Choose edge gilding when the deck uses uniform card stock with clean, burr-free trimmed edges and standard or thin surface coatings. Avoid or adjust edge gilding when cards carry thick lamination, when edge profiles vary across the stack, or when borderless dark ink coverage at the trim line is paired with heavy film that resists clean separation.
Specifications and Material Conditions
Edge gilding depends on how cleanly the paper core, surface coating, and corner geometry form a flat plane under pressure.
| Parameter | Specification | Production Implication |
|---|---|---|
| Standard offset run minimum | 200 decks (usual tiers 200/300/500/1,000+) | Applies to offset-printed decks scheduled with specialist finishing partners |
| 300 gsm art / blue-core stock | 0.28–0.31 mm (0.011–0.012 in) caliper | Lighter core requires firm, even clamping to prevent edge flutter |
| 310 gsm black-core linen stock | 0.30–0.32 mm (0.012–0.013 in) caliper | Embossed linen texture must be compressed flat at the edge |
| 330 gsm black-core stock | 0.32–0.34 mm (0.013 in) caliper | Rigid core holds a uniform vertical edge plane under clamp pressure |
| 350 gsm art stock | 0.34–0.38 mm (0.013–0.015 in) caliper | Thicker paper core exposes more fiber edge to preparation |
| 400 gsm stock | 0.40–0.44 mm (0.016–0.017 in) caliper | High-bulk edge absorbs preparation evenly when cleanly cut |
| PVC stock | 0.30 mm (0.012 in) caliper | Non-fibrous edge reacts differently to heat and adhesive transfer than paper |
| Double-sided film lamination | +0.03–0.05 mm (0.001–0.002 in) per card | Thick lamination can conflict with gilded edges during transfer and separation |
| Corner radius | R3–R3.5 mm (0.118–0.138 in) | Rounded corners must be cut cleanly so foil wraps smoothly around curves |
| Box clearance | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Leaves room for finished edges without scuffing against rigid box walls |
When specifying card stock weights, gsm (grams per square meter) measures basis weight directly, whereas US paper weights distinguish Cover LB (20 × 26 in / 508 × 660 mm basis sheet) from Text LB (25 × 38 in / 635 × 965 mm basis sheet). Card stocks in the 300–400 gsm range fall under Cover-weight board rather than Text-weight paper.
Production Steps
- Trimming and corner rounding: Die-cut or guillotine-trim the printed sheets to final deck dimensions and punch R3–R3.5 mm (0.118–0.138 in) corners. Because any step, burr, or blade nick leaves a recessed gap in the stack, blades must be sharp before gilding prep.
- Stack alignment and clamping: Jog the deck or multi-deck lift into tight registration and lock it in a mechanical or hydraulic clamp. Clamping compresses air out between cards and turns individual card edges into a single solid surface, preventing metallic layer bleed onto card faces.
- Edge preparation: Sand or smooth the clamped perimeter so paper fibers and coating edges sit flush across all four sides and around the corner radii. Dust and loose fibers are cleared from the clamped face before transfer.
- Metallic transfer: Apply heat, pressure, and metallic foil onto the prepared stack edges so the metallic layer bonds to the exposed card edges while releasing from the carrier film.
- Stack release and fanning: Unclamp the stack and fan the cards apart to break any thin metallic bridging between adjacent card edges without lifting the finish off the card perimeter.
Sign-Off Criteria
Verify the following conditions on finished deck samples before full-run sign-off:
- Continuous perimeter coverage: Metallic coverage is solid across all four straight edges and transitions smoothly around R3–R3.5 mm (0.118–0.138 in) corners without bare spots or streaks.
- Clean card-to-card separation: Cards fan apart smoothly with no stuck pairs, torn coating, or chipped edges at the separation line.
- No face bleed: Metallic transfer stops cleanly at the card edge with no foil flaking or haloing onto the front or back faces.
- Box fit: Finished decks slide into their packaging within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height clearance without scraping the gilded edges.
Failure Modes
- Thick lamination conflict: Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card; thick lamination creates a plastic lip along the trim edge that resists metallic adhesion and bridges adjacent cards, causing the foil to peel or tear when the deck is fanned.
- Uneven stack edges or cutting burrs: Dull die rules or shifted stacks leave microscopic steps between cards. The transfer roller or press bridges the high points and misses the recessed edges, leaving dull gaps or broken lines along the deck side.
- Insufficient clamping pressure: Loose clamping allows air gaps between cards, letting heat and metallic layer seep slightly inward onto card faces or leaving feathered, uneven edges.
- Corner-radius drag: Rough or inconsistent R3–R3.5 mm (0.118–0.138 in) corner cuts interrupt uniform pressure around the curve, resulting in thin coverage or flaking at the corners first.
Parent guide Printing and Tabletop Manufacturing Glossary