For related manufacturing definitions and tolerances, see the technical glossary.
Thickness, Stock Baseline, and Tolerances
Unlike liquid coatings that sit flush with or penetrate paper fibers, film lamination adheres a discrete plastic film to the printed sheet. Under double-sided lamination, the film applied to both faces adds 0.03–0.05 mm (0.0012–0.0020 in) to the total thickness of one card.
Paper stocks are specified by gsm (grams per square meter). When comparing specifications, note that US Text LB and US Cover LB are based on different basis sheet sizes and are not directly interchangeable with each other or with gsm without sheet-size conversion.
| Base Card Stock | Base Caliper (mm / in) | Estimated Finished Caliper with Double-Sided Film (mm / in) |
|---|---|---|
| 300 gsm art / blue core | 0.28–0.31 mm (0.0110–0.0122 in) | 0.31–0.36 mm (0.0122–0.0142 in) |
| 310 gsm black-core linen | 0.30–0.32 mm (0.0118–0.0126 in) | 0.33–0.37 mm (0.0130–0.0146 in) |
| 330 gsm black core | 0.32–0.34 mm (0.0126–0.0134 in) | 0.35–0.39 mm (0.0138–0.0154 in) |
| 350 gsm art stock | 0.34–0.38 mm (0.0134–0.0150 in) | 0.37–0.43 mm (0.0146–0.0169 in) |
| 400 gsm stock | 0.40–0.44 mm (0.0157–0.0173 in) | 0.43–0.49 mm (0.0169–0.0193 in) |
Because film thickness accumulates across every card in a deck, box dimensions must account for the laminated caliper rather than the raw sheet caliper:
Finished stack height = Card count x (Base stock caliper + 0.03 to 0.05 mm)
Finished stack height (in) = Card count x (Base stock caliper in inches + 0.0012 to 0.0020 in)
For boxed decks, standard box clearance is 1.5–3 mm (0.059–0.118 in) for stack height and 1.5–2.5 mm (0.059–0.098 in) across width and height.
Production Steps and Sign-Off Criteria
- Prepress and Color Setup: Prepare print files in AI, PDF, or PSD format as PDF/X-1a or PDF/X-4 with outlined or embedded fonts at ≥300 DPI. Use CMYK with separate spot layers, 100% K for fine text, rich black at
C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) ≤280%–300%. Set 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin, and ≥4–5 mm (0.157–0.197 in) safety margin for bordered backs. - Offset Printing: Print sheets onto the specified 300–400 gsm card stock and allow ink to set before film application.
- Double-Sided Film Bonding: Bond the selected film (such as anti-scuff matte for dark designs) to both sides of the printed sheet, adding 0.03–0.05 mm (0.0012–0.0020 in) per card.
- Cutting, Cornering, and Edge Finishing: Cut sheets to final card size, round corners to R3–R3.5 mm (0.118–0.138 in), and apply any downstream edge treatments.
- Stack and Box Fit Verification: Measure the finished deck stack height against the box interior to confirm it stays within the 1.5–3 mm (0.059–0.118 in) stack clearance.
Sign-Off Criteria
- Single-card caliper falls within the base stock range plus 0.03–0.05 mm (0.0012–0.0020 in).
- Film adheres smoothly across both faces with no bubbling, haze, or edge lifting at trimmed edges or R3–R3.5 mm (0.118–0.138 in) corners.
- Dark-ink areas using anti-scuff matte film show no visible scuffing after cutting and collation.
- Finished deck height fits the box within the 1.5–3 mm (0.059–0.118 in) stack-height clearance.
- Any specified edge gilding applies cleanly without interference from the laminated edge.
Concrete Failure Modes
- Box Stack-Height Overflow: Sizing a box from unlaminated paper caliper omits 0.03–0.05 mm (0.0012–0.0020 in) per card—adding 3.0–5.0 mm (0.118–0.197 in) across a 100-card deck—which can exceed the 1.5–3 mm (0.059–0.118 in) stack clearance and prevent the deck from seating in the box.
- Gilded-Edge Conflict: Specifying thick lamination alongside gilded edges causes the thicker film layer at the card perimeter to interfere with edge gilding application.
- Visible Scuffing on Dark Artwork: Pairing high-coverage dark areas or rich black (
C40–60 M30–40 Y30–40 K100) with standard film instead of anti-scuff matte leaves visible rub marks during cutting and handling. - Edge Lifting or Delamination: Incomplete film bonding at the trim line or around R3–R3.5 mm (0.118–0.138 in) corners causes the film layer to separate from the paper core during die-cutting.
Parent guide Printing and Tabletop Manufacturing Glossary