Conditions that change the choice:
- Heavy ink coverage on the card face: High total area coverage (TAC above 280%–300%) combined with a hard flood UV layer increases edge brittleness during guillotine trimming and corner rounding; aqueous or poker varnish is more forgiving on dark, full-bleed borders.
- Paper vs. PVC substrate: Paper cores absorb edge-coloring dyes and water- or solvent-based edge inks, whereas non-porous PVC (0.30 mm / 0.012 in) requires UV-curable or solvent-receptive edge inks and tighter mechanical prep so pigment does not wipe off in play.
- Deck thickness and run size: Standard offset runs with specialist manufacturing partners start at 200 decks (usual tiers 200, 300, 500, and 1,000+); thicker stocks (350–400 gsm) build taller clamped blocks per deck, increasing heat and pressure sensitivity during edge sanding and foil transfer.
Specifications: Liquid Coatings, Substrates, and Prepress Limits
Card stocks for offset decks are specified in grams per square meter (gsm). In US paper conventions, cardstocks sit in Cover LB weights (calculated from a 20 × 26 in / 508 × 660 mm basis sheet) rather than Text LB weights (calculated from a 25 × 38 in / 635 × 965 mm basis sheet); for reference, a 300 gsm sheet corresponds to roughly 111 lb Cover (about 50.3 kg / 110.9 lb per 500-sheet Cover basis ream).
| Parameter | Specification | Imperial / Notes |
|---|---|---|
| Minimum offset run | 200 decks (tiers: 200 / 300 / 500 / 1,000+) | Project/component minimums apply to boxed sets |
| 300 gsm art / blue core | 0.28–0.31 mm caliper | 0.011–0.012 in |
| 310 gsm black-core linen | 0.30–0.32 mm caliper | 0.012–0.013 in |
| 330 gsm black core | 0.32–0.34 mm caliper | 0.013–0.013 in |
| 350 gsm art stock | 0.34–0.38 mm caliper | 0.013–0.015 in |
| 400 gsm art stock | 0.40–0.44 mm caliper | 0.016–0.017 in |
| PVC stock | 0.30 mm caliper | 0.012 in; non-absorbent polymer |
| Double-sided film (reference conflict) | Adds 0.03–0.05 mm per card | 0.001–0.002 in; thick lamination conflicts with gilded edges |
| Bleed | 3 mm per side | 0.118 in |
| Safety margin | ≥3 mm (≥4–5 mm for bordered backs) | ≥0.118 in (≥0.157–0.197 in for bordered backs) |
| Corner radius | R3–R3.5 mm | 0.118–0.138 in |
| Color & ink limits | CMYK + separate spot layers, ≥300 DPI | Rich black C40–60 M30–40 Y30–40 K100; 100% K fine text; TAC ≤280%–300% |
Inch conversions use 25.4 mm = 1 in.
How Liquid Coatings Compare on the Edge
- Aqueous coating: Water-based dispersion applied inline on offset presses. It penetrates lightly into paper fibers, dries flat with minimal surface film build, and sands cleanly without gumming abrasive belts.
- Poker varnish: Slip-tuned oil- or water-based varnish formulated for card handling. Because it contains slip agents (waxes or silicones), excess varnish near the cut line can reduce edge-ink wetting or foil adhesion unless removed during edge milling.
- Flood UV coating: Instant-cured liquid polymer offering high gloss or matte rub resistance (anti-scuff matte suits dark artwork). Flood UV forms a harder, more brittle surface skin than aqueous coating, requiring sharp guillotine knives and controlled milling so the cured resin does not micro-chip along the trim edge.
Production Steps: Trimming, Milling, Gilding, and Edge Coloring
For any deck format, edge finishing happens after sheets are coated, cured, trimmed, and collated into clamped deck blocks.
- Press Printing and Coating Cure
- Sheets are printed in CMYK (with separate spot layers for any specialty face effects) at ≤280%–300% TAC and coated with aqueous, poker varnish, or flood UV.
- Coated sheets must reach full cure before stacking under heavy weight; uncured liquid varnish or UV under clamp pressure transfers tack to the sheet edge and causes cards to weld together during trimming.
- Guillotine Trimming and Corner Rounding
- Sheets are trimmed to the job's assigned dimensions with 3 mm (0.118 in) bleed removed per side, then die-punched to R3–R3.5 mm (0.118–0.138 in) corners.
- Because liquid coatings have negligible thickness compared to plastic film, the guillotine blade shears paper fibers and cured varnish cleanly without dragging a soft polymer lip over the card edge.
- For non-standard deck dimensions, clamp pressure and knife bevel angle are adjusted to the stock caliper and deck block height so the top and bottom cards do not flare.
