Full-bleed metallic foil or raised UV can run to the trim and bleed edge only when card edges remain raw, uncoated paperboard. As soon as a deck receives gilded foil or sprayed/dyed edge color, any raised resin or metallic layer crossing the cut path sits directly under the guillotine blade and edge-milling head, breaking adhesion at the perimeter. For broader multi-finish rules across coatings and substrates, see the finish compatibility guide.
Specifications and Compatibility Limits
| Parameter | Requirement for Gilded or Color-Edged Decks | Condition / Impact |
|---|---|---|
| Face decoration inset | 2–3 mm (0.079–0.118 in) inside trim line | Prevents blade shear and milling snag on hot foil, cold foil, and raised spot UV |
| CMYK bleed | 3 mm (0.118 in) per side | Base ink extends past trim; only specialty face layers pull back |
| Interior safety margin | ≥3 mm (0.118 in); ≥4–5 mm (0.157–0.197 in) for bordered backs | Keeps critical text and borders clear of trim and corner variance |
| Corner radius | R3–R3.5 mm (0.118–0.138 in) | Face accents must clear the corner arc by 2–3 mm (0.079–0.118 in) |
| File & spot setup | AI/PDF/PSD; PDF/X-1a or PDF/X-4; ≥300 DPI | Separate vector spot layers for each foil or raised UV pass; fonts outlined or embedded |
| Ink & dark-art limits | 100% K fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% | Anti-scuff matte suits dark artwork without overloading edge fibers |
| Stock & film caliper | 300–400 gsm (Cover LB, 20 × 26 in basis; distinct from Text LB, 25 × 38 in) or 0.30 mm (0.012 in) PVC | Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card; thick lamination can conflict with gilded edges |
| Offset run minimum | 200 decks (usual tiers: 200 / 300 / 500 / 1,000+) | Standard offset card tiers with specialist manufacturing partners |
Different deck formats follow the same 2–3 mm (0.079–0.118 in) perimeter inset regardless of card dimensions. Because edge finishing acts on the outer 0.1–0.3 mm (0.004–0.012 in) of the stacked block, changing card width or height does not reduce shear stress at the cut line.
Production Sequence
- Prepress separation: Build CMYK base art with 3 mm (0.118 in) bleed, then offset hot foil, cold foil, and raised spot UV vector masks 2–3 mm (0.079–0.118 in) inward from the dieline and R3–R3.5 mm (0.118–0.138 in) corner arcs.
- Offset printing and base coat: Print CMYK sheets and apply a thin, edge-compatible protective coating (such as anti-scuff matte on dark artwork) rather than thick lamination that resists edge-foil bonding.
- Face decoration: Apply cold foil, hot foil stamping, or raised spot UV curing within the inset zone before sheet cutting.
- Trimming and corner rounding: Guillotine-cut sheets to finished card size and round corners cleanly through bare or lightly coated paperboard rather than through cured UV resin or foil.
- Block clamping and edge finishing: Clamp the trimmed deck stack under pressure, mill or sand the stack edges smooth, and apply gilding foil or edge color across the uniform paper edge.
Sign-Off Criteria
- Prepress proof: Spot-layer overlays sit 2–3 mm (0.079–0.118 in) inside the trim line and corner curves on every face and back plate, with TAC ≤280%–300%.
- Cut-edge inspection: Trimmed, un-gilded cards show clean paperboard fibers at the perimeter with zero foil flake, UV ridge, or film delamination at the cut line.
- Finished deck stack: Gilded or colored edges show continuous, even adhesion across all four sides and corners without bridging between adjacent cards or lifting at face-accent boundaries.
Failure Modes
- Shear flaking: Guillotine blade compression fractures brittle raised spot UV or metallic foil layers that cross the trim line, leaving ragged chips and exposed adhesive along the card border.
- Milling snag: Edge-preparation sanding or milling catches raised UV edges or foil lips exposed at the perimeter, tearing face accents inward across the card face.
- Edge-foil overlap failure: Gilding foil and edge pigment bond poorly to cured UV resin, metallic face foil, or thick lamination at the cut edge, causing patchy edge color, flaking during shuffling, or cards sticking together after hot-foil edge pressing.
Parent guide Finish Compatibility