Within decorative finishes, flat spot UV is the right choice when you want selective gloss highlights—such as logos, frames, icons, or subtle background patterns—that sit flush with the card surface and slide cleanly in shuffles and card boxes.

Choose a different finish when conditions change:

  • Need tactile relief: Flat spot UV has negligible thickness; switch to raised/embossed spot UV if players need to feel the pattern with their fingertips.
  • Unlaminated dark artwork: Applying spot UV directly to uncoated or unlaminated dark ink reduces visual contrast and leaves the surrounding dark ink vulnerable to scuffing. Pair flat spot UV with an anti-scuff matte film base on dark artwork.
  • Gilded edges on thick decks: Double-sided film lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card and thick lamination can conflict with gilded edges; verify edge-finishing compatibility before combining heavy film bases with edge gilding.

Specifications and Surface Limits

Flat spot UV relies on surface-energy and sheen contrast between the cured gloss polymer and the underlying sheet, while keeping mechanical caliper unchanged.

  • Minimum run: Standard offset cards start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks). Boxed games and dedicated tooling follow project and component minimums.
  • Compatible substrates:
    • 300 gsm art or blue-core stock: 0.28–0.31 mm (0.011–0.012 in)
    • 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in)
    • 330 gsm black-core stock: 0.32–0.34 mm (0.0126–0.0134 in)
    • 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in)
    • 400 gsm card stock: 0.40–0.44 mm (0.016–0.017 in)
    • PVC stock: 0.30 mm (0.012 in)
    • Note on paper weight units: Card stocks in the 300–400 gsm range correspond to heavy US Cover LB (measured on a 20 × 26 in / 508 × 660 mm basis sheet), whereas interior booklet papers (80–120 gsm) are measured as US Text LB (25 × 38 in / 635 × 965 mm basis sheet).
  • Base lamination: Double-sided film lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card. Anti-scuff matte lamination suits dark artwork and provides the flat, low-glare background that maximizes flat spot UV contrast.
  • Artwork and prepress files:
    • Formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4, with all fonts outlined or embedded.
    • Resolution: ≥300 DPI for all raster elements.
    • Spot channel setup: Provide spot UV artwork as a separate, 100% solid spot-color layer (vector preferred) aligned to the CMYK artboard—never flattened into CMYK.
    • Ink limits: Use 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100 for solid dark areas, and keep total area coverage (TAC) at ≤280%–300%.
    • Bleed and safety: 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety margin from trim, increasing to ≥4–5 mm (0.157–0.197 in) for bordered backs.
    • Corners: R3–R3.5 mm (0.118–0.138 in) corner radius. Keep spot UV zones inside the safety margin so polymer does not cross die-cut edges or rounded corners.

Production Steps

  1. Prepress separation: Verify the CMYK artwork and separate spot UV layer share identical trim, bleed (3 mm / 0.118 in), and registration marks. Confirm TAC does not exceed 280%–300% beneath coated zones.
  2. Offset printing and curing: Print CMYK layers on the selected card stock (300–400 gsm or 0.30 mm / 0.012 in PVC) and allow press sheets to dry fully before lamination or coating.
  3. Base film lamination: Apply matte or anti-scuff matte film across both sides of the sheet when high contrast and scuff resistance are required.
  4. Selective UV application: Transfer the clear liquid UV polymer onto the designated artwork zones using a dedicated coating plate or screen registered to the sheet guides.
  5. UV lamp curing: Pass sheets under UV lamps to polymerize the coating instantly into a hard, flush gloss layer.
  6. Slitting, die-cutting, and corner rounding: Cut sheets to the final deck format, round corners to R3–R3.5 mm (0.118–0.138 in), and collate decks. Because flat spot UV adds no measurable stack height, box clearance remains governed by the base stock and film (1.5–2.5 mm / 0.059–0.098 in across width/height and 1.5–3 mm / 0.059–0.118 in for stack height).

Sign-Off Criteria

  • Registration accuracy: Spot UV edges align cleanly with underlying CMYK artwork shapes without visible haloing or offset drift.
  • Sheen contrast and uniformity: Coated zones show consistent, pinhole-free gloss against the matte or anti-scuff matte base, with sharp boundaries.
  • Full cure and surface slip: Coated areas are dry, non-tacky, and free of blocking when stacked under pressure.
  • Edge integrity: No chipping, flaking, or lifting along trim lines or R3–R3.5 mm (0.118–0.138 in) corners.
  • Stack height stability: Total deck caliper matches the base card stock plus any applied film lamination, fitting the planned box clearance.

Concrete Failure Modes

  • Registration drift on micro-details: Thin outlines, hairlines, and small 100% K text show visible misalignment when mechanical sheet-feed tolerances shift slightly between printing and UV coating. Keep spot UV on bold graphic zones, titles, and frames rather than fine body text.
  • Edge peeling and chipping: Running spot UV out to the trim line or across R3–R3.5 mm (0.118–0.138 in) rounded corners exposes the polymer edge to blade shear during cutting, causing the coating to lift during shuffling. Stop spot UV inside the ≥3 mm (0.118 in) safety margin—or ≥4–5 mm (0.157–0.197 in) on bordered backs—unless full-bleed flood coating is intended.
  • Weak visual contrast: Applying flat spot UV over an unlaminated gloss or semi-gloss paper surface reduces the sheen differential until highlights are barely visible. Pair flat spot UV with matte or anti-scuff matte lamination, especially over rich black (C40–60 M30–40 Y30–40 K100) backgrounds.
  • Adhesion failure or orange-peel texture: Coating over uncured offset ink or areas exceeding 280%–300% TAC prevents proper wetting and curing, leaving blotchy gloss or flaking spots. Enforce TAC limits in prepress and allow full ink drying before coating.