partitions hold wrapped decks snugly without crushing edges, and master cartons pass handling checks without corner denting.

Failure Modes & Mitigations

  • Deck Warping or Edge Curl from Tunnel Heat: Excessive tunnel temperature shrinks film faster than the unboxed card stack equilibrates, bowing 300 gsm art stock or 0.30 mm (0.012 in) PVC. Mitigation: Lower tunnel temperature, increase conveyor speed, or switch to cellophane tear-strip overwrap.
  • Card Blocking (Sticking Together): Wrapping decks before aqueous, UV, or anti-scuff matte coatings fully cure—combined with shrink-tunnel heat—fuses adjacent cards. Mitigation: Enforce full post-press curing time and verify exit stack temperature before brick packing.
  • Belly-Band Slippage or Film Burn-Through: A loose belly band shifts during wrapping, or a thick paper overlap traps heat under the seal bar. Mitigation: Size band length using actual deck stack height (card count × single-card caliper) and orient the band seam away from the seal jaw.
  • Crushed Corners in Transit: Bulk-packing unboxed decks without dividers allows decks to shift and dent exposed R3–R3.5 mm (0.118–0.138 in) corners through the film. Mitigation: Require full-height corrugated partitions inside every brick master carton and eliminate internal void space.