Specifications and Mechanisms
A die-cutting nick is created by grinding a small notch into the steel cutting rule. Where the blade is interrupted, the die does not sever the laminated board, leaving a narrow fiber bridge connecting the token or tile to the surrounding punchboard frame.
| Parameter | Specification / Condition | Production Impact |
|---|---|---|
| Greyboard caliper | 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), 3 mm (0.118 in) | Thicker boards carry stiffer bridges that resist flexing; thinner boards or heavy pieces need balanced nick placement to prevent premature drop-out. |
| Punchboard die gap | 3–4 mm (0.118–0.157 in) | Maintains a rigid matrix between adjacent cut lines so nicks anchor into solid board rather than a collapsing strip. |
| Bleed and safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety | Keeps critical artwork and text clear of the cut edge and any minor fiber disturbance where a bridge breaks. |
| Die-line layer | Separate spot layer in AI/PDF/PSD (PDF/X-1a or PDF/X-4) | Isolates cut contours from CMYK print plates so rule geometry and nick positions stay exact. |
Why Breaking the Bridge Leaves a Witness Mark
Because the bridge is an uncut section of both the greyboard core and the printed paper wrap, punching a piece out snaps those fibers under tension rather than slicing them cleanly. That fracture leaves a small raised burr or exposed core tab—known as a witness mark—at each nick location. Positioning nicks along straight, low-visibility edges rather than tight corners or focal art keeps the witness mark unobtrusive and prevents the wrap from peeling across the face of the piece.
Production Steps
- Prepare the die-line file: Place all punchboard cut contours on a dedicated spot layer with 3–4 mm (0.118–0.157 in) die gaps between pieces, 3 mm (0.118 in) bleed per side, and ≥3 mm (0.118 in) safety from the cut line.
- Assign nick positions: Mark nick locations on straight or secondary edges where breaking the bridge will not distort sharp tips or mar primary artwork.
- Notch the cutting rule and die-cut: Grind the notches into the steel rule, then die-cut the laminated greyboard sheet so exterior trim waste strips away while nicked pieces remain seated in the sheet.
- Test-punch a press sheet: Push pieces out by hand before full production to confirm release force and inspect witness marks on both printed faces.
Sign-Off Criteria
- Sheet retention: Pieces stay seated flat in the punchboard frame during normal handling, stacking, and transit without popping loose early.
- Clean release: Pieces push out by hand without delaminating the printed wrap or pulling tears into the ≥3 mm (0.118 in) safety zone.
- Controlled witness marks: Remaining burrs are small, flush enough not to snag during handling, and located on low-impact edges.
- Intact matrix: Surrounding 3–4 mm (0.118–0.157 in) die gaps hold firm without splitting when pieces are punched out.
Failure Modes
- Insufficient retention: Too few or overly shallow nicks allow pieces to drop out during waste stripping, collating, or shipping, resulting in loose components and scuffed corners.
- Excessive retention: Overly wide or numerous nicks require heavy thumb pressure to break, tearing the printed wrap across the piece face or leaving a jagged witness mark.
- Collapsed die gap: Spacing adjacent cuts closer than 3–4 mm (0.118–0.157 in) weakens the surrounding matrix so it splits under die pressure, causing uneven tears when pieces are removed.
- Nicks on delicate geometry: Placing a nick on a narrow tip or sharp corner bends or splits the tip instead of snapping cleanly along a straight edge.
Parent guide Printing and Tabletop Manufacturing Glossary