Choose rigid Kraft tubes for single-sheet or small-quantity collector mailings on 300–330 gsm card stocks where lower shipping volume and crush resistance matter most. Choose flat corrugated mailers when shipping multi-sheet stacks, thick 350–400 gsm stocks, double-sided laminated sheets, or heavy cold-foil and spot-UV coverage that cracks or retains permanent curl when rolled.


Finished Deliverable Bill of Materials

An uncut press sheet order skips the slitting, die-cutting, and R3–R3.5 mm (0.118–0.138 in) corner-rounding stages used for cut decks. For standard cut-and-packed decks starting at 200 decks (usual tiers 200, 300, 500, and 1,000+), see the custom trading card printing guide.

Component Specification Purpose
Untrimmed Press Sheet 700 x 1000 mm (27.6 in x 39.4 in) full sheet Preserves full card grid, registration targets, and press color bars
Core Card Stock 300–400 gsm card stock or 0.30 mm (0.012 in) PVC Determines sheet rigidity, caliper, and roll tolerance
Surface Coatings & Foils Offset varnish, matte/gloss lamination, spot UV, or hot/cold foil Applied in-line or post-press before sheets are pulled from finishing
Tissue Interleaving Acid-free or glassine protective sheet per press sheet Prevents ink set-off, foil scratching, and scuffing between stacked or rolled sheets
Outer Shipping Pack Spiral-wound rigid Kraft tube with end caps, or double-wall flat corrugated mailer with corner guards Protects sheet edges, corners, and surface flatness during transit

Sheet Specifications, Stocks, and Trim Margins

Stock Caliper and Weight Basis

Card stocks are specified in grams per square meter (gsm). In US paper weights, distinguish Cover LB (based on a 20 x 26 in / 508 x 660 mm basis sheet) from Text LB (based on a 25 x 38 in / 635 x 965 mm basis sheet); a 300 gsm card stock corresponds roughly to 110 lb Cover rather than Text weight.

Stock Option Caliper (mm / in) Single 700 x 1000 mm Sheet Weight (kg / lb) Tube vs. Flat Suitability
300 gsm Art / Blue Core 0.28–0.31 mm (0.011–0.012 in) 0.21 kg (0.46 lb) Suitable for wide-diameter Kraft tubes or flat mailers
310 gsm Black-Core Linen 0.30–0.32 mm (0.012–0.013 in) 0.22 kg (0.48 lb) Suitable for wide-diameter tubes; linen emboss resists light scuffing
330 gsm Black Core 0.32–0.34 mm (0.013 in) 0.23 kg (0.51 lb) Suitable for wide-diameter tubes or flat mailers
350 gsm Art Stock 0.34–0.38 mm (0.013–0.015 in) 0.25 kg (0.54 lb) Flat mailers recommended to avoid permanent roll curl
400 gsm Art Stock 0.40–0.44 mm (0.016–0.017 in) 0.28 kg (0.62 lb) Flat mailers required; rolling creases fibers and cracks coatings
PVC (0.30 mm) 0.30 mm (0.012 in) — Flat mailers recommended for multi-sheet packs or heavy print
  • Lamination thickness: Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per sheet and increases stiffness, pushing 330 gsm laminated sheets toward flat-mailer packing.
  • Anti-scuff matte: Recommended for dark artwork to reduce visible rubbing marks during handling and interleaving.

Sheet Trim Margin and Prepress Imposition

Because the 700 x 1000 mm (27.6 in x 39.4 in) sheet remains untrimmed, the outer perimeter retains press-side artifacts that are normally guillotined off:

  • Gripper and tail margins: The leading edge (gripper) and trailing edge carry mechanical clamp marks, registration crosshairs, and CMYK/spot color control bars.
  • Card grid and bleed: Individual card slots on the sheet must include 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) internal safety margin, and ≥4–5 mm (0.157–0.197 in) safety margin for bordered card backs. Grid count and cell dimensions follow the chosen deck format without forcing a single default card trim.
  • Prepress files: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 at ≥300 DPI with outlined or embedded fonts, CMYK plus separate spot layers for foils or spot UV, 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) ≤280%–300%.

