For the broader finish mechanics and substrate rules, see Raised 3D UV. On rulebook covers, hardcover case wraps, and heavyweight postcards, raised UV relies on a rigid outer sheet and a matte or anti-scuff matte base film so the cured polymer bonds cleanly without cracking under folding, binding, or guillotine shear.

Selection Conditions and Weight Thresholds

  • Rulebook and booklet covers (250–300 gsm): Ideal for raised UV when paired with a matte base film. Covers at 200 gsm sit at the lower boundary of booklet cover stock (200–300 gsm) and flex more readily under heavy UV buildup; stepping up to 250–300 gsm prevents curl and keeps tactile peaks crisp.
  • Hardcover art books: Apply raised UV only to the outer printed wrap before case-making onto 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard. Keep the 15–20 mm (0.591–0.787 in) wrap margin and board hinge channels completely free of raised UV, and leave interior endpapers uncoated so they bond flat to the board.
  • Postcards: Treat heavyweight postcards like single-sheet covers at 250–300 gsm or above (up to 350–400 gsm card stocks where rigidity is required). Keep raised UV clear of the guillotine trim line and postal/writing zones.
  • Interior signatures (80–120 gsm): Unsuitable for raised UV. At roughly 0.08–0.13 mm (0.0031–0.0051 in) per sheet, interior text stock lacks the stiffness to support cured UV peaks without cockling or showing through.

Specifications

Cover Stock and Basis Weight Distinctions

In US paper specifications, pound (lb) weights depend on the uncut basis sheet size, so Text LB and Cover LB are not interchangeable:

  • Cover LB (20 × 26 in / 508 × 660.4 mm basis sheet): Used for booklet covers and postcards. A 250–300 gsm cover stock corresponds to approximately 92–111 lb Cover, while a lighter 200 gsm cover is approximately 74 lb Cover.
  • Text LB (25 × 38 in / 635 × 965.2 mm basis sheet): Used for interior booklet and art book pages. Standard 80–120 gsm interior stock corresponds to approximately 54–81 lb Text.

Spine-Hinge Margins, Binding, and Trim Clearances

  • Binding formats (signatures in multiples of 4):
    • Saddle stitch (12–40 pages): Keep raised UV off the center spine fold so the cover does not crack when stapled and folded flat.
    • Perfect binding (28+ pages): Keep raised UV off the spine face and the side hinge-score lines where the cover flexes open.
    • Sewn binding (80–100+ pages recommended) and hardcover art books: Keep raised UV clear of the spine, hinge joints, and the 15–20 mm (0.591–0.787 in) greyboard wrap turn-in so the wrap folds smoothly around the 1.5–3 mm (0.059–0.118 in) board edges.
  • Guillotine-trim clearances: Maintain 3 mm (0.118 in) bleed per side on all cover, wrap, and postcard artwork, and keep raised UV elements at least ≥3 mm (0.118 in) inside the trim line (≥4–5 mm / 0.157–0.197 in for bordered backs and postcards) so the guillotine clamp and blade do not shear cured polymer.
  • Base lamination compatibility: Pair raised UV with a matte or anti-scuff matte film—especially on dark artwork—to create tactile and gloss contrast while protecting against rub marks. Double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) to sheet thickness.

Prepress and File Setup

  • Formats and color: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 at ≥300 DPI in CMYK with a separate vector spot layer dedicated to the raised UV mask.
  • Type and ink limits: Outline or embed all fonts, use 100% K for fine text, build deep darks with rich black (C40–60 M30–40 Y30–40 K100), and keep Total Area Coverage (TAC) at ≤280%–300%.

Production Steps

  1. Prepress separation: Separate the CMYK print layers from the raised UV spot layer. Verify that the spot mask stops inside the ≥3 mm (0.118 in) trim safety zone (≥4–5 mm / 0.157–0.197 in for bordered backs) and clears all spine scores, hinge channels, and 15–20 mm (0.591–0.787 in) wrap margins.
  2. Offset printing and base lamination: Print the CMYK cover or postcard sheet, cure the ink, and apply matte or anti-scuff matte lamination to provide a uniform, scuff-resistant foundation.
  3. Raised UV application and curing: Deposit the high-build UV polymer onto the outer cover face according to the spot layer and cure immediately under UV lamps, leaving interior endpapers and inside spreads flat.
  4. Scoring, trimming, and binding: Guillotine-trim postcards and covers outside the UV mask, score spine and hinge lines through clear un-coated channels, and complete saddle-stitching, perfect-binding, sewn-binding, or greyboard case-wrapping.

Sign-Off Criteria

  • Spot-to-CMYK registration: Raised UV peaks align cleanly over underlying printed graphics with no haloing or offset bleed.
  • Clear hinges and trim margins: Zero raised UV sits on spine folds, hinge scores, greyboard wrap turn-ins, or within the ≥3 mm (0.118 in) guillotine safety zone.
  • Flat interiors and intact edges: Interior endpapers and text signatures remain flat and unblemished; trimmed postcard and cover edges show clean paper/board cuts with no polymer chipping.
  • Surface integrity on dark solids: Dark rich black areas (C40–60 M30–40 Y30–40 K100, TAC ≤280%–300%) show uniform matte/anti-scuff contrast without scuffing around the UV peaks.

Failure Modes

  • Spine-hinge cracking and flaking: Extending raised UV across saddle-stitch folds, perfect-bound hinge scores, or hardcover board joints causes the rigid cured polymer to fracture when the book opens.
  • Guillotine edge chipping and delamination: Placing raised UV inside the 3 mm (0.118 in) bleed or ≥3 mm (0.118 in) safety margin exposes the polymer ridge to guillotine clamp pressure and blade shear, lifting the coating along the cut edge.
  • Cover curl and show-through: Applying heavy raised UV buildup to stocks below 250–300 gsm (such as 200 gsm covers or 80–120 gsm interior pages) pulls the sheet toward the coated side as the polymer cures.
  • Scuffing on dark backgrounds: Running raised UV directly over unlaminated dark CMYK solids leaves surrounding areas vulnerable to rub marks during trimming, binding, and stacking; an anti-scuff matte base film prevents this wear.