The core process variable is the combined thickness of the face stock, any surface film or varnish, and the adhesive layer. Because the cut must stop at the top surface of the release liner, any change in face thickness, lamination, or adhesive weight changes the required cut depth. For related finishing and die-making terms, see the manufacturing glossary.
Mechanism and Specifications
A pressure-sensitive sticker sheet consists of three functional layers:
- Face stock and surface finish: The printable top paper or film, plus any protective coating or lamination.
- Adhesive layer: The pressure-sensitive bond between the face and the liner.
- Release liner: The silicone-coated backing sheet that carries the stickers until application.
In kiss cutting, target cut depth follows a direct relationship:
target cut depth = face thickness + surface film thickness + adhesive thickness
The tooling—either a calibrated steel-rule die, rotary die, or controlled-depth plotter blade—penetrates through the face and adhesive and stops at the silicone release interface without severing the liner fibers or backing film.
Prepress and Artwork Specifications
- File format and color: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts, CMYK print layers at 300 DPI or higher, and a separate spot-color layer for the kiss-cut vector path.
- Bleed and safety: Extend artwork 3 mm (0.118 in) beyond the kiss-cut line on every side, and keep critical text or graphics at least 3 mm (0.118 in) inside the cut line.
- Ink density: Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for large dark fills, and keep total area coverage (TAC) at or below 280%–300%.
Production Steps
- Dieline separation and nesting: Verify the kiss-cut path sits on its own named spot layer with clean, closed vector paths and 3 mm (0.118 in) bleed around each sticker shape.
- Printing and surface finishing: Print the CMYK layers and apply any protective matte or gloss finish. If a surface film is added, record the added thickness before setting the cutter.
- Cut-depth calibration: Set die pressure or blade depth on make-ready sheets from the same material lot so the tool severs the face and adhesive cleanly without cutting into the release liner.
- Matrix handling and sheet trim: Strip the surrounding waste matrix if the job specifies weeded sheets, or leave the matrix in place as a flat border, then trim the outer release liner to final sheet size.
Sign-Off Criteria
- Clean peel: Each sticker lifts smoothly from the liner at a sharp fold angle without tearing the sticker edge or pulling the surrounding matrix.
- Intact release liner: The back of the liner shows no cut-through marks, fiber cracking, or split lines when the sheet is flexed along the kiss-cut paths.
- Cut-to-print registration: Printed borders and graphics align with the kiss-cut edge with no unprinted white slivers.
Failure Modes
- Under-cutting (bridging): Insufficient blade depth leaves fibers of the face stock or adhesive intact. Stickers snag, tear at the edge, or pull adjacent waste material when peeled.
- Over-cutting (liner scoring or cut-through): Excessive pressure cuts into or through the release liner. The sheet splits along the cut path during packing or handling, and stickers detach prematurely.
- Adhesive stringing or re-welding: Thick or soft adhesives stretch rather than part cleanly under a dull blade, or flow back together across a narrow cut kerf, causing edges to stick during peeling.
- Registration drift: Sheet movement between printing and die-cutting shifts the cut path off center; without 3 mm (0.118 in) bleed, the shifted edge exposes unprinted stock.
Parent guide Printing and Tabletop Manufacturing Glossary