Tube vs. Flat Shipping Protection

Factor Rigid Kraft Tube Flat Corrugated Mailer
Best Use Case 1–5 unlaminated sheets (300–330 gsm) shipped individually Multi-sheet stacks, 350–400 gsm stocks, laminated or heavy-foil sheets
Surface Protection Roll sheets print-side out or with full tissue interleaving so layers do not rub Tissue-interleaved flat stack sandwiched between rigid corrugated backing boards
Edge & Corner Risk Low edge-crush risk when end caps are taped; ends can dent if sheets shift axially High corner-impact risk unless oversized by 25–50 mm (1.0–2.0 in) with corner guards
Flatness on Arrival Retains roll memory; requires counter-rolling or flat pressing after unboxing Arrives dead-flat for immediate framing or archival storage
Stack Weight Example 5 sheets at 330 gsm weigh 1.16 kg (2.55 lb) before tube weight 50 sheets at 330 gsm weigh 11.55 kg (25.46 lb) before pallet/box reinforcement

Job-Specific Production Steps

  1. Imposition & Proofing: Arrange the card fronts and backs onto the 700 x 1000 mm (27.6 in x 39.4 in) press layout with 3 mm (0.118 in) shared or guttered bleed, color bars, and separate spot/foil plates.
  2. Offset Printing & Surface Finishing: Print CMYK and spot inks, cure thoroughly, then apply lamination, anti-scuff matte, spot UV, or hot/cold foil across the full sheet.
  3. Pull Before Slitting: Divert the designated collector sheet count from the finishing line prior to guillotine slitting and die-cutting.
  4. Tissue Interleaving: Place one protective tissue sheet over the printed face of every press sheet before stacking or rolling.
  5. Tube or Flat Packing:
    • For tubes: Roll 1–5 interleaved sheets loosely to match the tube's inner diameter without kinking, insert into the Kraft tube with end-buffer paper, and tape both end caps securely.
    • For flat mailers: Stack interleaved sheets between stiff corrugated boards, wrap in moisture-barrier film, secure corner protectors, and seal inside a rigid double-wall mailer.

Sign-Off Criteria

Verify each batch against these physical checkpoints before sealing outbound packaging:

  • Front-to-back registration: Crosshairs and card borders align within press tolerance across all four quadrants of the 700 x 1000 mm (27.6 in x 39.4 in) sheet.
  • Foil and spot-UV alignment: Foil edges and spot coatings register cleanly over underlying artwork without flaking or bridging across card gutters.
  • Surface integrity: Dark solids and matte finishes show zero roller streaks, ink set-off, or scratch marks when inspected under raking light.
  • Edge and corner condition: Sheet perimeter is free of dog-eared corners, guillotine nicking, or moisture waviness.
  • Interleaving and pack fit: Every sheet has a dedicated tissue separator, and packed sheets show zero axial rattle in tubes or corner compression in flat mailers.

Concrete Failure Modes

  • Foil cracking and film delamination in tubes: Rolling 350–400 gsm stocks, double-sided laminated sheets, or large solid foil areas into narrow tubes fractures the coating along the curve and leaves permanent crease lines.
  • Ink set-off and scuffing: Stacking freshly cured dark-ink sheets without tissue interleaving transfers ink onto adjacent sheet backs and mars matte surfaces during transit vibration.
  • Permanent curl memory: Shipping 330 gsm or heavier sheets rolled for extended transit durations creates curl tension that resists flat framing.
  • Corner crushing in undersized flat mailers: Packing sheets flush to the mailer wall without rigid backing boards and corner clearance allows drop impacts to bend or split sheet corners.
  • End-cap blowout in Kraft tubes: Unsecured plastic caps pop off under axial shift from heavy multi-sheet rolls, exposing sheet edges to moisture and tearing.

Packaging & Regulatory Context

When distributing packaged uncut sheets into regulated markets, verify applicable packaging producer-responsibility registration and sorting-label rules against official requirements such as Germany's VerpackG packaging register and France's Triman sorting signage, and assess toy-safety obligations under EU EN 71 toy safety where products are marketed for children.