For general polymer curing and substrate behavior across non-deck print items, see the parent Raised 3D UV guide. On playing and tarot cards, restrict raised UV to centered or balanced interior motifs, pair it with a compatible base film such as anti-scuff matte on dark artwork, and size the tuck or rigid box after measuring the finished deck height.
When Raised UV Fits Playing and Tarot Cards
Card decks amplify small surface variations by the card count. A single sheet or box lid tolerates localized polymer build, whereas a 54-card playing deck or 78-card tarot deck multiplies that height across every card in the stack.
- Balanced card backs vs. asymmetric faces: Centered, symmetrical raised UV on card backs distributes height across the deck center. Placing heavy raised UV in one corner or across varying face artwork areas creates a wedge-shaped stack.
- Deck count and base caliper: Standard offset card runs start at 200 decks (usual tiers are 200, 300, 500, and 1,000+ decks). Moving from 54 cards to 78 cards increases cumulative polymer build by 44%, tightening the margin inside the box.
- Shuffle handling: Full-bleed or high-relief patterns near card edges catch during riffle and overhand shuffles. Smooth, low-area interior accents preserve consistent card slip.
- Edge finishing compatibility: Thick lamination combined with raised UV build interferes with stack compression and clean foil transfer on gilded edges.
Specifications for Stack Balance, Box Fit, and Card Stock
Card stocks for playing and tarot decks are specified in gsm and Cover LB (calculated on a 20 × 26 in basis sheet, distinct from Text LB on a 25 × 38 in basis sheet). Double-sided lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card before any raised UV is applied.
| Stock / Component | Weight / Spec | Caliper / Allowance (mm) | Caliper / Allowance (in) | Role in Raised UV Decks |
|---|---|---|---|---|
| Art / blue core | 300 gsm (Cover LB) | 0.28–0.31 mm | 0.0110–0.0122 in | Lighter deck baseline; lower stack rigidity |
| Black-core linen | 310 gsm (Cover LB) | 0.30–0.32 mm | 0.0118–0.0126 in | Embossed linen texture alters UV leveling |
| Black core | 330 gsm (Cover LB) | 0.32–0.34 mm | 0.0126–0.0134 in | Common card balance for 54–78 card stacks |
| Art stock | 350 gsm (Cover LB) | 0.34–0.38 mm | 0.0134–0.0150 in | Higher stiffness resists localized curl |
| Heavy art stock | 400 gsm (Cover LB) | 0.40–0.44 mm | 0.0157–0.0173 in | Thickest paper stack; tightest box allowance |
| Plastic card stock | PVC | 0.30 mm | 0.0118 in | Non-absorbent surface; requires compatible ink/UV adhesion |
| Double-sided film | Matte / anti-scuff matte | +0.03–0.05 mm | +0.0012–0.0020 in | Adds to every card; anti-scuff matte suits dark art |
| Box width/height clearance | Per side total | 1.5–2.5 mm | 0.059–0.098 in | Prevents tight edge binding during insertion |
| Box stack clearance | Stack height allowance | 1.5–3 mm | 0.059–0.118 in | Absorbs stock tolerance plus raised UV build |
Calculate the target stack height before finalizing box dielines:
Total Deck Height = (Card Count * (Base Stock Caliper + Film Thickness)) + (Card Count * Local Raised UV Build)
Prepress and Trim-Edge Parameters
- File formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts.
- Color and ink limits: CMYK at ≥300 DPI with a separate vector spot layer for the raised UV mask; 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) ≤280%–300%.
- Bleed, safety, and corners: 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin for artwork and raised UV (≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (0.118–0.138 in) rounded corners.
Job-Specific Production Steps
- Spot-layer zoning and area balancing: Place all raised UV shapes inside the ≥3 mm (0.118 in) safety zone—or ≥4–5 mm (0.157–0.197 in) on bordered backs—and clear of the R3–R3.5 mm (0.118–0.138 in) corner curves. Balance coverage across opposing quadrants on card backs so the deck compresses evenly.
- Offset printing and base lamination: Print CMYK sheets within the ≤280%–300% TAC limit and apply double-sided film (adding 0.03–0.05 mm / 0.0012–0.0020 in per card). Use anti-scuff matte film on dark card designs so raised UV sits cleanly without scuff marks from press handling.
- Raised UV application and curing: Deposit and UV-cure the polymer layer in register with the printed CMYK artwork. Maintain uniform polymer build across all sheet positions so card-to-card height stays consistent across the 54 or 78 card layout.
- Die-cutting, corner rounding, and box sizing: Cut cards and round corners to R3–R3.5 mm (0.118–0.138 in). Measure the finished stacked deck height across all 54 to 78 cards and verify that the box dieline maintains 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack height clearance.
Sign-Off Criteria
- Stack plumbness: A full 54-card or 78-card stack sits flat on a level surface without tilting, rocking, or fanning open on one side.
- Box clearance: The finished deck slides into and out of its box smoothly, preserving 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack clearance without crushing card corners.
- Edge and corner integrity: Trim borders and R3–R3.5 mm (0.118–0.138 in) corners show clean paper or PVC cuts with zero polymer cracking, flaking, or film lifting.
- Registration and shuffle slip: Raised UV aligns cleanly to underlying CMYK elements, and cards fan and riffle-shuffle without catching on adjacent UV ridges.
Concrete Failure Modes
- Asymmetric stack lean and box jamming: Heavy raised UV concentrated on one side or corner across 54 to 78 cards creates a wedge stack. The thick edge exceeds the 1.5–3 mm (0.059–0.118 in) stack clearance and binds against the box flap or lid.
- Trim-edge chipping and corner delamination: Extending raised UV into the 3 mm (0.118 in) bleed or closer than the ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in on bordered backs) puts cured polymer under the cutting rule and R3–R3.5 mm (0.118–0.138 in) corner die, fracturing the brittle resin along the card perimeter.
- Shuffle catching and deck clumping: Dense or sharp-stepped raised UV near card edges hooks neighboring cards during riffle shuffles and creates localized friction pockets that cause cards to stick in pairs.
- Gilded-edge and thick-film conflicts: Combining thick lamination with raised UV build prevents even stack clamping during edge finishing, resulting in broken or uneven gilded edges.
Parent guide Raised 3D Tactile UV