Part of the Card Deck Press manufacturing glossary.
Specifications and Tolerances
| Parameter | Specification | Notes |
|---|---|---|
| Rigid greyboard thickness | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), 3 mm (0.118 in) | Selected by board span, rigidity target, and folding or puzzle die requirements |
| Wrap margin | 15–20 mm (0.591–0.787 in) | Allowance extending past the board edge for turned-in wrapped boards |
| Punchboard die gap | 3–4 mm (0.118–0.157 in) | Minimum spacing between die-cut tokens or pieces on mounted punchboards |
| Prepress bleed | 3 mm (0.118 in) per side | Required on all printed facing and liner sheets |
| Prepress safety margin | >= 3 mm (0.118 in) | Minimum distance from trim, fold, or die line to critical graphics |
| Print resolution and color | >= 300 DPI, CMYK with separate spot layers | PDF/X-1a or PDF/X-4; TAC <= 280%–300% |
| Surface film thickness | 0.03–0.05 mm (0.001–0.002 in) | Combined caliper added when double-sided film is applied; anti-scuff matte suits dark artwork |
Facing and backing papers are specified in grams per square meter (gsm) for cross-market consistency. When converting to US pound weights, Text LB (measured on a 25 x 38 in / 635 x 965 mm basis sheet) and Cover LB (measured on a 20 x 26 in / 508 x 660 mm basis sheet) represent different sheet areas and cannot be compared by pound number alone. For example, an 80–120 gsm interior-weight sheet corresponds to lighter Text LB stock, whereas 200–300 gsm heavier sheets fall into Cover LB territory.
Adhesive Bond, Moisture, and Stress Balance
A mounted board is a layered composite: a printed facing sheet, an adhesive layer, a rigid greyboard core, and typically a backing liner. When wet adhesive is applied, the paper fibers in the facing sheet absorb moisture and expand. As the assembly dries, the moisture evaporates and the facing sheet contracts, creating tensile stress across the glue line.
- Unequal contraction: If only one side of the greyboard is mounted, the contracting facing pulls that side inward while the unmounted back remains stable, producing a concave bow toward the printed face.
- Counter-lining: Mounting a matching backing sheet (liner) onto the reverse face introduces an opposing contraction force during drying, neutralizing directional pull and keeping the board flat.
- Grain direction: Aligning the paper grain of the facing sheet, greyboard, and backing liner prevents diagonal twist caused by cross-grain expansion differences.
- Lamination tension: Applying a surface film such as anti-scuff matte lamination before mounting seals the outer face against ambient humidity, but if the reverse side lacks a comparable barrier, rapid changes in environmental moisture can still bow the board.
Production Steps
- Prepress and sheet finishing: Output facing artwork at >= 300 DPI in CMYK with separate spot layers, 3 mm (0.118 in) bleed per side, and >= 3 mm (0.118 in) safety margin. Apply surface lamination (such as anti-scuff matte for dark artwork) before mounting so the film stabilizes the paper surface.
- Board and sheet conditioning: Match the greyboard caliper—1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in)—and align grain directions across facing, board, and liner.
- Adhesive metering: Apply a uniform, controlled layer of adhesive across the mating surface. Excess adhesive introduces unnecessary moisture and squeeze-out; starved zones leave unbonded pockets.
- Registration and nip pressing: Register the printed facing onto the greyboard within the bleed or 15–20 mm (0.591–0.787 in) wrap margin, then pass the assembly through calibrated nip rollers to expel trapped air and establish full-area contact.
- Edge wrapping or counter-lining: Turn in the 15–20 mm (0.591–0.787 in) wrap margins cleanly over the board edges where specified, and mount the backing liner to balance drying stress.
- Weighted curing: Stack mounted boards flat under even pressure until adhesive moisture equilibrates and the bond reaches full strength before folding, scoring, or die-cutting (leaving 3–4 mm / 0.118–0.157 in die gaps on punchboards).
Sign-Off Criteria
- Flatness: Finished boards lie flat on a level surface after curing, without directional cupping or diagonal twist.
- Bond integrity: Full-area adhesion with no hollow spots, air blisters, or lifting along perimeters and corners.
- Edge and registration accuracy: Wrapped edges seat tightly within the 15–20 mm (0.591–0.787 in) turn-in allowance without exposed greyboard; die-cut punchboards and puzzles maintain clean 3–4 mm (0.118–0.157 in) die spacing and >= 3 mm (0.118 in) artwork safety.
- Surface condition: Dark solids and folded hinges show no scuffing, adhesive bleed, or cracking at the crease.
Failure Modes
- Warping and cupping: Caused by mounting a single face without a balancing counter-liner, mismatched grain direction between facing and greyboard, or uneven drying in stacked piles.
- Bubbling and blistering: Caused by air trapped during nip pressing, inconsistent adhesive roller pressure, or dry spots in the adhesive film.
- Edge lift and corner delamination: Caused by adhesive starvation near the sheet perimeter, wrap margins narrower than 15 mm (0.591 in), or trimming and die-cutting before the adhesive has cured.
- Hinge cracking or surface scuffing: Caused by exceeding TAC 280%–300% on dark artwork without protective anti-scuff matte lamination, or by folding mounted boards before moisture levels stabilize.
Parent guide Printing and Tabletop Manufacturing Glossary