In the Card Deck Press Glossary, compression set describes the irreversible or slow-recovering deformation that separates initial press-fit grip on the packing line from actual retention after warehouse storage and freight transit.
Mechanism and Specifications
When an EVA foam insert is compressed—either by tight-fitting game pieces pressing outward against cavity walls or by a box lid and stacked cartons pressing downward—the closed-cell structure absorbs energy. Once the load is removed, elastic recovery restores part of the original dimension, while collapsed or permanently deformed cells remain thinner.
In plain text, compression set is expressed as the unrecovered fraction of the applied compression:
Compression Set (%) = ((Original Thickness - Recovered Thickness) / (Original Thickness - Compressed Thickness)) x 100
A value of 0% means the foam returns completely to its original thickness; 100% means it retains zero recovery and stays at its compressed thickness.
Key dimensional and physical conditions governing EVA inserts in boxed games:
- Box and stack clearances: Standard boxed-game tolerances allow 1.5–2.5 mm (0.059–0.098 in) clearance across width and height and 1.5–3 mm (0.059–0.118 in) for stack height. If the insert and packed components exceed the vertical stack allowance, the closed lid applies continuous compressive force throughout storage.
- Load and mass distribution: Heavier components (measured in kg/lb) and high carton-stacking loads in transit increase compression depth on load-bearing ribs and tray floors.
- Time and temperature: Longer packed storage and elevated warehouse or container temperatures accelerate permanent cell collapse, increasing residual compression set even under moderate pressure.
- Cavity wall geometry: Thin ribs between adjacent recesses deform more readily under lateral pressure than wider, well-supported foam walls.
Production and Packaging Steps
- Size cavities for post-storage grip: Set interference fit and wall thickness so that minor permanent wall compression does not drop holding force below what is needed to keep pieces seated.
- Verify vertical stack clearance: Confirm that the insert height plus manuals, boards, and top components fits within the 1.5–3 mm (0.059–0.118 in) stack-height clearance and 1.5–2.5 mm (0.059–0.098 in) width/height box clearance so the lid does not pre-load the foam.
- Run a packed-box compression check: Pack sample components into the EVA cavities, close the box under representative top load, unpack after holding, and check whether cavities still grip each piece securely.
- Control master-carton orientation: Pack finished boxes so outer carton weight (kg/lb) transfers through rigid box walls and corners rather than pressing through the lid onto interior foam ribs.
Sign-Off Criteria
- Post-load cavity retention: Components remain seated in their EVA recesses without rattling or slipping out when the tray is tilted after a packed-box holding cycle.
- Clearance recovery: Insert height and outer perimeter stay within the planned 1.5–3 mm (0.059–0.118 in) stack-height and 1.5–2.5 mm (0.059–0.098 in) width/height box clearances without bowing the lid.
- Visual surface integrity: Foam walls, dividers, and floor recesses show no permanent creasing, flattened ribs, or collapsed corners after unloading.
Failure Modes
- Loose cavity grip after transit: Tightly wedged components compress the surrounding EVA walls during storage; when the customer lifts a piece out, the foam fails to rebound, leaving an oversized recess that no longer holds the piece.
- Crushed divider ribs: Over-tall inserts or heavy components stacked above the 1.5–3 mm (0.059–0.118 in) vertical allowance force the lid to crush narrow foam dividers, causing neighboring pieces to shift and collide.
- Permanent floor indentations: Dense or sharp-edged components press into the base of the tray under carton stacking loads, leaving deep impressions that tilt pieces or reduce support on subsequent repacking.