- Block Clamping and Edge Milling (Sanding)
- Finished decks are stacked and clamped under uniform mechanical or hydraulic pressure (typically holding multiple decks in a rigid block weighing several kg / lb depending on card count and caliper) so no air gaps remain between cards.
- A fine-grit milling head or sanding belt skims the clamped edges. This step levels microscopic trim steps, removes residual slip agents from poker varnish, and opens clean paper fibers (or lightly scuffs PVC) for uniform contact.
- Hot-Foil Gilding
- While still clamped flat, heated brass or silicone rollers press metallic or pigment foil onto the milled edges.
- Film-free coatings tolerate gilding heat without shrinking, bubbling, or delaminating at the card perimeter—unlike thick plastic lamination, which softens under heat and creates a raised barrier that blocks foil release.
- After foil cooling, decks are fanned and flexed to break the inter-card foil bridge cleanly along each card's R3–R3.5 mm (0.118–0.138 in) corner and straight edges.
- Edge Coloring (Paper vs. PVC Workflow)
- Paper substrates (300–400 gsm art, blue-core, or black-core): Milled paper edges accept roller-applied or sprayed edge ink directly into the exposed fibers. Controlled ink viscosity prevents deep wicking past the edge into the ≥3 mm (0.118 in) safety zone or ≥4–5 mm (0.157–0.197 in) bordered-back margin.
- PVC substrates (0.30 mm / 0.012 in): Non-porous PVC cannot absorb water-based dyes. Edge coloring on PVC requires UV-curable or solvent-based edge inks matched to the polymer surface, followed by immediate UV pinning or flash drying while clamped so the pigment bonds mechanically and chemically without smearing onto the card face.
Sign-Off Criteria
- Prepress files: AI, PDF, or PSD supplied as PDF/X-1a or PDF/X-4, with outlined or embedded fonts, ≥300 DPI raster art, 3 mm (0.118 in) bleed on all sides, and separate spot layers for any specialty finishes.
- Physical edge inspection: Under raking light, milled and gilded/colored deck blocks show zero step lines, no foil bridging across card faces, and uniform color saturation around the R3–R3.5 mm (0.118–0.138 in) corners.
- Flex and fan check: After breaking a gilded or edge-colored deck, individual cards separate smoothly without sticking, flaking foil, or lifting the face varnish along the perimeter.
- Regulatory documentation (when applicable): For decks marketed as toys or intended for children in the EU, edge inks, coatings, and foils are subject to EN 71 assessment and testing under the EU Toy Safety framework, with batch material records retained alongside the finished deck specifications.
Concrete Failure Modes
| Failure Mode | Root Cause | Physical Outcome | Prevention |
|---|---|---|---|
| Edge chipping / white flecks | Brittle flood UV over high TAC (>300%) or dull guillotine blade | Cured coating fractures at the cut line, exposing white paper core along dark borders | Keep TAC ≤280%–300%; use aqueous or anti-scuff matte varnish on dark full-bleed art; sharpen blades before trimming |
| Foil peeling or patchy gilding | Slip agents in poker varnish not removed by sanding, or uneven block clamping | Foil fails to anchor to the card edge and lifts off when the deck is fanned | Perform a full-perimeter edge milling pass prior to gilding; verify uniform clamp pressure across the block |
| Edge-ink wicking (bleed-in) | Low-viscosity edge ink on porous, lightly sized paper cores | Edge color capillaries inward 1–2 mm (0.039–0.079 in) onto the card face or back border | Use higher-viscosity edge ink, clamp tightly to seal face-to-face gaps, and maintain ≥4–5 mm (0.157–0.197 in) bordered-back margins |
| Edge-ink beading / rub-off | Water-based edge ink applied to 0.30 mm (0.012 in) PVC | Ink pools on the non-absorbent plastic edge and wipes onto hands during shuffling | Route PVC decks to UV-curable or solvent-receptive edge-ink systems with fine mechanical scuffing |
| Corner-rounding tear or foil snag | Uncured varnish buildup or film-lamination overhang at R3–R3.5 mm (0.118–0.138 in) corners | Corners show ragged fuzz or foil bridges that rip the coating when separated | Confirm full face-coating cure before die-cutting; avoid thick film lamination on gilded decks |
Guides in this section
Parent guide Finish Compatibility
Related guides
- BOPP Lamination and Edge Finishing Compatibility
- Full-Bleed Face Decoration and Edge Finishing Compatibility
- Soft-Touch Lamination and Edge Finishing Compatibility
- Varnish Coatings and Hot Foil Stamping Compatibility