Choose offset metallic spot ink when artwork combines fine linework, halftone tints, or small accents with CMYK graphics on standard card runs (starting at 200 decks; usual tiers 200, 300, 500, and 1,000+ decks). Choose screen metallic ink when a project requires heavier, more opaque flake laydown on dark or uncoated substrates and meets component minimums. When a design requires mirror-like specular reflection rather than satin shimmer, select foil stamping instead under Decorative Finishes.
Substrate smoothness and topcoats directly alter the final luster:
- Smooth coated stocks (such as 300 gsm art/blue core or 350 gsm art stock) allow metal flakes to lie flat near the surface for higher sheen.
- Textured or porous stocks (such as 310 gsm black-core linen or uncoated paper) scatter light across fibers and emboss patterns, softening the metallic effect.
- Protective coatings (aqueous varnish or film lamination) lock flakes against shuffling friction; anti-scuff matte lamination protects dark backgrounds from finger marks while further muting metallic brightness.
Specifications and Compatibility
| Parameter | Requirement / Range | Notes |
|---|---|---|
| Minimum run | 200 decks (offset cards); project minimums for boxes/screen | Usual card tiers: 200, 300, 500, 1,000+ decks |
| File format & color | AI, PDF, or PSD; PDF/X-1a or PDF/X-4; ≥300 DPI | CMYK process builds + separate named spot-ink layers |
| Ink limits & black | TAC ≤280%–300%; 100% K for fine text | Rich black: C40–60 M30–40 Y30–40 K100 |
| Fonts | Outlined or embedded | Avoid knocking tiny text out of metallic fills |
| Bleed & safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety | ≥4–5 mm (0.157–0.197 in) safety for bordered backs |
| Card corners | R3–R3.5 mm (0.118–0.138 in) | Standard die-cut corner radius |
| Card stocks | 300–400 gsm paperboard; 0.30 mm (0.012 in) PVC | Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card |
| Box & board greyboard | 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) | 15–20 mm (0.591–0.787 in) wrap margin |
| Booklet stocks | 200–300 gsm cover; 80–120 gsm interior | Interior caliper ~0.08–0.13 mm (0.003–0.005 in) per sheet |
Card and cover weights in the 200–400 gsm range correspond to US Cover LB (measured on a 20 × 26 in / 508 × 660 mm basis sheet), whereas 80–120 gsm booklet interior papers correspond to US Text LB (measured on a 25 × 38 in / 635 × 965 mm basis sheet).
Compatible card calipers before lamination:
- 300 gsm art/blue core: 0.28–0.31 mm (0.011–0.012 in)
- 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in)
- 330 gsm black core: 0.32–0.34 mm (0.013 in)
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in)
- 400 gsm art/board: 0.40–0.44 mm (0.016–0.017 in)
Production Steps
- Separate spot channels in prepress: Place all metallic ink elements on dedicated spot-color layers separate from CMYK. Set CMYK layers to knock out beneath solid metallic fills so process pigments do not muddy the flake reflection, and apply trapping to fine metallic borders.
- Image plates or screens: Output dedicated offset plates (for fine detail and multi-deck card runs) or screen stencils (for heavier metallic coverage on rigid wraps or dark components).
- Print and cure: Run suspended aluminum (cool silver) or bronze (gold/copper) flake ink at controlled press density so flakes align parallel to the sheet. Allow full drying or curing before stacking to prevent ink set-off.
- Seal with varnish or film: Apply an overprint varnish or double-sided film lamination (adding 0.03–0.05 mm / 0.001–0.002 in per card) to encapsulate surface flakes, then proceed to corner rounding (R3–R3.5 mm / 0.118–0.138 in), box wrapping, or booklet binding.
Sign-Off Criteria
- Prepress proof: Spot layer separates cleanly from CMYK in PDF/X-1a or PDF/X-4; 3 mm (0.118 in) bleed and ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in on bordered backs) are intact; fine text uses 100% K; TAC stays ≤280%–300%.
- Press sheet inspection: Metallic areas show even satin sheen without mottling or streaking, sharp edges on fine rules, and tight registration against adjacent rich black or CMYK elements.
- Coating and fit check: Sealed metallic surfaces resist rub-off during handling; anti-scuff matte surfaces remain uniform over dark artwork; finished deck stack height and box dimensions maintain 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack height clearance.
- Regulatory documentation (when applicable): For tabletop products subject to toy safety rules, retain ink safety data sheets and finished-component records for EN 71 assessment and testing as outlined on the European Commission Toy Safety portal.
Concrete Failure Modes
- Flake rub-off and tarnishing: Leaving metallic spot ink unvarnished or unlaminated exposes aluminum and bronze flakes to skin oils and card-on-card friction, causing dark smudging and dulling.
- Muddied metallic tone: Overprinting metallic spot ink on top of heavy CMYK builds—or failing to knock out CMYK underneath—mixes translucent process pigments with the metal flakes, turning silver grey or gold brownish.
- Reduced sheen on textured or uncoated stock: Linen embossing (such as 310 gsm black-core linen) or uncoated paper disrupts flat flake alignment, scattering light and producing a flat, granular appearance.
- Halos around small knocked-out text: Setting fine body text as a knockout inside a metallic spot fill causes visible paper-white fringes if press registration shifts slightly; keep fine text at 100% K instead.
- Edge conflict with thick lamination and gilding: Combining thick protective film over metallic-printed cards with gilded edges can interfere with edge adhesion or cause perimeter peeling; align coating thickness with edge treatments under Decorative Finishes.